[go: up one dir, main page]

SU109540A1 - Method of restoring the active mass of the negative electrode - Google Patents

Method of restoring the active mass of the negative electrode

Info

Publication number
SU109540A1
SU109540A1 SU361095A SU361095A SU109540A1 SU 109540 A1 SU109540 A1 SU 109540A1 SU 361095 A SU361095 A SU 361095A SU 361095 A SU361095 A SU 361095A SU 109540 A1 SU109540 A1 SU 109540A1
Authority
SU
USSR - Soviet Union
Prior art keywords
active mass
restoring
negative electrode
mass
active
Prior art date
Application number
SU361095A
Other languages
Russian (ru)
Inventor
Г.И. Беляев
ев Г.И. Бел
Original Assignee
Г.И. Беляев
ев Г.И. Бел
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Г.И. Беляев, ев Г.И. Бел filed Critical Г.И. Беляев
Priority to SU361095A priority Critical patent/SU109540A1/en
Application granted granted Critical
Publication of SU109540A1 publication Critical patent/SU109540A1/en

Description

Дл  уменьшени  расхода дефицитных активных материалов, необходимых дл  производства щелочных кадмиево-никелевых аккумул торов , на аккумул торные заводы обычно доставл ют отработанные аккумул торы, с целью восстановлени  активной массы их отрицательных пластин. При этом активную массу высушенных блоков отрицательных пластин отдел ют механическим путем от металлической оболочки, подвергают тонкому помолу и рассеву и используют затем дл  изготовлени  новых элементов .To reduce the consumption of scarce active materials required for the production of alkaline cadmium-nickel batteries, waste batteries are usually delivered to battery plants in order to restore the active mass of their negative plates. In this case, the active mass of the dried blocks of negative plates is separated mechanically from the metal shell, subjected to fine grinding and sieving and then used to make new elements.

Предлагаемый способ позвол ет ускорить процесс отделени  активной массы отрицательных пластин от металлической оболочки и повысить благодар  этому производительность труда.The proposed method makes it possible to accelerate the process of separating the active mass of the negative plates from the metal shell and thereby increase the labor productivity.

Дл  этого блоки пластин измельчают ножницами или другими подобными приспособлени ми до состо ни  «лапши и отдел ют электромагнитным путем активную массу от металла оболочки (мелких кусочков ламельной ленты и остатков ребер). В дальнейшем активную массу отмывают в нагретой до 80-90° воде (производ т 4 отмывки ), сушат в сушилках при температуре 60-80° и подвергают затем тонкому помолу и рассеву.To do this, the blocks of the plates are crushed with scissors or other similar devices to the noodle state and the active mass is separated from the shell metal (small pieces of lamella tape and ribbed edges) by electromagnetic means. Subsequently, the active mass is washed in water heated to 80-90 ° (4 washes are made), dried in a dryer at a temperature of 60-80 ° and then subjected to fine grinding and sieving.

Предмет изобретени Subject invention

Способ восстановлени  активной массы отрицательного электрода из отработанных ш,елочных кадмиевоникелевых аккумул торов, состо ш ,ий в том, что активную массу высушенных блоков отрицательных электродов механическим путем отдел ют от металлической оболочки, подвергают тонкому помолу и рассеву , после чего используют дл  изготовлени  новых элементов, отличающийс  тем, что, дл  отделени  массы от металлической оболочки , блоки измельчают ножницами или т. п. приспособлени ми до состо ни  «лапши и сепарируют электромагнитным путем, а отделенную от металла массу отмывают в нагретой до 80-90° воде, сушат и после этого подвергают вышеуказанному помолу.The method of restoring the active mass of the negative electrode from spent wedges, cadmium-nickel nickel batteries, consists in that the active mass of the dried blocks of negative electrodes is mechanically separated from the metal shell, subjected to fine grinding and sieving, and then used to make new elements characterized in that, in order to separate the mass from the metal shell, the blocks are crushed with scissors or the like with devices to the noodle state and separated by electromagnetic means, and from Elena from metal mass is washed in heated to 80-90 ° water, dried and then subjected to the above milled.

SU361095A 1947-12-17 1947-12-17 Method of restoring the active mass of the negative electrode SU109540A1 (en)