RU2013126823A - METHOD FOR DEPLETING COPPER CONTAINING SLAGS - Google Patents
METHOD FOR DEPLETING COPPER CONTAINING SLAGS Download PDFInfo
- Publication number
- RU2013126823A RU2013126823A RU2013126823/02A RU2013126823A RU2013126823A RU 2013126823 A RU2013126823 A RU 2013126823A RU 2013126823/02 A RU2013126823/02 A RU 2013126823/02A RU 2013126823 A RU2013126823 A RU 2013126823A RU 2013126823 A RU2013126823 A RU 2013126823A
- Authority
- RU
- Russia
- Prior art keywords
- slag
- reducing agent
- oxygen
- copper containing
- terms
- Prior art date
Abstract
Способ обеднения медьсодержащих шлаков, включающий их обработку оксидом кальция в присутствии твердого углеродистого восстановителя при повышенной температуре, отличающийся тем, что обработку шлака в присутствии восстановителя ведут при соотношении шлака к восстановителю по содержанию в нем углерода 1:(0,05-0,09) и продувают поверхность шлака кислородсодержащим окислителем с использованием верхнего непогружного дутья при расходе кислородсодержащего окислителя в количестве, по содержанию в нем кислорода, 50-100 кг на тонну шлака.A method of depletion of copper-containing slags, including their treatment with calcium oxide in the presence of a solid carbonaceous reducing agent at an elevated temperature, characterized in that the processing of slag in the presence of a reducing agent is carried out at a slag to reducing agent ratio in terms of carbon content of 1: (0.05-0.09) and the surface of the slag is blown with an oxygen-containing oxidizer using an overhead non-submersible blast at a flow rate of an oxygen-containing oxidizer in an amount, in terms of oxygen content, of 50-100 kg per ton of slag.
Claims (1)