SU548396A1 - The method of adjusting the geometric parameters of the weld - Google Patents
The method of adjusting the geometric parameters of the weldInfo
- Publication number
- SU548396A1 SU548396A1 SU1230938A SU1230938A SU548396A1 SU 548396 A1 SU548396 A1 SU 548396A1 SU 1230938 A SU1230938 A SU 1230938A SU 1230938 A SU1230938 A SU 1230938A SU 548396 A1 SU548396 A1 SU 548396A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- weld
- adjusting
- geometric parameters
- welding
- gas mixture
- Prior art date
Description
так как подоор необходимой дл проплавдеии 1г формироваин шва газовой смеси на каждом участке осуществл ют при неизменной скоростн сварки. Как показали испытани изменение количественного соотношени газовой смесн приводит к изменению в зкости жидкого металла сварочной ванны, что улучшает формирование шва в различных нространственных положени х . Фор м л а изобретени Снособ регулировани геометрических иараметров сварного шва при автоматической сварке Неповоротных стыков труб иутем регулироваии мош.иост1( дуги, о т л и ч а ю 1И и и с тем, что, с н,елыо упрощени настройки программы и повышени качества сварного соединени при сварке в смеси аргона и гели , регулировани мощности дуги осуществл ют путем изменени количественного соотношени между компонентами газовой смеси в зависимости от пространственного положенн сварочной ванны. Источники информаиии, прии тые во внимание при экспертизе 1. Юрченко Ю. Ф. и др. Монтаж и сварка трубопроводов нз коррозионно-стойких сталей в атомиой промыи1ленности. .М., Лтомпздат, 1966, с. 146-149.Since the necessary for proplavia 1g of the formation of the weld gas mixture in each section is carried out at a constant welding speed. As shown by tests, a change in the quantitative ratio of the gas mixture leads to a change in the viscosity of the liquid metal of the weld pool, which improves the formation of the seam in various spatial positions. Formula of the invention The method of adjusting the geometric parameters of the weld in automatic welding of the non-turn joints with pipes and the regulation of mosh.Iost1 (arcs, which are used to simplify the program settings and improve the quality of when welding in a mixture of argon and gels, adjusting the arc power is carried out by varying the quantitative ratio between the components of the gas mixture depending on the spatial position of the weld pool. s at examination 1 Yurchenko J. F., et al. Assembly and welding of pipes nz corrosion-resistant steels in promyi1lennosti atoms. .M., Ltompzdat, 1966, pp. 146-149.