WO2016180362A1 - Dispositif de découpe et de broyage permettant d'homogénéiser et d'épurer des coulées métalliques et procédé de formation rhéologique - Google Patents
Dispositif de découpe et de broyage permettant d'homogénéiser et d'épurer des coulées métalliques et procédé de formation rhéologique Download PDFInfo
- Publication number
- WO2016180362A1 WO2016180362A1 PCT/CN2016/081982 CN2016081982W WO2016180362A1 WO 2016180362 A1 WO2016180362 A1 WO 2016180362A1 CN 2016081982 W CN2016081982 W CN 2016081982W WO 2016180362 A1 WO2016180362 A1 WO 2016180362A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- cutting
- metal melt
- melt
- breaking device
- metal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Ceased
Abstract
La présente invention concerne un dispositif de découpe et de broyage permettant d'homogénéiser et d'épurer des coulées métalliques, comprenant un mécanisme de lame de coupe, une cavité d'agitation (8), un couvercle de protection de niveau de liquide (3) ou un orifice de blocage supérieur (24), un coupleur (4), un mécanisme d'additif (41) et un moteur électrique (6). Le mécanisme de disque de coupe prévu dans une direction axiale de la cavité d'agitation (8) comprend une lame de coupe (1) et un arbre rotatif (2), et la lame de coupe (1) est montée sur l'arbre rotatif (2) ; l'arbre rotatif (2) et le moteur électrique (6) sont raccordés par l'intermédiaire du coupleur (4) ; le couvercle de protection de niveau de liquide (3) ou l'orifice de blocage supérieur est disposé en dessous ou au-dessus d'un niveau de liquide fondu (10) à l'intérieur de la cavité d'agitation (8). La lame de coupe (1) est un type de couteau, présentant une extrémité avant rotative pointue, et une surface latérale inclinée, plane ou incurvée. Le dispositif peut en outre comprendre un rail mobile (7) ou une plate-forme de levage. L'arbre rotatif peut également effectuer un mouvement de va-et-vient vers le haut et vers le bas dans la direction axiale tout en entraînant la lame de coupe en rotation à une vitesse élevée à l'intérieur de la cavité d'agitation, et est apte à générer une "turbulence réglable"ainsi qu'un "effet de coupe et de rupture", de telle sorte que l'ensemble du soluté à l'intérieur des matières fondues est hautement dispersé et homogénéisé, ce qui permet d'obtenir une structure de solidification de coulée homogénéisée, fine et parfaitement compactée. La présente invention concerne en outre un procédé de découpe, de broyage et de formation rhéologique permettant d'homogénéiser et d'épurer des coulées métalliques.
Applications Claiming Priority (12)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| CN201520311108.2U CN204584206U (zh) | 2015-05-14 | 2015-05-14 | 金属熔体均匀化处理的切割破散装置 |
| CN201520311108.2 | 2015-05-14 | ||
| CN201510245587.7 | 2015-05-14 | ||
| CN201510245587.7A CN106270420B (zh) | 2015-05-14 | 2015-05-14 | 金属熔体均匀化处理的切割破散装置与方法 |
| CN201520771948.7 | 2015-09-30 | ||
| CN201520771948.7U CN205046175U (zh) | 2015-09-30 | 2015-09-30 | 一种金属熔体扰动隔离器装置 |
| CN201521078338.5U CN205551420U (zh) | 2015-12-22 | 2015-12-22 | 用于搅拌金属熔体的搅拌腔 |
| CN201521078338.5 | 2015-12-22 | ||
| CN201510971278.8 | 2015-12-22 | ||
| CN201510971278.8A CN105436436B (zh) | 2015-12-22 | 2015-12-22 | 一种用于搅拌金属熔体的搅拌腔及其使用方法 |
| CN201521126795.7U CN205341841U (zh) | 2015-12-29 | 2015-12-29 | 一种金属熔体均匀化处理的切割片装置 |
| CN201521126795.7 | 2015-12-29 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| WO2016180362A1 true WO2016180362A1 (fr) | 2016-11-17 |
Family
ID=57248560
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PCT/CN2016/081982 Ceased WO2016180362A1 (fr) | 2015-05-14 | 2016-05-13 | Dispositif de découpe et de broyage permettant d'homogénéiser et d'épurer des coulées métalliques et procédé de formation rhéologique |
Country Status (1)
| Country | Link |
|---|---|
| WO (1) | WO2016180362A1 (fr) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN113102861A (zh) * | 2021-05-13 | 2021-07-13 | 重庆大学 | 一种具有随焊超声振动和碾压特征的电弧增材制造方法 |
| CN113102862A (zh) * | 2021-05-13 | 2021-07-13 | 重庆大学 | 一种超声辅助的电弧增材制造方法 |
| CN113188332A (zh) * | 2021-05-08 | 2021-07-30 | 宁波兴展旺节能科技有限公司 | 一种集中熔化炉 |
Citations (9)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4046559A (en) * | 1976-02-23 | 1977-09-06 | Kennecott Copper Corporation | Pyrometallurgical system for liquid-liquid contacting |
| CN1676237A (zh) * | 2005-04-05 | 2005-10-05 | 北京交通大学 | 一种制备颗粒增强铝基复合材料的真空机械双搅拌铸造法 |
| CN101391294A (zh) * | 2008-05-30 | 2009-03-25 | 北京科技大学 | 一种悬挂锥桶式半固态金属浆料制备及输送装置 |
| JP4319387B2 (ja) * | 2002-10-22 | 2009-08-26 | アルキャン・インターナショナル・ネットワーク・ジャパン株式会社 | アルミニウム溶湯の処理方法 |
| CN101733368A (zh) * | 2008-11-26 | 2010-06-16 | 北京有色金属研究总院 | 一种金属基复合材料的制备方法 |
| CN102181672A (zh) * | 2011-04-10 | 2011-09-14 | 北京交通大学 | 一种铝20锡半固态浆料的机械均匀分散方法 |
| CN204584206U (zh) * | 2015-05-14 | 2015-08-26 | 北京有色金属研究总院 | 金属熔体均匀化处理的切割破散装置 |
| CN205046175U (zh) * | 2015-09-30 | 2016-02-24 | 北京有色金属研究总院 | 一种金属熔体扰动隔离器装置 |
| CN105436436A (zh) * | 2015-12-22 | 2016-03-30 | 北京有色金属研究总院 | 一种用于搅拌金属熔体的搅拌腔及其使用方法 |
-
2016
- 2016-05-13 WO PCT/CN2016/081982 patent/WO2016180362A1/fr not_active Ceased
Patent Citations (9)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4046559A (en) * | 1976-02-23 | 1977-09-06 | Kennecott Copper Corporation | Pyrometallurgical system for liquid-liquid contacting |
| JP4319387B2 (ja) * | 2002-10-22 | 2009-08-26 | アルキャン・インターナショナル・ネットワーク・ジャパン株式会社 | アルミニウム溶湯の処理方法 |
| CN1676237A (zh) * | 2005-04-05 | 2005-10-05 | 北京交通大学 | 一种制备颗粒增强铝基复合材料的真空机械双搅拌铸造法 |
| CN101391294A (zh) * | 2008-05-30 | 2009-03-25 | 北京科技大学 | 一种悬挂锥桶式半固态金属浆料制备及输送装置 |
| CN101733368A (zh) * | 2008-11-26 | 2010-06-16 | 北京有色金属研究总院 | 一种金属基复合材料的制备方法 |
| CN102181672A (zh) * | 2011-04-10 | 2011-09-14 | 北京交通大学 | 一种铝20锡半固态浆料的机械均匀分散方法 |
| CN204584206U (zh) * | 2015-05-14 | 2015-08-26 | 北京有色金属研究总院 | 金属熔体均匀化处理的切割破散装置 |
| CN205046175U (zh) * | 2015-09-30 | 2016-02-24 | 北京有色金属研究总院 | 一种金属熔体扰动隔离器装置 |
| CN105436436A (zh) * | 2015-12-22 | 2016-03-30 | 北京有色金属研究总院 | 一种用于搅拌金属熔体的搅拌腔及其使用方法 |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN113188332A (zh) * | 2021-05-08 | 2021-07-30 | 宁波兴展旺节能科技有限公司 | 一种集中熔化炉 |
| CN113102861A (zh) * | 2021-05-13 | 2021-07-13 | 重庆大学 | 一种具有随焊超声振动和碾压特征的电弧增材制造方法 |
| CN113102862A (zh) * | 2021-05-13 | 2021-07-13 | 重庆大学 | 一种超声辅助的电弧增材制造方法 |
| CN113102862B (zh) * | 2021-05-13 | 2023-06-16 | 重庆大学 | 一种超声辅助的电弧增材制造方法 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN110280746B (zh) | 一种单源高强超声辅助铸造大规格2xxx系铝合金圆锭的方法 | |
| CN105772654B (zh) | 固液态金属搅拌混合方法 | |
| CN102345023B (zh) | 复合变质细化和电磁搅拌制备汽车铝车轮用半固态浆料的方法和装置 | |
| CN1768979A (zh) | 一种QTi3.5-10石墨半固态浆料制备方法 | |
| WO2016180362A1 (fr) | Dispositif de découpe et de broyage permettant d'homogénéiser et d'épurer des coulées métalliques et procédé de formation rhéologique | |
| CN107024115A (zh) | 一种熔炼装置及合金熔炼方法 | |
| CN106270420B (zh) | 金属熔体均匀化处理的切割破散装置与方法 | |
| CN112139472A (zh) | 快速制备半固态金属浆料的装置及方法 | |
| CN100574939C (zh) | 一种半固态合金浆料的制备与成型装置 | |
| CN202322960U (zh) | 一种轻合金半固态浆料制备装置 | |
| CN105149529A (zh) | 一种温控型金属铸造方法 | |
| Zhou et al. | Forced convection rheomoulding process for semisolid slurry preparation and microstructure evolution of 7075 aluminum alloy | |
| CN210085544U (zh) | 一种铝液在线精炼装置 | |
| CN202779647U (zh) | 一种半固态的有色金属连铸装置 | |
| CN108580814B (zh) | 一种制备金属半固态浆料的方法 | |
| CN108543921A (zh) | 强剪切与电磁场协同制备大规格均质铸锭的装置及方法 | |
| CN213437073U (zh) | 快速制备半固态金属浆料的装置 | |
| CN104439196B (zh) | 自耗剪切流法细化凝固组织的工艺及其装置 | |
| CN215998698U (zh) | 一种制备颗粒增强铝基复合材料的底部浇铸装置 | |
| CN116043046A (zh) | 一种无叶片搅拌法制备金属基复合材料的方法 | |
| CN102873291A (zh) | 一种电磁流振镁合金半固态半连续铸造装置及方法 | |
| CN102806329A (zh) | 一种可进行半固态加工的有色合金连续铸胚系统 | |
| CN108187560A (zh) | 一种无卷气铝-石墨半固态浆料的高效搅拌方法及装置 | |
| CN208131936U (zh) | 一种制备金属半固态浆料的装置 | |
| CN107983245A (zh) | 一种无卷气铁-石墨熔体的高效搅拌方法及装置 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| 121 | Ep: the epo has been informed by wipo that ep was designated in this application |
Ref document number: 16792212 Country of ref document: EP Kind code of ref document: A1 |
|
| NENP | Non-entry into the national phase |
Ref country code: DE |
|
| 122 | Ep: pct application non-entry in european phase |
Ref document number: 16792212 Country of ref document: EP Kind code of ref document: A1 |