WO2020175607A1 - 容器の金型装置および容器の製造方法 - Google Patents
容器の金型装置および容器の製造方法 Download PDFInfo
- Publication number
- WO2020175607A1 WO2020175607A1 PCT/JP2020/007959 JP2020007959W WO2020175607A1 WO 2020175607 A1 WO2020175607 A1 WO 2020175607A1 JP 2020007959 W JP2020007959 W JP 2020007959W WO 2020175607 A1 WO2020175607 A1 WO 2020175607A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- mold
- container
- preform
- die
- shape
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Ceased
Abstract
容器の金型装置は、容器の胴部の形状を規定する型空間を有する割型と、容器の底面の形状を規定する底型面を有し、割型に対し進退可能な底型部と、を備える。割型は、型空間の底部側に連絡されるとともに底型部を受ける底型受け部を有する。割型に対して底型部を型閉じしたときに、底型受け部の底型面に対向する面と底型面との間が、容器の径方向に突出する構造体の形状を規定する空間をなす。
Description
\¥02020/175607 1 卩(:17 2020 /007959 明 細 書
発明の名称 : 容器の金型装置および容器の製造方法
技術分野
[0001] 本発明は、 容器の金型装置および容器の製造方法に関する。
背景技術
[0002] 従来から、 容器の底部に、 例えば吊り具や脚部などの構造体が形成された 容器が種々提案されている (例えば、 特許文献 1〜 6参照) 。 この種の容器 の製造方法としては、 例えば、 ダイレクトブロー成形法やストレッチブロー 成形法が用いられうる。
[0003] ダイレクトブロー成形法で製造される容器は、 一般的にストレッチブロー 成形法で製造される容器と比べて美的外観や寸法精度等の面で劣る。 また、 ダイレクトブロー成形法によると、 ブロー成型後に容器に残存するバリの切 除やその切除面のトリミングといった後工程が必要になり、 廃棄される樹脂 の量も多い。 このような背景の下、 比較的に加工が困難な形状の容器であっ てもストレッチブロー成形法で製造したいという要望が高まっている。 先行技術文献
特許文献
[0004] 特許文献 1 :特開 2002— 355885号公報
特許文献 2 :特開 2005 - 1 69698号公報
特許文献 3 :特開 201 6-373 1 3号公報
特許文献 4 :特開 201 7 -5 1 2686号公報
特許文献 5 :特開平 8-244749号公報
特許文献 6 :米国特許第 9254604号明細書
発明の概要
発明が解決しようとする課題
[0005] ストレッチブロー成形法を適用して、 例えば、 径方向に突出する固形状の 構造体を容器の底面側に形成することは比較的困難であり、 さらなる工夫が
\¥0 2020/175607 2 卩(:171? 2020 /007959
要望されている。
課題を解決するための手段
[0006] 本発明の一態様に係る容器の金型装置は、 容器の胴部の形状を規定する型 空間を有する割型と、 容器の底面の形状を規定する底型面を有し、 割型に対 し進退可能な底型部と、 を備える。 割型は、 型空間の底部側に連絡されると ともに底型部を受ける底型受け部を有する。 割型に対して底型部を型閉じし たときに、 底型受け部の底型面に対向する面と底型面との間が、 容器の径方 向に突出する構造体の形状を規定する空間をなす。
[0007] 本発明の一態様に係る容器の製造方法は、 _の態様の容器の金型装置を用 いるものであって、 有底形状の加熱された樹脂製のプリフォームを割型の型 空間内に配置する工程と、 プリフォームを延伸ロッ ドで延伸させる工程と、 プリフォームに加圧流体を導入して、 底型受け部に膨出するように容器をブ 口一成形する工程と、 底型部を型閉じし、 膨出した容器の部位を底型受け部 と底型面で圧縮して容器に構造体を形成する工程と、 を有する。
発明の効果
[0008] 本発明によれば、 ストレッチブロー成形法を適用して、 径方向に突出する 固形状の構造体を底面側に有する容器を形成することができる。
図面の簡単な説明
[0009] [図 1] (八) は容器の正面図であり、 (巳) は容器の底面図であり、 (〇) は 容器の 1〇-1〇線断面図である。
[図 2]ブロー成形装置の構成を模式的に示すブロック図である。
[図 3] ( ) 、 (巳) は温度調整用金型の構成例を模式的に示す図である。
[図 4] (八) はブローキヤビティ割型および底型部の型開き位置における図で あり、 (巳) はブローキヤビティ割型の型閉じ位置 (底型部の上昇前) にお ける図であり、 (〇) はブローキヤビティ割型および底型部の型閉じ位置 ( 底型部の上昇後) における図である。
[図 5]ブローキヤビティ割型と底型部の型閉じ状態を示す拡大図である。
[図 6]第 1スぺーサー部材および底型部の構成例を示す分解斜視図である。
\¥0 2020/175607 3 卩(:171? 2020 /007959
[図 7]ブロー成形方法の工程を示すフローチヤートである。
[図 8]ブロー成形部での工程を示す図である。
[図 9]図 8の続きの図である。
[図 10]図 9の続きの図である。
[図 1 1]図 1 0の続きの図である。
[図 12]第 2実施形態の温度調整部における動作例を示す図である。
[図 13]第 2実施形態のブロー成形部における動作例を示す図である。
発明を実施するための形態
[0010] 以下、 本発明の実施形態について図面を参照して説明する。
実施形態では説明を分かり易くするため、 本発明の主要部以外の構造や要 素については、 簡略化または省略して説明する。 また、 図面において、 同じ 要素には同じ符号を付す。 なお、 図面において、 容器およびプリフォームの 厚さ、 形状などは模式的に示したもので、 実際の厚さや形状などを示すもの ではない。
[001 1] (第 1実施形態)
<容器の構成例>
まず、 図 1 を参照して、 本実施形態に係る樹脂製の容器 1 〇の構成例を説 明する。
図 1 (八) は容器 1 0の正面図であり、 図 1 (巳) は容器 1 0の底面図で あり、 図 1 (〇) は容器の 1〇-1〇線断面図である。 図 1 において容器の軸線方 向!-を矢印で示す。
[0012] 容器 1 0は、 例えば薬剤の輸液などに使用される容器であって、 後述する 有底円筒形状のプリフォーム 2 0からストレッチブロー成形法により製造さ れる。
容器 1 〇は、 正面視で略矩形状に形成された胴部 1 1 と、 胴部 1 1の上側 中央に形成されて容器 1 〇の出入口となる首部 1 2と、 胴部 1 1の下側中央 に形成されて底面側が閉塞されている底筒部 1 3とを有する。 底筒部 1 3の 底面には、 底筒部 1 3の径方向外側に張り出した構造体の一例である環状の
\¥0 2020/175607 4 卩(:171? 2020 /007959
フランジ 1 4が形成されている。 なお、 底筒部 1 3の底面部 1 3 3には後エ 程で輸液用の開口などが形成されてもよい。
[0013] 容器 1 0の材料は、 熱可塑性の合成樹脂であり、 容器 1 0の用途に応じて 適宜選択することができる。 具体的な材料の種類としては、 例えば、 巳丁 (ポリエチレンテレフタレート) 、 巳 (ポリエチレンナフタレート) 、
9 0 7 A (ポリシクロへキサンジメチレンテレフタレート) 、 7 r \ t a n (トライタン (登録商標) :イーストマンケミカル社製のコポリエステル)
、 (ポリプロピレン) 、 巳 (ポリエチレン) 、 〇 (ポリカーボネー 卜) 、
(ポリエーテルスルホン) 、 3 11 (ポリフエニルスルホン ) 、 (ポリスチレン) 、 〇〇 /〇〇〇 (環状オレフイン系ポリマー)
、 IV! IV!八 (ポリメタクリル酸メチル: アクリル) 、 1_八 (ポリ乳酸) な どが挙げられる。
[0014] <ブロー成形装置の説明 >
次に、 図 2を参照して容器 1 0を製造するためのブロー成形装置 1 0 0に ついて説明する。 図 2は、 ブロー成形装置 1 0 0の構成を模式的に示すブロ ック図である。 本実施形態のブロー成形装置 1 〇〇は、 プリフォーム 2 0を 室温まで冷却せずに射出成形時の保有熱 (内部熱量) を活用してブロー成形 するホッ トパリソン方式 (1ステージ方式とも称する) の装置である。
[0015] ブロー成形装置 1 0 0は、 射出成形部 1 1 0と、 温度調整部 1 2 0と、 ブ 口一成形部 1 3 0と、 取り出し部 1 4 0と、 搬送機構 1 5 0とを備える。 射 出成形部 1 1 〇、 温度調整部 1 2 0、 ブロー成形部 1 3 0および取り出し部 1 4 0は、 搬送機構 1 5 0を中心として所定角度 (例えば 9 0度) ずつ回転 した位置に配置されている。
[0016] 搬送機構 1 5 0は、 図 2の紙面垂直方向 ( 方向) の軸を中心に回転する 回転板 (不図示) を備える。 回転板には、 プリフォーム 2 0または容器 1 0 の首部を保持するネック型 1 5 1 (図 2では不図示) が、 所定角度ごとにそ れぞれ 1以上配置されている。 搬送機構 1 5 0は、 回転板を回転させること で、 ネック型 1 5 1で首部が保持されたプリフォーム 2 0 (または容器 1 0
\¥0 2020/175607 5 卩(:171? 2020 /007959
) を、 射出成形部 1 1 〇、 温度調整部 1 2 0、 ブロー成形部 1 3 0、 取り出 し部 1 4 0の順に搬送する。
[0017] 射出成形部 1 1 0は、 それぞれ図示を省略する射出キヤビティ型、 射出コ ア型を備え、 プリフォーム 2 0を製造する。 射出成形部 1 1 0には、 プリフ ォームの原材料である樹脂材料を供給する射出装置 1 1 2が接続されている 射出成形部 1 1 0においては、 上記の射出キヤビティ型、 射出コア型と、 搬送機構 1 5 0のネック型 1 5 1 とを型閉じしてプリフォーム形状の型空間 を形成する。 そして、 このようなプリフォーム形状の型空間内に射出装置 1 1 2から樹脂材料を流し込むことで、 射出成形部 1 1 0でプリフォーム 2 0 が製造される。
[0018] なお、 射出成形部 1 1 0の型開きをしたときにも、 搬送機構 1 5 0のネッ ク型 1 5 1は開放されずにそのままプリフォーム 2 0を保持して搬送する。 射出成形部 1 1 〇で同時に成形されるプリフォーム 2 0の数 (すなわち、 ブ 口一成形装置 1 〇〇で同時に成形できる容器 1 〇の数) は、 適宜設定できる
[0019] 温度調整部 1 2 0は、 プリフォーム 2 0を収容可能な温度調整用金型 (加 熱ポッ トまたは温調ポッ ト) 1 2 1 を有する。 温度調整部 1 2 0は、 温度調 整用金型 1 2 1 にプリフォーム 2 0を収容し、 射出成形部 1 1 0で製造され たプリフォーム 2 0の延伸部分 (胴部や底部) の温度を最終ブローに適した 温度 (例えば 巳丁で約 9 0〜 1 0 0 °〇、 で約 1 3 0〜 1 4 0 °〇 (約 1 3 5 °〇前後) ) に調整する。
[0020] 図 3 ( ) は、 温度調整用金型 1 2 1の構成例を模式的に示す図である。
温度調整用金型 1 2 1は、 プリフォーム 2 0の首部より下の部分 (胴部お よび底部) を収容する空間を有する。 温度調整用金型 1 2 1 に対しては、 プ リフォーム 2 0の軸方向にプリフォーム 2 0を外部から加熱する複数のヒー 夕 1 2 2 3、 1 2 2匕が配置されている。
そのため、 各々のヒータ 1 2 2 3、 1 2 2 13の温度を変化させることで、
\¥0 2020/175607 6 卩(:171? 2020 /007959
プリフォーム 2 0の温度を軸方向に変化させることができる。 本実施形態で は、 首部側のヒータ 1 2 2 3の底部側のヒータ 1 2 2 13よりも高い温度に設 定される。 なお、 プリフォーム 2 0の内側の中空部に加熱ロッ ド (不図示) を非接触で挿入し、 プリフォーム 2 0を内外同時に温度調整 (加熱または冷 却) してもよい。
[0021 ] ここで、 温度調整用金型 1 2 1は、 その内部に所定温度 (例えば 4 0〜 8 〇°〇) の温調媒体を循環的に流通させる温調回路 (ヒータ (温調媒体流通回 路) ) を内蔵した構造としても構わない。 より好適には、 図 3 (巳) に示す ように、 温度調整用金型を、 温調回路 (ヒータ (温調媒体流通回路) 1 2 2 1 2 2匕) を内蔵した一対の割型 (1 2 1 3、 1 2 1 6) により構成し 、 プリフォーム 2 0を収容する空間の上方のみ拡径させた形状とさせるのが 望ましい。 さらに、 プリフォーム 2 0を収容する空間の深さ (長さ) は、 プ リフォーム 2 0の長さと略同一に設定され、 例えば、 プリフォーム 2 0の長 さに対して〇. 9 5 ~ 1 . 1 0倍、 好ましくは 1 . 0 ± 0 . 0 2倍に設定さ れているのが望ましい。 図 3 (巳) に示す温度調整用金型 1 2 1 3、 1 2 1 匕を用いてプリフォーム 2 0を予備ブロー (温度調整部 1 2 0における圧縮 エアによる延伸処理) することにより、 プリフォーム 2 0は温度調整用金型 1 2 1の内面に接触して温度調整される。 このとき、 プリフォーム 2 0の胴 部上方のみが拡径 (延伸) されて薄肉になり容器 1 0の形状に近づく一方、 胴部下方や底部はほとんど拡径されずに射出成形部 1 1 0と略同等の厚さが 維持される。 これにより、 良好な品質 (外観や肉厚分布 (物性) ) の容器 1 0が最終ブロー (ブロー成形部 1 3 0における圧縮エアおよび延伸ロッ ドに よる延伸処理) で製造可能になる。 つまり、 温度調整用金型 1 2 1でプリフ ォーム 2 0を予備ブローすることにより、 プリフォーム 2 0の温度や内部熱 量、 肉厚の分布状況を好適に調整できる。 具体的には、 最終ブローで膨張さ れるプリフォーム 2 0において、 環状のフランジ 1 4が形成される底部側に 好適に肉を残すことが可能になる。
[0022] ブロー成形部 1 3 0は、 温度調整部 1 2 0で温度調整されたプリフォーム
\¥0 2020/175607 7 卩(:171? 2020 /007959
2 0に対してブロー成形を行い、 容器 1 0を製造する。
ブロー成形部 1 3 0は、 容器 1 0の形状に対応するブロー成形金型 1 3 1 と、 プリフオーム 2 0を延伸させる延伸ロッ ド 1 3 2と、 ブローノズル (不 図示) と、 後述の底型部 6 0を昇降させる昇降機構 1 3 3と、 を備えている
[0023] 図 4を参照して、 ブロー成形金型 1 3 1の構成例を説明する。 図 4 (八) はブローキヤビティ割型および底型部の型開き位置における図であり、 図 4 (B) はブローキヤビティ割型の型閉じ位置 (底型部の上昇前) における図 であり、 図 4 (〇 はブローキヤビティ割型および底型部の型閉じ位置 (底 型部の上昇後) における図である。
[0024] ブロー成形金型 1 3 1は、 一対のブローキヤビティ割型 4 0 , 4 0と、 一 対の収容部 (ブローキヤビティ固定板) 5 0 , 5 0と、 底型部 6 0と、 を備 えている。
[0025] ブローキヤビティ割型 4 0 , 4 0は、 フランジ 1 4を除いた容器 1 0の主 要部 (胴部 1 1および底筒部 1 3) の形状を規定する型空間 3を有する型材 である。 ブローキヤビティ割型 4 0 , 4 0は、 図 4 (八) の上下方向 ( 方 向) に沿ったパーティング面で分割され、 図 4 (八) の左右方向 (X方向) に開閉可能に構成される。
[0026] ブローキヤビティ割型 4 0 , 4 0において容器の型空間 3の下側には、 底 型部 6 0を受ける底型受け部 4 1が形成されている。 底型受け部 4 1は、 型 空間 3において容器 1 0の底筒部 1 3の底部側と連絡し、 その内径が底筒部 1 3よりも広い円筒形状の空間を有している。 底型受け部 4 1の下側は開口 されており、 ブローキヤビティ割型 4 0 , 4 0の下側から底型部 6 0を揷入 可能である。
[0027] 底型受け部 4 1で型空間 3と連絡している上側の段差部分には、 一対の第
1スぺーサー部材 4 2 , 4 2がそれぞれブローキヤビティ割型 4 0 , 4 0に 交換可能に取り付けられている。 一対の第 1スぺーサー部材 4 2 , 4 2は、 後述の図 5に示すように半割円筒形状である。
\¥0 2020/175607 8 卩(:171? 2020 /007959
—対の第 1スぺーサー部材 4 2 , 4 2は、 ブローキヤビティ割型 4 0 , 4 0 とパーティング面が一致するようにボルト (不図示) などを用いてブローキ ヤビティ割型 4 0 , 4 0にそれぞれ取り付けられる。
[0028] —対の第 1スぺーサー部材 4 2 , 4 2は、 型閉じしたときに円筒形状をな す。 第 1 スぺーサー部材 4 2 , 4 2の内周面は、 容器 1 0のフランジ 1 4の 突出量 (図 5に示すフランジの径寸法幅 0) やフランジ 1 4の外周形状を規 定する。 なお、 本実施形態でのフランジ 1 4の形状は円形である。
[0029] 一対の収容部 5 0 , 5 0は、 ブローキヤビティ割型 4 0 , 4 0を隔てて配 置され、 それぞれ対応するブローキヤビティ割型 4 0を収容する。 また、 収 容部 5 0は、 ブローキヤビティ割型 4 0 , 4 0の開閉機構 (不図示) と接続 され、 ブローキヤビティ割型 4 0 , 4 0を図 4 (八) の左右方向 (X方向) に移動させる。
また、 図 4 (八) の収容部 5 0は底型部 6 0の昇降を許容する空間を備え ている。
[0030] 底型部 6 0は、 ブローキヤビティ割型 4 0 , 4 0の下側に配置され、 容器
1 〇の底面の形状を規定する型材である。 底型部 6 0は、 図 4 (巳) 、 (〇 ) に示すようにブロー成形装置 1 0 0の昇降機構 1 3 3と連結され、 型閉じ したブローキヤビティ割型 4 0 , 4 0に対して昇降により進退可能である。
[0031 ] 図 5は、 ブローキヤビティ割型 4 0 , 4 0と底型部 6 0の型閉じ状態を示 す拡大図である。 図 6は、 第 1スぺーサー部材 4 2 , 4 2および底型部 6 0 の構成例を示す分解斜視図である。
[0032] 底型部 6 0は、 底型本体 6 1 と、 位置決めリング部材 6 2と、 割リング状 の押さえ部材 6 3と、 第 2スぺーサー部材 6 4と、 ストッパー部材 6 5とを 有する。
[0033] 底型本体 6 1は、 昇降機構 1 3 3との連結部を有し、 底型部 6 0の組立状 態において昇降機構 1 3 3からの力を受ける部材である。 底型本体 6 1は、 一端側から他端側に向けて外径が段階的に大きくなる段付の円筒形であり、 大径部 6 1 3と小径部 6 1 匕を有している。 底型本体 6 1 において、 大径部
\¥0 2020/175607 9 卩(:171? 2020 /007959
6 1 3と小径部 6 1 匕をつなぎ円周形状をなす段差面 6 1 〇には複数のボル 卜穴が開口されている。 大径部 6 1 3の外周には、 押さえ部材 6 3を受ける 溝 6 1 ㊀が周方向に沿って環状をなすように形成されている。
[0034] また、 小径部 6 1 匕の径寸法は、 第 1スぺーサー部材 4 2 , 4 2の内径に 対応する寸法に設定され、 底型本体 6 1の小径部 6 1 匕を第 1スぺーサー部 材 4 2 , 4 2の内側に揷入することが可能である。 底型本体 6 1の小径部 6 1 匕の先端は、 型空間 3および底型受け部 4 1の上面 4 1 3に臨む底型面 6 1 をなしている。 本実施形態において底型面 6 1 の形状は平坦である。 底型部 6 0が上昇した状態では、 底型受け部 4 1の上面 4 1 3と底型本体 6 1の底型面 6 1 との間でプリフォーム 2 0が圧縮され、 これにより容器 1 0のフランジ 1 4が成形される。
[0035] 位置決めリング部材 6 2は、 型閉じされたブローキヤビティ割型 4 0 , 4 〇に対し、 底型部 6 0を位置決めするための部材である。 位置決めリング部 材 6 2の外径は、 底型受け部 4 1の内径に対応する寸法に設定され、 底型部 6 0が昇降するときには位置決めリング部材 6 2の外周面が底型受け部 4 1 の内周面と接触するように構成される。
[0036] また、 位置決めリング部材 6 2の内径は、 底型本体 6 1の大径部 6 1 3の 外径に対応する寸法に設定され、 位置決めリング部材 6 2の厚さは、 底型本 体 6 1の大径部 6 1 3の高さに対応する寸法に設定される。 そのため、 位置 決めリング部材 6 2の下端は、 底型本体 6 1の大径部 6 1 3の外周に支持さ れる。 また、 位置決めリング部材 6 2の上端は、 底型本体 6 1の外周に形成 された溝 6 1 6に嵌合した割リング状の押さえ部材 6 3で押さえられ、 上下 方向の動きが規制される。
[0037] 第 2スぺーサー部材 6 4は、 リング状部材であり、 厚さの異なる部材に交 換可能である。 第 2スぺーサー部材 6 4の内径は、 底型本体 6 1の小径部 6 1 匕の径に対応する寸法に設定される。 また、 第 2スぺーサー部材 6 4には 、 底型本体 6 1のボルト穴と対応する位置に揷通穴が設けられている。
[0038] 第 2スぺーサー部材 6 4は、 底型本体 6 1の小径部 6 1 匕に揷入され、 底
\¥0 2020/175607 10 卩(:171? 2020 /007959
型本体 6 1の段差面 6 1 〇に当接された状態で固定される。
また、 第 2スぺーサー部材 6 4は、 底型部 6 0が上昇した状態における底 型面 6 1 の位置を調整するために用いられる。 第 2スぺーサー部材 6 4の 厚さを調整することで、 底型部 6 0が上昇した状態において、 図 5に示す底 型受け部 4 1の上面 4 1 3と底型部 6 0の底型面 6 1 との間隔が変化し、 容器 1 0のフランジ 1 4の厚さ寸法 (図 5に示す厚さ丁) を調整することが できる。
[0039] ストッパー部材 6 5は、 樹脂製のリング状部材である。 ストッパー部材 6
5の内径は、 底型本体 6 1の小径部 6 1 匕の径に対応する寸法に設定される 。 そのため、 ストッパー部材 6 5は、 底型本体 6 1の小径部 6 1 匕に揷入可 能である。 また、 ストッパー部材 6 5には、 底型本体 6 1のボルト穴と対応 する位置に揷通穴が設けられている。
[0040] 図 5に示すように、 ストッパー部材 6 5は、 底型本体 6 1の段差面 6 1 〇 との間で第 2スぺーサー部材 6 4を挟み込むように配置される。 ストッパー 部材 6 5は、 底型部 6 0が上昇したときにブローキヤビティ割型 4 0の底型 受け部 4 1 と接触し、 底型部 6 0の損傷を防ぐ機能を担う。
[0041 ] 底型部 6 0を組み立てるときには、 底型本体 6 1の大径部 6 1 3に位置決 めリング部材 6 2を挿入し割リング状の押さえ部材 6 3で固定した後、 底型 本体 6 1の小径部 6 1 匕に、 第 2スぺーサー部材 6 4と、 ストッパー部材 6 5を取り付ける。 そして、 揷通穴を揷通するように配置されたボルト 6 6を 、 ボルト穴に螺合することで底型部 6 0の各部材が固定される。
[0042] ここで、 ブローキヤビティ割型 4 0 , 4 0に取り付けられる一対の第 1 ス ぺーサー部材 4 2 , 4 2と、 底型本体 6 1の形状を変更することで、 容器 1 0のフランジ 1 4の形状を変更することが可能である。 また、 底型部 6 0の 第 2スぺーサー部材 6 4を変更することで、 容器 1 0のフランジ 1 4の厚さ を調整することが可能である。 さらに、 底型部 6 0において底型本体 6 1の 底型面 6 1 の形状を変更することで、 例えば、 容器 1 0の底筒部 1 3の底 面形状を変えることができる。
\¥0 2020/175607 1 1 卩(:171? 2020 /007959
[0043] 図 2に戻って、 取り出し部 1 4 0は、 ブロー成形部 1 3 0で製造された容 器 1 0の首部 1 2をネック型 1 5 1から開放し、 容器 1 0をブロー成形装置 1 0 0の外部へ取り出すように構成されている。
[0044] <ブロー成形方法の説明 >
次に、 本実施形態のブロー成形装置 1 0 0によるブロー成形方法について 説明する。 図 7は、 ブロー成形方法の工程を示すフローチヤートである。
[0045] まず、 射出成形部 1 1 0において、 射出キヤビティ型、 射出コア型および ネック型 1 5 1で形成された型空間に射出装置 1 1 2から樹脂を射出し、 有 底円筒形状のプリフォーム 2 0が製造される (ステップ 3 1 0 1) 。
[0046] 続いて、 搬送機構 1 5 0の回転板が所定角度回転し、 射出成型時の保有熱 を含んだ状態のプリフォーム 2 0が温度調整部 1 2 0に搬送される。 温度調 整部 1 2 0においては、 プリフォーム 2 0の温度を最終ブローに適した温度 に近づけるための温度調整が行われる (ステップ 3 1 0 2) 。
[0047] ここで、 温度調整部 1 2 0の温度調整用金型 1 2 1 においては、 軸方向に 配置された複数のヒータ 1 2 2 3、 1 2 2 13の温度差により、 プリフォーム 2 0の胴部では首部側が底部側よりも高い温度に加熱される。 そのため、 温 度調整後のプリフォーム 2 0の胴部の温度は首部側が底部側よりも高くなる
[0048] 続いて、 搬送機構 1 5 0の回転板が所定角度回転し、 温度調整されたプリ フォーム 2 0がブロー成形部 1 3 0に搬送される。
ブロー成形部 1 3 0においてプリフォーム 2 0が所定の位置に配置される と、 図 8に示すように、 ブローキヤビティ割型 4 0 , 4 0が型閉じされる ( ステップ 3 1 0 3) 。 図 8に示す状態において、 底型部 6 0は昇降機構 1 3 3と連結されるが、 底型部 6 0の位置は、 ブローキヤビティ割型 4 0 , 4 0 に対して下方に退避した位置にある。
[0049] その後、 図 9に示すように、 プリフォーム 2 0内に延伸ロッ ド 1 3 2が揷 入され、 延伸ロッ ド 1 3 2の下降により、 プリフォーム 2 0が鉛直方向のみ に僅かに延伸される (ステップ 3 1 0 4) 。
\¥0 2020/175607 12 卩(:171? 2020 /007959
[0050] 続いて、 図 1 0に示すように、 プリフォーム 2 0内に、 ブローノズルから 加圧流体の一例であるブローエアーが導入される。 同時に、 延伸ロッ ド 1 3 2も更に下降される。 これにより、 底型受け部 4 1 に膨出するようにプリフ 才ーム 2 0が容器 1 0にブロー成形される (ステップ 3 1 0 5) 。 このとき のブローキヤビティ割型 4 0 , 4 0の温度は、 6 0 °〇以上に設定することが 好ましい。 なお、 最終ブロー成形において、 プリフォーム 2 0を加圧する媒 体は空気に限定されることなく、 空気以外の気体や水等の液体を加圧媒体と してもよい。
[0051 ] ここで、 ホッ トパリソン方式のブロー成形では、 プリフォーム 2 0の保有 する内部熱量 (保有熱) が大きいほどプリフォーム 2 0が変形しやすくなる 。 上記のように、 温度調整後のプリフォーム 2 0の胴部の温度は首部側が底 部側よりも高くなり、 プリフォーム 2 0の胴部では首部側が底部側よりも内 部熱量が大きくなる。 すなわち、 プリフォーム 2 0の胴部は、 首部側の方が 底部側よりも内部熱量が大きいので変形しやすい。
[0052] したがって、 プリフォーム 2 0にブローエアーが導入されると、 プリフォ —ム 2 0の胴部では内部熱量の大きい首部側が先行して延伸され、 内部熱量 の小さい底部側が遅れて延伸される。 これにより、 プリフォーム 2 0の底部 側が過剰に延伸されなくなり、 容器 1 〇の底筒部 1 3の底面側に肉が残りや すくなる。
[0053] このブロー成形時に延伸ロッ ド 1 3 2を上昇させた後、 底型部 6 0が 方 向に移動して上昇し、 図 1 1 に示すように、 容器 1 0の底筒部 1 3の底面側 から膨出した部分が底型部 6 0に押圧される。 このときの底型部 6 0の温度 は、 6 0 °〇以上に設定することが好ましい。 なお、 簡単のため、 図 1 1では 延伸ロッ ド 1 3 2の図示は省略している。
そうすると、 図 5に示す底型受け部 4 1の上面 4 1 3、 第 1スぺーサー部 材 4 2 , 4 2の内周面、 底型本体 6 1の底型面 6 1 との間でプリフォーム 2 0が圧縮される。 これにより、 容器 1 0の底筒部 1 3の底面が平坦に加工 されるとともに、 底筒部 1 3の底面にフランジ 1 4が形成される (ステップ
\¥0 2020/175607 13 卩(:171? 2020 /007959
3 1 0 6) 〇
[0054] 容器 1 0のフランジ 1 4の成形が終了すると、 容器 1 0からブローエアー の排気と延伸ロッ ド 1 3 2の引き抜き (さらなる上昇) が行われ、 ブローキ ャビティ割型 4 0 , 4 0および底型部 6 0が型開きされる (ステップ 3 1 0 7) 。 これにより、 ブロー成形後の容器 1 0が移動可能となる。
[0055] 続いて、 搬送機構 1 5 0の回転板が所定角度回転し、 容器 1 0が取り出し 部 1 4 0に搬送される。 取り出し部 1 4 0において、 容器 1 0の首部 1 2が ネック型 1 5 1から開放され、 容器 1 0がブロー成形装置 1 〇〇の外部へ取 り出される (ステップ3 1 0 8) 。
以上で、 ブロー成形方法の一連の工程が終了する。 その後、 搬送機構 1 5 0の回転板を所定角度回転させることで、 上記の 3 1 0 1から 3 1 0 8の各 工程が繰り返される。
[0056] 本実施形態によれば、 プリフォーム 2 0を延伸ロッ ド 1 3 2で延伸させて 容器 1 〇をブロー成形し、 その後に底型部 6 0を型閉じして底型受け部 4 1 に膨出した容器 1 0の部位を底型受け部 4 1の上面 4 1 3、 底型部 6 0の底 型面 6 1 で圧縮する。 これにより、 ストレッチブロー成形法で成形された 容器 1 〇の底面側に、 径方向に突出する固形状の構造体 (フランジ 1 4) を 形成することができる。
[0057] また、 本実施形態においては、 第 1スぺーサー部材 4 2 , 4 2、 底型本体
6 1、 第 2スぺーサー部材 6 4を交換することで、 容器 1 0に形成される固 形状の構造体の形状 (厚さ、 幅および形状) を変更することができる。 その ため、 例えば、 各々の構造体が異なっている複数種類の容器 1 〇を少量多品 種生産するときにも容易に対応できる。
[0058] (第 2実施形態)
第 2実施形態は、 第 1実施形態の変形例であって、 容器 1 0の底筒部 1 3 においてフランジ 1 4を除く底面部 1 3 3に薄膜状の部位を形成する例を説 明する。
なお、 第 2実施形態の説明では、 第 1実施形態と同様の要素には同一符号
\¥0 2020/175607 14 卩(:171? 2020 /007959
を付し、 重複説明はいずれも省略する。
[0059] 第 2実施形態では、 温度調整部 1 2 0での温度調整工程と、 ブロー成形部
1 3 0でのブロー成形工程が、 以下のように第 1実施形態と相違する。
[0060] 図 1 2 ( ) 〜 (〇 は、 第 2実施形態の温度調整部 1 2 0における動作 例を示す図である。
図 1 2 (八) は、 ネック型 1 5 1 に保持されて搬送されるプリフォーム 2 0を示している。 プリフォーム 2 0の底部には、 射出成形時のホッ トランナ —のゲート痕であるゲート部 2 1がプリフォーム 2 0の外側に突出するよう に形成されている。
[0061 ] 図 1 2 (巳) は、 プリフォーム 2 0が温度調整用金型 1 2 1 に収容された 状態を示している。 第 2実施形態の温度調整用金型 1 2 1は、 図 3 (巳) に 示す割型 1 2 1 3、 1 2 1 匕と同様である。 ただし、 第 2実施形態の温度調 整用金型 1 2 1は、 プリフォーム 2 0のゲート部 2 1 に臨む底部中央の部分 に空気の逃げ穴がなく、 温度調整用金型 1 2 1の底部中央の部分はプリフォ —ム 2 0の底部形状に倣った曲面である点で図 3 (巳) の例と相違する。
[0062] 第 2実施形態において、 プリフォーム 2 0が温度調整用金型 1 2 1 に収容 されると、 プリフォーム 2 0のゲート部 2 1は、 温度調整用金型 1 2 1の底 部中央の曲面と接触する。 温度調整部 1 2 0でのプリフォーム 2 0は射出成 形時の保有熱を有し、 変形しやすい状態にある。 そのため、 温度調整用金型 1 2 1 に接触したゲート部 2 1は温度調整用金型 1 2 1の底部の曲面に倣っ て変形しうる。 ただし、 図 1 2 (巳) においても、 プリフォーム 2 0の底部 中央にはゲート部 2 1の樹脂が残り、 比較的に厚肉の状態にある。
[0063] プリフォーム 2 0が温度調整用金型 1 2 1 に収容された後、 図 1 2 (巳) に示すように、 プリフォーム 2 0の底部に向けて加熱ロッ ド 1 2 3がプリフ ォーム 2 0内に挿入される。 加熱ロッ ド 1 2 3は、 少なくともその先端部よ り上方側にヒータが内蔵され加熱されている。 図 1 2 (〇 に示すように、 加熱ロッ ド 1 2 3はプリフォーム 2 0の底部中央を内側から押圧する。 する と、 加熱ロッ ド 1 2 3の先端部と温度調整用金型 1 2 1の間でプリフォーム
\¥0 2020/175607 15 卩(:171? 2020 /007959
2 0が挟み込まれ、 挟み込まれた部分の樹脂が周囲に逃げてプリフォーム 2 〇の底部中央が薄肉となる。 以上のようにして、 温度調整部 1 2 0において 、 プリフォーム 2 0の底部中央の肉厚を周囲よりも薄くすることができる。 また、 上述の挟み込み処理の前または後にプリフォーム 2 0を予備ブローし て、 プリフォーム 2 0を胴部上方が拡径して胴部下方や底部が拡径していな い形状に変形させるのが望ましい。 さらに、 予備ブローされたプリフォーム 2 0は所定時間、 温度調整用金型 1 2 1 と加熱ロッ ド 1 2 3により、 内外同 時に温度調整させるのが好ましい。 これにより、 プリフォーム 2 0に対し、 最終ブローに適した肉厚分布と温度分布が付与できる。
その後、 上記のプリフォーム 2 0は、 ブロー成形部 1 3 0に搬送される。
[0064] 図 1 3 (八) 、 (巳) は、 第 2実施形態のブロー成形部 1 3 0における動 作例を示す図である。
第 2実施形態のブロー成形部 1 3 0の動作は、 図 7の 3 1 0 3 ~ 3 1 0 6 の工程 (図 8〜図 1 1) までは第 1実施形態と同様である。
[0065] ステップ 3 1 0 6で底筒部 1 3の底面にフランジ 1 4が形成された後、 図
1 3 (八) に示すように、 延伸ロッ ド 1 3 2が底型部 6 0に向けて降下する 。 そして、 図 1 3 (巳) に示すように、 延伸ロッ ド 1 3 2と底型部 6 0の底 型面 6 1 との間で容器 1 0の底面部 1 3 3が挟み込まれて押圧変形する。 これにより、 容器 1 0の底面部 1 3 8の中央に、 周囲より肉厚の薄い薄膜状 の部位が形成される。
[0066] その後、 図 7の 3 1 0 7の工程と同様に、 延伸ロッ ド 1 3 2の引き抜きが 行われ、 ブローキヤビティ割型 4 0 , 4 0および底型部 6 0が型開きされる 。 これにより、 ブロー成形部 1 3 0から容器 1 0が移動可能となる。
[0067] 第 2実施形態のブロー成形部 1 3 0では、 容器 1 0の底面側にフランジ 1 4を形成した後に、 延伸ロッ ド 1 3 2と底型部 6 0の間で容器 1 0の底面部 1 3 3を押圧変形させて、 底面部 1 3 3に周囲より肉厚の薄い薄膜状の部位 を形成する。 これにより、 後工程において底面部 1 3 3の薄膜状の部位に穿 刺等で輸液用の開口などを形成しやすくなり、 容器 1 〇の使いやすさを一層
\¥0 2020/175607 16 卩(:171? 2020 /007959
向上させることができる。
[0068] 第 2実施形態の温度調整部 1 2 0では、 加熱ロッ ドと温度調整用金型 1 2
1 によってプリフォーム 2 0のゲート部 2 1 を挟み込み、 ゲート部 2 1の樹 脂を周囲に移動させてプリフォーム 2 0の底部中央を予め薄肉にしている。 これにより、 容器 1 0の底面部 1 3 3に薄膜状の部位を形成するときの加工 性が向上し、 容器 1 0の歩留まりを向上させることができる。
[0069] 本発明は、 上記実施形態に限定されることなく、 本発明の趣旨を逸脱しな い範囲において、 種々の改良並びに設計の変更を行ってもよい。
[0070] 例えば、 上記実施形態での容器 1 0はあくまで一例にすぎず、 本発明の容 器の全体形状は種々変更することができる。 また、 フランジ 1 4の外周形状 は、 円形に限定されず、 例えば多角形や歯車状であってもよい。 また、 容器 1 0の底部側に形成される固形状の構造体はフランジに限定されることなく 、 例えば、 円柱、 多角柱、 円錐、 多角錐、 円錐台、 多角錐台、 半球あるいは これらの形状を組み合わせた任意の形状の構造体を形成することができる。 また、 容器 1 0の底面形状は平坦面に限定されることなく、 適宜変更するこ とが可能である。
[0071 ] 加えて、 今回開示された実施形態は、 全ての点で例示であって制限的なも のではないと考えられるべきである。 本発明の範囲は、 上記した説明ではな くて特許請求の範囲によって示され、 特許請求の範囲と均等の意味及び範囲 内での全ての変更が含まれることが意図される。 符号の説明
[0072] 1 〇 容器、 1 1 胴部、 1 2 首部、 1 3 底筒部、 1 4 フランジ、 2 〇 プリフォーム、 2 1 ゲート部、 4〇 ブローキヤビティ割型、 4 1 底型受け部、 4 2 第 1スぺーサー部材、 6 0 底型部、 6 1 底型本体、
6 底型面、 6 4 第 2スぺーサー部材、 1 0 0 ブロー成形装置、 1 1 〇 射出成形部、 1 2 0 温度調整部、 1 2 1 温度調整用金型、 1 2 2 8、 1 2 2 13 ヒータ、 1 2 3 加熱ロッ ド、 1 3 0 ブロー成形部、 1 3 1 ブロー成形金型、 1 3 2 延伸ロッ ド、 1 3 3 昇降機構、 1 4 0 取
\¥0 2020/175607 17 卩(:17 2020 /007959
り出し部、 1 5 0 搬送機構
Claims
[請求項 1 ] 容器の胴部の形状を規定する型空間を有する割型と、
前記容器の底面の形状を規定する底型面を有し、 前記割型に対し進 退可能な底型部と、 を備え、
前記割型は、 前記型空間の底部側に連絡されるとともに前記底型部 を受ける底型受け部を有し、
前記割型に対して前記底型部を型閉じしたときに、 前記底型受け部 の前記底型面に対向する面と前記底型面との間が、 前記容器の径方向 に突出する構造体の形状を規定する空間をなす
容器の金型装置。
[請求項 2] 前記割型の前記底型受け部の内周には、 前記構造体の径方向の突出 量または前記構造体の外周形状を規定する第 1スぺ _サ_部材が交換 可能に取り付けられる
請求項 1 に記載の容器の金型装置。
[請求項 3] 前記底型部は、 前記型閉じしたときの前記底型面の位置を調整し、 前記構造体の厚さを規定する第 2スぺ _サ_部材の取付部を有する 請求項 1 または請求項 2に記載の容器の金型装置。
[請求項 4] 請求項 1から請求項 3のいずれか 1項に記載の容器の金型装置を用 いた容器の製造方法であって、
有底形状の加熱された樹脂製のプリフォームを前記割型の前記型空 間内に配置する工程と、
前記プリフォームを延伸ロッ ドで延伸させる工程と、
前記プリフォームに加圧流体を導入して、 前記底型受け部に膨出す るように容器をブロー成形する工程と、
前記底型部を型閉じし、 前記膨出した容器の部位を前記底型受け部 と前記底型面で圧縮して前記容器に前記構造体を形成する工程と、 を 有する
容器の製造方法。
\¥0 2020/175607 19 卩(:171? 2020 /007959
[請求項 5] 前記プリフォームを射出成形する工程と、
射出成型後の保有熱を含む前記プリフォームを加熱して温度調整す る工程と、 をさらに有する
請求項 4に記載の容器の製造方法。
[請求項 6] 前記温度調整のときに、 前記プリフォームの胴部の首部側が底部側 よりも高い温度に加熱される
請求項 5に記載の容器の製造方法。
[請求項 7] 前記構造体を形成した後に、 前記延伸ロッ ドと前記底型面で容器底 面部を挟み込み、 容器底面部に薄膜状の部位を形成する工程をさらに 有する
請求項 5または請求項 6に記載の容器の製造方法。
[請求項 8] 前記温度調整のときに、 前記プリフォームを収容する第 1部材と前 記プリフォーム内に挿入される第 2部材によって、 前記プリフォーム の底部に形成されるゲート部が挟み込まれて潰される 請求項 7に記載の容器の製造方法。