FR2360362A1 - Coquille de coulee pour la coulee des metaux - Google Patents
Coquille de coulee pour la coulee des metauxInfo
- Publication number
- FR2360362A1 FR2360362A1 FR7723548A FR7723548A FR2360362A1 FR 2360362 A1 FR2360362 A1 FR 2360362A1 FR 7723548 A FR7723548 A FR 7723548A FR 7723548 A FR7723548 A FR 7723548A FR 2360362 A1 FR2360362 A1 FR 2360362A1
- Authority
- FR
- France
- Prior art keywords
- casting
- shell
- metal
- steel
- wear
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
a. Coquille de coulée, plus spécialement pour la coulée de l'acier, constituée par un corps métallique avec une couche intérieure en matériau résistant à l'usure. b. Coquille caractérisée en ce que la couche anti-usure consiste en une couche métallique déposée par électrolyse ou sans courant, avec des particules solides, insolubles dans l'électrolyte, qui sont incorporées dans le réseau cristallin du métal. c. Coquille applicable à la coulée en continu d'acier.
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| DE2634633A DE2634633C2 (de) | 1976-07-31 | 1976-07-31 | Stranggießkokille aus einem Kupferwerkstoff, insbesondere zum Stranggießen von Stahl |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| FR2360362A1 true FR2360362A1 (fr) | 1978-03-03 |
| FR2360362B1 FR2360362B1 (fr) | 1980-12-05 |
Family
ID=5984487
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| FR7723548A Granted FR2360362A1 (fr) | 1976-07-31 | 1977-07-29 | Coquille de coulee pour la coulee des metaux |
Country Status (16)
| Country | Link |
|---|---|
| US (1) | US4197902A (fr) |
| JP (1) | JPS5319930A (fr) |
| AT (1) | AT360684B (fr) |
| BE (1) | BE857251A (fr) |
| CA (1) | CA1097024A (fr) |
| CH (1) | CH624860A5 (fr) |
| DD (1) | DD130559A5 (fr) |
| DE (1) | DE2634633C2 (fr) |
| ES (1) | ES460895A1 (fr) |
| FI (1) | FI772271A7 (fr) |
| FR (1) | FR2360362A1 (fr) |
| GB (1) | GB1546307A (fr) |
| IT (1) | IT1079888B (fr) |
| SE (1) | SE427630B (fr) |
| YU (1) | YU39681B (fr) |
| ZA (1) | ZA774567B (fr) |
Families Citing this family (40)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5519428A (en) * | 1978-07-28 | 1980-02-12 | Sumitomo Metal Ind Ltd | Lubricating method in casting mold of horizontal continuous casting method |
| CH644040A5 (de) * | 1979-11-07 | 1984-07-13 | Accumold Ag | Verfahren zur behandlung der innenoberflaeche eines kokillenrohres zum stranggiessen. |
| JPS56136263A (en) * | 1980-03-29 | 1981-10-24 | Kobe Steel Ltd | Electromagnetic stirrer built-in type assembled mold in continuous casting plant |
| DE3038289A1 (de) * | 1980-10-10 | 1982-05-27 | Egon 5650 Solingen Evertz | Verfahren zum abscheiden von metallschichten auf den waenden von kokillen |
| DE3218100A1 (de) * | 1982-05-13 | 1983-11-17 | Kabel- und Metallwerke Gutehoffnungshütte AG, 3000 Hannover | Verfahren zur herstellung einer rohrkokille mit rechteckigem bzw. quadratischem querschnitt |
| EP0108744B1 (fr) * | 1982-11-04 | 1988-08-17 | VOEST-ALPINE Aktiengesellschaft | Lingotière à extrémités ouvertes pour une installation de coulée continue |
| DE3313503A1 (de) * | 1983-04-14 | 1984-10-18 | Evertz, Egon, 5650 Solingen | Einteilige durchlaufstranggiesskokille und verfahren zu ihrer herstellung |
| DE3336373A1 (de) * | 1983-10-06 | 1985-04-25 | Egon 5650 Solingen Evertz | Kokille fuer das stranggiessen von stahl und verfahren zu ihrer herstellung |
| DE3415050A1 (de) * | 1984-04-21 | 1985-10-31 | Kabel- und Metallwerke Gutehoffnungshütte AG, 3000 Hannover | Verfahren zur herstellung einer stranggiesskokille mit verschleissfester schicht |
| JPS60238078A (ja) * | 1984-04-27 | 1985-11-26 | Mazda Motor Corp | 鋳物表面の高合金化法 |
| JPS6115998A (ja) * | 1984-06-29 | 1986-01-24 | Toshiba Corp | 圧縮機等の摺動部品 |
| US4669529A (en) * | 1984-12-03 | 1987-06-02 | Egon Evertz | Continuous casting mould |
| JPS61149499A (ja) * | 1984-12-25 | 1986-07-08 | Suzuki Motor Co Ltd | 分散めつき被膜 |
| FI75748C (fi) * | 1986-08-15 | 1988-08-08 | Outokumpu Oy | Kokill. |
| DE3718372A1 (de) * | 1987-06-02 | 1988-12-15 | Stolberger Metallwerke Gmbh | Stranggiesskokille zum kontinuierlichen giessen von nichteisenmetallen |
| US4802436A (en) * | 1987-07-21 | 1989-02-07 | Williams Gold Refining Company | Continuous casting furnace and die system of modular design |
| US5014768A (en) * | 1989-06-30 | 1991-05-14 | Waters & Associates | Chill plate having high heat conductivity and wear resistance |
| FR2666756B1 (fr) * | 1990-09-14 | 1993-08-13 | Usinor Sacilor | Cylindre pour la coulee continue de bandes de metal entre deux cylindres, notamment d'acier, et procede de fabrication de ce cylindre. |
| US5377526A (en) * | 1992-09-03 | 1995-01-03 | Racine Flame Spray Inc. | Traction analyzer |
| JP2000517246A (ja) * | 1996-09-03 | 2000-12-26 | エイジー インダストリーズ インコーポレイテッド | 連続鋳造法のための改良された鋳型表面及びその製造方法 |
| WO1998042460A2 (fr) * | 1997-03-25 | 1998-10-01 | Komtek, Inc. | Systeme de mise en forme de metal |
| DE19852473C5 (de) * | 1998-11-13 | 2005-10-06 | Sms Demag Ag | Kokillenplatte einer Stranggießanlage |
| US6470550B1 (en) * | 1999-11-11 | 2002-10-29 | Shear Tool, Inc. | Methods of making tooling to be used in high temperature casting and molding |
| JP3061186B1 (ja) * | 1999-11-26 | 2000-07-10 | 株式会社野村鍍金 | 連続鋳造用鋳型及びその製造方法 |
| US7021363B2 (en) | 2000-04-27 | 2006-04-04 | Sms Demag | Mold wall, especially a broad side wall of a continuous casting mold for steel |
| DE10062490A1 (de) | 2000-04-27 | 2001-10-31 | Sms Demag Ag | Kokillenwand, insbesondere Breitseitenwand einer Stranggießkokille für Stahl |
| US6447704B1 (en) | 2000-05-23 | 2002-09-10 | Gmic, Corp. | Thermal-sprayed tooling |
| DE10227034A1 (de) * | 2002-06-17 | 2003-12-24 | Km Europa Metal Ag | Kupfer-Gießform |
| CN1747797B (zh) * | 2003-02-07 | 2011-08-17 | 戴蒙得创新股份有限公司 | 具有扩大抵抗能力的设备磨损表面及其加工方法 |
| WO2005028143A1 (fr) * | 2003-09-24 | 2005-03-31 | Sumitomo Metal Industries, Ltd. | Moule de coulage et procede de coulage en continu pour alliage de cuivre |
| BRPI0506625A (pt) * | 2004-02-11 | 2007-05-02 | Diamond Innovations Inc | artigo e método para produzir um objeto moldado |
| JP4354315B2 (ja) * | 2004-03-22 | 2009-10-28 | 東芝機械株式会社 | アルミニウム溶湯接触部材およびその製造方法 |
| US7562858B2 (en) * | 2005-03-16 | 2009-07-21 | Diamond Innovations, Inc. | Wear and texture coatings for components used in manufacturing glass light bulbs |
| JP4499024B2 (ja) * | 2005-12-02 | 2010-07-07 | 東芝機械株式会社 | アルミダイカスト用給湯管およびその製造方法 |
| DE102005061134A1 (de) * | 2005-12-19 | 2007-06-21 | Siemens Ag | Bauteil eines Stahlwerks, wie Stranggussanlage oder Walzwerk, Verfahren zur Herstellung eines solchen Bauteils sowie Anlage zur Erzeugung oder Verarbeitung von metallischen Halbzeugen |
| MX2008011590A (es) * | 2006-03-24 | 2008-09-22 | Toshiba Machine Co Ltd | Tuberia de alimentacion de fusion para pieza fundida de aluminio. |
| US20080093047A1 (en) * | 2006-10-18 | 2008-04-24 | Inframat Corporation | Casting molds coated for surface enhancement and methods of making |
| GB0807627D0 (en) * | 2008-04-25 | 2008-06-04 | Accentus Plc | A thermal barrier, an article with a thermal barrier and a method of applying a thermal barrier to a surface |
| DE102010012309A1 (de) | 2010-03-23 | 2011-09-29 | Sms Siemag Ag | Kokillenelement und Verfahren zu dessen Beschichtung |
| CN105583300B (zh) * | 2013-06-29 | 2017-12-05 | 盐城咏恒投资发展有限公司 | 一种具有较好刚性和耐冲击强度的耐磨冲压模具 |
Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| FR911817A (fr) * | 1945-06-27 | 1946-07-22 | Fond Jules Bonvarlet | Procédé de protection des coquilles de moulage et produits industriels nouveaux enrésultant |
| FR2189145A1 (fr) * | 1972-05-08 | 1974-01-25 | Sherwood Refractories | |
| FR2264610A1 (fr) * | 1974-03-20 | 1975-10-17 | Alusuisse |
Family Cites Families (12)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US2090408A (en) * | 1931-10-30 | 1937-08-17 | Eaton Erb Foundry Company | Mold coating |
| US3061525A (en) * | 1959-06-22 | 1962-10-30 | Platecraft Of America Inc | Method for electroforming and coating |
| AT234930B (de) * | 1960-02-25 | 1964-07-27 | Boehler & Co Ag Geb | Stranggußkokillen zum Stranggießen von hochschmelzenden Metallen wie Eisen und Stahl, die im wesentlichen aus Kupfer bestehen |
| US3266107A (en) * | 1964-07-02 | 1966-08-16 | American Radiator & Standard | Coated mold and method of coating same |
| DE1621206B2 (de) * | 1967-01-18 | 1971-12-16 | Friedr. Blasberg Gmbh & Co, Kg, 5650 Solingen | Verfahren zur beschichtung gleitend reibend auf verschleiss beanspruchter werkstuecke |
| US3753667A (en) * | 1968-01-16 | 1973-08-21 | Gen Am Transport | Articles having electroless metal coatings incorporating wear-resisting particles therein |
| US3762882A (en) * | 1971-06-23 | 1973-10-02 | Di Coat Corp | Wear resistant diamond coating and method of application |
| JPS4828255A (fr) * | 1971-08-17 | 1973-04-14 | ||
| JPS5318970B2 (fr) * | 1972-07-11 | 1978-06-17 | ||
| US3891542A (en) * | 1973-11-05 | 1975-06-24 | Ford Motor Co | Method for insuring high silicon carbide content in elnisil coatings |
| US3990955A (en) * | 1974-02-04 | 1976-11-09 | The International Nickel Company, Inc. | Electrodeposition of hard nickel |
| US4037646A (en) * | 1975-06-13 | 1977-07-26 | Sumitomo Metal Industries, Ltd. | Molds for continuously casting steel |
-
1976
- 1976-07-31 DE DE2634633A patent/DE2634633C2/de not_active Expired
-
1977
- 1977-06-20 CH CH751477A patent/CH624860A5/de not_active IP Right Cessation
- 1977-07-04 IT IT50111/77A patent/IT1079888B/it active
- 1977-07-12 GB GB29218/77A patent/GB1546307A/en not_active Expired
- 1977-07-20 ES ES460895A patent/ES460895A1/es not_active Expired
- 1977-07-25 FI FI772271A patent/FI772271A7/fi not_active Application Discontinuation
- 1977-07-27 YU YU1849/77A patent/YU39681B/xx unknown
- 1977-07-28 US US05/819,773 patent/US4197902A/en not_active Expired - Lifetime
- 1977-07-28 AT AT555577A patent/AT360684B/de active
- 1977-07-28 BE BE179719A patent/BE857251A/fr not_active IP Right Cessation
- 1977-07-28 ZA ZA00774567A patent/ZA774567B/xx unknown
- 1977-07-29 CA CA283,733A patent/CA1097024A/fr not_active Expired
- 1977-07-29 DD DD7700200354A patent/DD130559A5/xx unknown
- 1977-07-29 SE SE7708708A patent/SE427630B/xx not_active IP Right Cessation
- 1977-07-29 JP JP9049577A patent/JPS5319930A/ja active Granted
- 1977-07-29 FR FR7723548A patent/FR2360362A1/fr active Granted
Patent Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| FR911817A (fr) * | 1945-06-27 | 1946-07-22 | Fond Jules Bonvarlet | Procédé de protection des coquilles de moulage et produits industriels nouveaux enrésultant |
| FR2189145A1 (fr) * | 1972-05-08 | 1974-01-25 | Sherwood Refractories | |
| FR2264610A1 (fr) * | 1974-03-20 | 1975-10-17 | Alusuisse |
Also Published As
| Publication number | Publication date |
|---|---|
| CA1097024A (fr) | 1981-03-10 |
| SE427630B (sv) | 1983-04-25 |
| ATA555577A (de) | 1980-06-15 |
| DE2634633C2 (de) | 1984-07-05 |
| GB1546307A (en) | 1979-05-23 |
| ES460895A1 (es) | 1978-04-16 |
| IT1079888B (it) | 1985-05-13 |
| YU39681B (en) | 1985-03-20 |
| SE7708708L (sv) | 1978-02-01 |
| ZA774567B (en) | 1978-06-28 |
| DD130559A5 (de) | 1978-04-12 |
| DE2634633A1 (de) | 1978-02-02 |
| CH624860A5 (fr) | 1981-08-31 |
| FI772271A7 (fr) | 1978-02-01 |
| US4197902A (en) | 1980-04-15 |
| JPS6124100B2 (fr) | 1986-06-09 |
| JPS5319930A (en) | 1978-02-23 |
| YU184977A (en) | 1982-10-31 |
| AT360684B (de) | 1981-01-26 |
| BE857251A (fr) | 1978-01-30 |
| FR2360362B1 (fr) | 1980-12-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| FR2360362A1 (fr) | Coquille de coulee pour la coulee des metaux | |
| GB1503706A (en) | Durable alloys | |
| FR2406008A1 (fr) | Electrode pour le depot electrolytique de metaux | |
| FR2436478A1 (fr) | Fermeture de forages de stockage destines au stockage definitif de dechets radioactifs, et procede de mise en place de cette fermeture | |
| ES8403052A1 (es) | Metodo de preparacion de un producto conglomerado para piezas de fundicion resistentes al desgaste. | |
| BE903578A (fr) | Procede de fabrication d'une lingotiere de coulee continue munie de profiles resistant a l'usure. | |
| FR2513981B1 (fr) | Compose ternaire d'intercalation d'un graphite avec un fluorure d'un metal et du fluor, procede pour sa production et materiau electriquement conducteur le contenant | |
| FR2457462A1 (fr) | Procede de fusion de composes d'oxydes fusibles de metaux et autres materiaux et four electrique pour sa mise en oeuvre | |
| ES368084A1 (es) | Procedimiento de fundicion continua de metales. | |
| FR2455633A1 (fr) | Acier a coupe rapide du type tungstene, contenant du vanadium et produit selon la metallurgie des poudres | |
| DE2704918A1 (de) | Verfahren zum kontinuierlichen vergiessen von schmelzfluessigen metallen im magnetischen drehfeld | |
| ES469349A1 (es) | Procedimiento para la admision del caldo metalico a un moldede fundicion de tipo oruga | |
| DE1483338B2 (de) | Verfahren und vorrichtung zum elektrolytischen herstellen von aluminium oder dessen legierungen | |
| FR2367557A1 (fr) | Perfectionnements aux rouleaux de guidage, notamment pour installation de coulee continue | |
| ES485731A1 (es) | Procedimiento de revestimiento de hornos electrometalurgicos | |
| FR2355920A1 (fr) | Alliage anti-friction | |
| FR2418275A1 (fr) | Alliage d'aluminium resistant a la corrosion | |
| FR2398117A1 (fr) | ||
| US3074876A (en) | Anode for cathodic protection | |
| SU583206A1 (ru) | Катодный узел электролизера дл получени алюмини | |
| Arvia et al. | Kinetics of the hydrogen-evolution reaction on palladium electrodes in molten potassium bisulphate | |
| FR2448951A1 (fr) | Perfectionnements de, ou concernant, la coulee de lingots metalliques | |
| SU439364A1 (ru) | Электрод дл холодной сварки чугуна | |
| FR1455669A (fr) | Procédé et dispositif pour la réduction de l'usure d'électrodes métalliques servant à la production d'arcs électriques | |
| GB965426A (en) | Improvements in or relating to the continuous-casting of metals |