[go: up one dir, main page]

CN109956681A - A kind of glass strip cleaning method and glass decoating liquid - Google Patents

A kind of glass strip cleaning method and glass decoating liquid Download PDF

Info

Publication number
CN109956681A
CN109956681A CN201711423676.1A CN201711423676A CN109956681A CN 109956681 A CN109956681 A CN 109956681A CN 201711423676 A CN201711423676 A CN 201711423676A CN 109956681 A CN109956681 A CN 109956681A
Authority
CN
China
Prior art keywords
glass
cleaning method
preset temperature
mass fraction
strip cleaning
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201711423676.1A
Other languages
Chinese (zh)
Other versions
CN109956681B (en
Inventor
周群飞
蔡杰勇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Lens Technology Changsha Co Ltd
Original Assignee
Lens Technology Changsha Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Lens Technology Changsha Co Ltd filed Critical Lens Technology Changsha Co Ltd
Priority to CN201711423676.1A priority Critical patent/CN109956681B/en
Publication of CN109956681A publication Critical patent/CN109956681A/en
Application granted granted Critical
Publication of CN109956681B publication Critical patent/CN109956681B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

This application discloses a kind of glass strip cleaning method and glass decoating liquids, the glass strip cleaning method carries out main strip to glass including the use of the decoating liquid comprising metasilicate pentahydrate sodium and neopelex with the first preset temperature, continues preset time;The glass is scrubbed using the cleaning solution comprising metasilicate pentahydrate sodium and neopelex with the second preset temperature;Spray cleaning is carried out to the glass using the deionized water with third preset temperature;Dewatered drying is carried out to the glass.Above-mentioned glass strip cleaning method and glass decoating liquid, can be avoided and damage to the ink after exposure development, and production cost is low, high production efficiency.

Description

A kind of glass strip cleaning method and glass decoating liquid
Technical field
The invention belongs to glass working arts fields, more particularly to a kind of glass strip cleaning method and glass strip Liquid.
Background technique
With the development of the society, 2D, 3D glass have been applied on electronic product, and become a kind of fashion, with tradition Plastics are compared with metallic mobile phone battery cover, and 2D, 3D bend glass have frivolous, transparent cleaning, anti-fingerprint, anti-dazzle, scratch resistant, resistance to The advantages that time property.Withdrawal plating has obtained fine utilization as a kind of novel operation mode on glass at present, and the technique is not Only available graceful accurate pattern, and the pattern does not have concave-convex sense, is of close texture.However, use in the prior art For strip cleaning process using strong basicity decoating liquid, this will cause injury to the ink after exposure development.
Summary of the invention
To solve the above problems, can be avoided the present invention provides a kind of glass strip cleaning method and glass decoating liquid Ink after exposure development is damaged, and production cost is low, high production efficiency.
A kind of glass strip cleaning method provided by the invention, comprising:
Using the decoating liquid comprising metasilicate pentahydrate sodium and neopelex with the first preset temperature to glass Glass carries out main strip, continues preset time;
Using the cleaning solution comprising metasilicate pentahydrate sodium and neopelex with the second preset temperature to institute Glass is stated to be scrubbed;
Spray cleaning is carried out to the glass using the deionized water with third preset temperature;
Dewatered drying is carried out to the glass.
Preferably, in above-mentioned glass strip cleaning method, the decoating liquid includes five that mass fraction is 3% to 10% The neopelex that water sodium metasilicate and mass fraction are 1% to 3%.
Preferably, in above-mentioned glass strip cleaning method, the decoating liquid further include mass fraction be 0.5% to 1.5% EDTA-2NA.
Preferably, in above-mentioned glass strip cleaning method, the cleaning solution includes five that mass fraction is 3% to 10% The neopelex that water sodium metasilicate and mass fraction are 1% to 3%.
Preferably, in above-mentioned glass strip cleaning method, the cleaning solution further include mass fraction be 0.5% to 1.5% EDTA-2NA.
Preferably, in above-mentioned glass strip cleaning method, the range of first preset temperature is 65 DEG C to 75 DEG C.
Preferably, in above-mentioned glass strip cleaning method, the range of second preset temperature is 50 DEG C to 55 DEG C.
It is preferably, described that the glass is scrubbed in above-mentioned glass strip cleaning method are as follows:
The hair for being 280r/min to 380r/min using revolving speed on the 3D purl machine that linear speed is 2.5m/min to 3m/min Brush scrubs the glass.
Preferably, in above-mentioned glass strip cleaning method, the range of the third preset temperature is 45 DEG C to 55 DEG C.
A kind of glass decoating liquid provided by the invention, metasilicate pentahydrate sodium, quality including mass fraction for 3% to 10% The EDTA-2NA that the neopelex and mass fraction that score is 1% to 3% are 0.5% to 1.5%.
As can be seen from the above description, above-mentioned glass strip cleaning method and glass decoating liquid provided by the invention, due to this Method is including the use of the decoating liquid comprising metasilicate pentahydrate sodium and neopelex with the first preset temperature to glass Glass carries out main strip, continues preset time;Include metasilicate pentahydrate sodium and detergent alkylate using with the second preset temperature The cleaning solution of sodium sulfonate scrubs the glass;The glass is carried out using the deionized water with third preset temperature Spray cleaning;Dewatered drying is carried out to the glass, therefore can be avoided and the ink after exposure development is damaged, and is produced It is at low cost, high production efficiency.
Detailed description of the invention
In order to more clearly explain the embodiment of the invention or the technical proposal in the existing technology, to embodiment or will show below There is attached drawing needed in technical description to be briefly described, it should be apparent that, the accompanying drawings in the following description is only this The embodiment of invention for those of ordinary skill in the art without creative efforts, can also basis The attached drawing of offer obtains other attached drawings.
Fig. 1 is the schematic diagram of the first glass strip cleaning method provided by the embodiments of the present application.
Specific embodiment
Core of the invention thought is to provide a kind of glass strip cleaning method and glass decoating liquid, can be avoided to exposure Ink after photodevelopment damages, and production cost is low, high production efficiency.
Following will be combined with the drawings in the embodiments of the present invention, and technical solution in the embodiment of the present invention carries out clear, complete Site preparation description, it is clear that described embodiments are only a part of the embodiments of the present invention, instead of all the embodiments.It is based on Embodiment in the present invention, it is obtained by those of ordinary skill in the art without making creative efforts every other Embodiment shall fall within the protection scope of the present invention.
As shown in FIG. 1, FIG. 1 is the embodiment of the present application to mention for the first glass strip cleaning method provided by the embodiments of the present application The schematic diagram of the first the glass strip cleaning method supplied, this method comprises the following steps:
S1: the decoating liquid pair comprising metasilicate pentahydrate sodium and neopelex with the first preset temperature is utilized Glass carries out main strip, continues preset time;
Wherein, metasilicate pentahydrate sodium is main strip agent, and neopelex is wet cleaning grease, remaining be from Sub- water, first preset temperature are higher than room temperature.In general, the processing technology for the glass product that the program is directed to includes that product is clear It washes, NCVM (non-conducting vacuum plating), exposure, development, strip, cleaning and inspection is electroplated, and this programme is for strip therein The improvement carried out with cleaning process.
S2: the cleaning solution pair comprising metasilicate pentahydrate sodium and neopelex with the second preset temperature is utilized The glass is scrubbed;
The step is a kind of fool proof measure, it is therefore an objective to prevent film layer and not move back the occurrence of net.
S3: spray cleaning is carried out to the glass using the deionized water with third preset temperature;
It can be avoided the residual of cleaning solution in this way.
S4: dewatered drying is carried out to the glass.
Appearance test is carried out after drying, the product upchecked enters subsequent processing and carries out plated film.
As can be seen from the above description, the first glass strip cleaning method provided by the embodiments of the present application, due to including benefit Master is carried out to glass with the decoating liquid comprising metasilicate pentahydrate sodium and neopelex with the first preset temperature to move back Plating continues preset time;Include the clear of metasilicate pentahydrate sodium and neopelex using with second preset temperature Washing lotion scrubs the glass;Spray cleaning is carried out to the glass using the deionized water with third preset temperature; Dewatered drying is carried out to the glass, therefore can be avoided and injury will cause to the ink after exposure development, and production cost is low, High production efficiency.
Second of glass strip cleaning method provided by the embodiments of the present application is in the first above-mentioned glass strip cleaning side Further include following technical characteristic on the basis of method:
The decoating liquid includes the metasilicate pentahydrate sodium that mass fraction is 3% to 10% and mass fraction is 1% to 3% Neopelex.
It should be noted that remaining ingredient is deionized water.
The third glass strip cleaning method provided by the embodiments of the present application is in above-mentioned second of glass strip cleaning side Further include following technical characteristic on the basis of method:
The decoating liquid further includes the EDTA-2NA that mass fraction is 0.5% to 1.5%.
Wherein, EDTA-2NA is disodium ethylene diamine tetraacetate, is as complexing agent, if not adding this in mixed liquor Kind substance also has no effect on the realization of above scheme.
4th kind of glass strip cleaning method provided by the embodiments of the present application is in the first above-mentioned glass strip cleaning side Further include following technical characteristic on the basis of method:
The cleaning solution includes the metasilicate pentahydrate sodium that mass fraction is 3% to 10% and mass fraction is 1% to 3% Neopelex.
It should be noted that remaining ingredient is deionized water.
5th kind of glass strip cleaning method provided by the embodiments of the present application is in above-mentioned 4th kind of glass strip cleaning side Further include following technical characteristic on the basis of method:
The cleaning solution further includes the EDTA-2NA that mass fraction is 0.5% to 1.5%.
6th kind of glass strip cleaning method provided by the embodiments of the present application, be it is above-mentioned the first move back to the 5th kind of glass Plate cleaning method in it is any on the basis of, further include following technical characteristic:
The range of first preset temperature is 65 DEG C to 75 DEG C.
The range of first preset temperature not only can guarantee strip effect, but also can guarantee that ink is not injured, when described default Between may range from 8 minutes to 15 minutes, can guarantee in this time range strip it is enough thoroughly, and will not be to moving back Plating solution causes to waste.
7th kind of glass strip cleaning method provided by the embodiments of the present application, be it is above-mentioned the first move back to the 5th kind of glass Plate cleaning method in it is any on the basis of, further include following technical characteristic:
The range of second preset temperature is 50 DEG C to 55 DEG C.
In this temperature range, each ingredient in cleaning solution can play sufficiently strong activity, can play more preferable Cleaning action.
8th kind of glass strip cleaning method provided by the embodiments of the present application, be it is above-mentioned the first move back to the 5th kind of glass Plate cleaning method in it is any on the basis of, further include following technical characteristic:
It is described that the glass is scrubbed are as follows:
The hair for being 280r/min to 380r/min using revolving speed on the 3D purl machine that linear speed is 2.5m/min to 3m/min Brush scrubs the glass.
It should be noted that this is one of preferred embodiment, in fact, can also use nine other than 3D purl machine The cleaning of groove ultrasonic cleaning machine, is not intended to limit herein.
9th kind of glass strip cleaning method provided by the embodiments of the present application, be it is above-mentioned the first move back to the 5th kind of glass Plate cleaning method in it is any on the basis of, further include following technical characteristic:
The range of the third preset temperature is 45 DEG C to 55 DEG C.
The advantages of third preset temperature this temperature range of selection is to reduce cost, energy saving.
A kind of glass decoating liquid provided by the embodiments of the present application, the five water metasilicic acids for being 3% to 10% including mass fraction The EDTA-2NA that the neopelex and mass fraction that sodium, mass fraction are 1% to 3% are 0.5% to 1.5%.
Wherein, metasilicate pentahydrate sodium is main strip agent, and neopelex is wet cleaning grease, and EDTA-2NA is Disodium ethylene diamine tetraacetate is as complexing agent in mixed liquor, remaining is deionized water.Utilize this glass decoating liquid pair Glass carries out strip processing, can be avoided and damages to the ink after exposure development, and production cost is low, high production efficiency.
The foregoing description of the disclosed embodiments enables those skilled in the art to implement or use the present invention. Various modifications to these embodiments will be readily apparent to those skilled in the art, as defined herein General Principle can be realized in other embodiments without departing from the spirit or scope of the present invention.Therefore, of the invention It is not intended to be limited to the embodiments shown herein, and is to fit to and the principles and novel features disclosed herein phase one The widest scope of cause.

Claims (10)

1. a kind of glass strip cleaning method characterized by comprising
Using the decoating liquid with first preset temperature comprising metasilicate pentahydrate sodium and neopelex to glass into The main strip of row, continues preset time;
Using the cleaning solution comprising metasilicate pentahydrate sodium and neopelex with the second preset temperature to the glass Glass is scrubbed;
Spray cleaning is carried out to the glass using the deionized water with third preset temperature;
Dewatered drying is carried out to the glass.
2. glass strip cleaning method according to claim 1, which is characterized in that the decoating liquid includes that mass fraction is The neopelex that 3% to 10% metasilicate pentahydrate sodium and mass fraction is 1% to 3%.
3. glass strip cleaning method according to claim 2, which is characterized in that the decoating liquid further includes mass fraction For 0.5% to 1.5% EDTA-2NA.
4. glass strip cleaning method according to claim 1, which is characterized in that the cleaning solution includes that mass fraction is The neopelex that 3% to 10% metasilicate pentahydrate sodium and mass fraction is 1% to 3%.
5. glass strip cleaning method according to claim 4, which is characterized in that the cleaning solution further includes mass fraction For 0.5% to 1.5% EDTA-2NA.
6. glass strip cleaning method according to claim 1-5, which is characterized in that first preset temperature Range be 65 DEG C to 75 DEG C.
7. glass strip cleaning method according to claim 1-5, which is characterized in that second preset temperature Range be 50 DEG C to 55 DEG C.
8. glass strip cleaning method according to claim 1-5, which is characterized in that it is described to the glass into Row scrub are as follows:
The hairbrush pair for being 280r/min to 380r/min using revolving speed on the 3D purl machine that linear speed is 2.5m/min to 3m/min The glass is scrubbed.
9. glass strip cleaning method according to claim 1-5, which is characterized in that the third preset temperature Range be 45 DEG C to 55 DEG C.
10. a kind of glass decoating liquid, which is characterized in that metasilicate pentahydrate sodium, quality point including mass fraction for 3% to 10% The EDTA-2NA that the neopelex and mass fraction that number is 1% to 3% are 0.5% to 1.5%.
CN201711423676.1A 2017-12-25 2017-12-25 Glass deplating and cleaning method and glass deplating liquid Active CN109956681B (en)