SU128579A1 - Method of casting steel - Google Patents

Method of casting steel

Info

Publication number
SU128579A1
SU128579A1 SU633770A SU633770A SU128579A1 SU 128579 A1 SU128579 A1 SU 128579A1 SU 633770 A SU633770 A SU 633770A SU 633770 A SU633770 A SU 633770A SU 128579 A1 SU128579 A1 SU 128579A1
Authority
SU
USSR - Soviet Union
Prior art keywords
casting steel
casting
stand
steel
ingot
Prior art date
Application number
SU633770A
Other languages
Russian (ru)
Inventor
В.И. Бельский
Г.А. Гарбуз
А.М. Почтман
Original Assignee
В.И. Бельский
Г.А. Гарбуз
А.М. Почтман
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by В.И. Бельский, Г.А. Гарбуз, А.М. Почтман filed Critical В.И. Бельский
Priority to SU633770A priority Critical patent/SU128579A1/en
Application granted granted Critical
Publication of SU128579A1 publication Critical patent/SU128579A1/en

Description

Обычно при существующем способе разливки кип щей стали в изложницы с уширением книзу нижн   часть слитка получаетс  плоской и широкой. При прокатке таких слитков отрезаетс  от донной части слитка и направл етс  в отход 3,, металла.Usually, with the existing method of casting boiling steel into molds with widening downwards, the lower part of the ingot is flat and wide. When rolling such ingots, it is cut off from the bottom part of the ingot and sent to waste 3 ,, metal.

В описываемом способе при разливке кип щей стали сифоном илп сверху предлагаетс  примен ть подставку дл  изложниц, уширенных книзу. Предлагаема  подставка имеет трапецеидальную или сферическую форму внутренней поверхности. Подставку устанавливают иа поддон , после чего на нее помещают изложницу. Форма предлагаемой подставки дл  нижней части слитка уменьшает количество отходов металла при обрезке слитка и улучшает поверхности донной части блумсов или сл баПредмет изобретени In the described method, when casting boiling steel with a siphon or on the top, it is proposed to use a stand for the molds broadened downwards. The proposed stand has a trapezoidal or spherical shape of the inner surface. The stand is installed on a pallet, after which a mold is placed on it. The shape of the proposed stand for the lower part of the ingot reduces the amount of metal waste when trimming the ingot and improves the surfaces of the bottom part of the blooms or slab of the invention.

Способ разливки стали, отличающийс  тем, что, с целью уменьшени  отходов при обрезке слитков, применена подставка дл  изложниц , уширенных книзу, при разливке кип щей стали сифоном и сверху.A method of casting steel, characterized in that, in order to reduce waste when cutting ingots, a stand was used for the downwardly casting molds, when casting boiling steel with a siphon and on top.

SU633770A 1959-07-13 1959-07-13 Method of casting steel SU128579A1 (en)