WO2019223106A1 - Contact coating lip structure and extrusion coating head thereof - Google Patents
Contact coating lip structure and extrusion coating head thereof Download PDFInfo
- Publication number
- WO2019223106A1 WO2019223106A1 PCT/CN2018/097865 CN2018097865W WO2019223106A1 WO 2019223106 A1 WO2019223106 A1 WO 2019223106A1 CN 2018097865 W CN2018097865 W CN 2018097865W WO 2019223106 A1 WO2019223106 A1 WO 2019223106A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- contact
- coating
- coating lip
- substrate
- contact coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Ceased
Abstract
Description
技术领域Technical field
本发明涉及一种挤压涂布头的改进,尤其是一种接触式涂布唇结构及其挤压涂布头。The invention relates to an improvement of an extrusion coating head, in particular to a contact coating lip structure and an extrusion coating head thereof.
背景技术Background technique
现有的湿料挤压涂布,如锂电池电极材料的涂布,分为非接触式涂布和接触式涂布两大类。所谓非接触式涂布是指涂布头悬在基材上方,浆料从涂布头的狭缝被挤压出来后,靠自由落体的方式落到基材上,非接触式涂布具有涂布精度高(涂布精度包括但不限于厚度,均匀性等指标)的优点,其缺点是非接触式涂布只能在有背辊的情况下才可能涂布,无背辊时是无法涂布的。Existing wet material extrusion coating, such as coating of lithium battery electrode materials, is divided into two categories: non-contact coating and contact coating. The so-called non-contact coating means that the coating head is suspended above the substrate, the slurry is squeezed out of the slit of the coating head, and then falls on the substrate by free falling. The non-contact coating has coating The advantage of high cloth accuracy (including but not limited to thickness, uniformity and other indicators). The disadvantage is that non-contact coating can only be applied with a back roller, and it cannot be applied without a back roller. of.
所谓接触式涂布(如图1所示)是指挤压涂布头的一侧涂布唇100的唇部较另一侧涂布唇(200)的唇部长,其具有长的唇部的涂布唇100与基材300相接触,浆料从涂布头的狭缝400被挤压出来后,顺着较长的涂布唇100的唇部110外侧面流到基材300上被带走,形成涂布层。接触式涂布头由于浆料从涂布头的狭缝被挤压出来后是顺着较长的唇部外侧面流到基材上的,一直以来,受较长的唇部外侧面的表面光洁度,以及涂布唇的材料等因素的影响,其涂布精度没有非接触式的涂布精度高。但是,它的优点是可以在无背辊的情况下实现涂布。The so-called contact coating (as shown in FIG. 1) refers to that the lip portion of the coating lip 100 on one side of the extrusion coating head is longer than the lip portion of the coating lip (200) on the other side. The coating lip 100 is in contact with the substrate 300. After the slurry is squeezed out from the slit 400 of the coating head, it flows along the outer surface of the lip 110 of the longer coating lip 100 to the substrate 300 and is taped. Walk to form a coating layer. Because the contact coating head is squeezed out from the slit of the coating head, it flows along the outer surface of the longer lip to the substrate. The coating accuracy is not as high as the non-contact coating accuracy due to factors such as the finish and the material of the coating lip. However, it has the advantage that it can be applied without a back-up roll.
所在,现状是要想涂布精度高,就要采用非接触式涂布方式与背辊配合使用;但是,有些情况下,如受空间的限制无法安装背辊时,只能牺牲质量选择接触式涂布。Where it is, the status quo is to use a non-contact coating method with the back roll to achieve high coating accuracy; however, in some cases, if the back roll cannot be installed due to space constraints, the quality can only be sacrificed for the contact Coated.
发明内容Summary of the invention
针对现有技术的以上缺陷或改进需求,本发明提供了一种利用接触式涂布方式,可以达到非接触式的涂布效果的接触式涂布唇结构及其挤压涂布头。Aiming at the above defects or improvement needs of the prior art, the present invention provides a contact coating lip structure and a squeeze coating head that can achieve a non-contact coating effect by using a contact coating method.
本发明的技术方案是:提供一种接触式涂布唇结构,包括接触式涂布唇主体,所述接触式涂布唇主体的一侧面为浆料流动面,在所述接触式涂布唇主体的远离所述流动面的一侧设有接触部,所述接触部被设置成所述接触部的底面与基材相接触后,所述浆料流动面的下底悬在所述基材的上方,使浆料流出时呈自由状态流出。The technical solution of the present invention is to provide a contact coating lip structure, which includes a contact coating lip body. One side of the contact coating lip body is a slurry flow surface. A contact portion is provided on a side of the main body remote from the flow surface, and the contact portion is provided so that a bottom of the slurry flow surface is suspended on the substrate after the bottom surface of the contact portion contacts the substrate. Above, the slurry flows out in a free state when it flows out.
作为对本发明的改进,所述接触部是远离所述下底与所述接触式涂布唇主体的凸块。As an improvement to the present invention, the contact portion is a bump away from the lower bottom and the contact-type coating lip body.
作为对本发明的改进,所述凸块的底面是平面。As an improvement to the present invention, the bottom surface of the bump is flat.
作为对本发明的改进,所述凸块的底面是弧面。As an improvement to the present invention, the bottom surface of the bump is a curved surface.
作为对本发明的改进,所述接触式涂布唇主体和接触部是一体成型的。As an improvement to the present invention, the contact coating lip body and the contact portion are integrally formed.
作为对本发明的改进,所述接触式涂布唇主体和接触部是耐磨材料制成的。As an improvement to the present invention, the contact coating lip body and the contact portion are made of a wear-resistant material.
本发明还提供一种挤压涂布头,包括两个相对而设的接触式涂布唇主体,两个接触式涂布唇主体中的一个为上述的接触式涂布唇结构。The present invention also provides a squeeze coating head, which includes two contact coating lip bodies arranged opposite to each other, and one of the two contact coating lip bodies is the above-mentioned contact coating lip structure.
本发明由于采用了在所述接触式涂布唇主体的远离所述流动面的一侧设有接触部,所述接触部被设置成所述接触部的底面与基材相接触后,所述浆料流动面的下底悬在所述基材的上方,使浆料流出时呈自由状态流出的结构,这样,在无背辊涂布时,其接触部的底面可以与基材相接触,达到背辊稳定基材的作用,同时,涂布头的浆料出口悬在基材上方,并且浆料流出时呈自由状态流出,与非接触式的涂布效果一样,这样,就达到用接触式涂布的方式,达到了非接触式的涂布效果的目的。According to the present invention, a contact portion is provided on a side of the contact-type coating lip body that is far from the flow surface, and the contact portion is provided so that a bottom surface of the contact portion is in contact with a substrate. The bottom of the slurry flow surface is suspended above the substrate, so that the slurry flows out in a free state when the slurry flows out. In this way, when coating without a back roll, the bottom surface of the contact portion can contact the substrate. To achieve the role of the back roll to stabilize the substrate, at the same time, the slurry outlet of the coating head is suspended above the substrate, and the slurry flows out in a free state when the slurry flows out. The coating method achieves the purpose of non-contact coating effect.
附图说明Brief description
图1是现有的接触式涂布头的实施例的剖视结构示意图;FIG. 1 is a schematic cross-sectional structure diagram of an embodiment of a conventional contact coating head;
图2是本发明的接触式涂布唇结构第一种实施例的剖视结构示意图;FIG. 2 is a cross-sectional structural diagram of a first embodiment of a contact coating lip structure of the present invention;
图3是本发明的接触式涂布唇结构第二种实施例的剖视结构示意图;FIG. 3 is a cross-sectional structural diagram of a second embodiment of the contact coating lip structure of the present invention;
图4是图3所示实施例的外观结构示意图。FIG. 4 is a schematic diagram of the appearance structure of the embodiment shown in FIG. 3.
图5是图4所示实施例的一种使用状态结构示意图;FIG. 5 is a schematic diagram of a use state structure of the embodiment shown in FIG. 4;
图6是图3所示实施例的一种使用状态结构示意图;FIG. 6 is a schematic diagram of a use state structure of the embodiment shown in FIG. 3;
图7是图3所示实施例的另一种使用状态结构示意图。FIG. 7 is a schematic diagram of another use state structure of the embodiment shown in FIG. 3.
具体实施方式Detailed ways
下面结合具体案例对本发明进行说明。The present invention is described below with reference to specific cases.
请参见图2,图2揭示的是本发明的接触式涂布唇结构的第一种实施例;本实施例提供的一种接触式涂布唇结构,包括接触式涂布唇主体1,所述接触式涂布唇主体1的一侧面为浆料流动面11,在所述接触式涂布唇主体1的远离所述流动面11的一侧设有接触部12,所述接触部12被设置成所述接触部12的底面121与基材2相接触后,所述浆料流动面11的下底111悬在所述基材2的上方,使浆料流出时呈自由状态流出。本实施例中,所述接触部12是远离所述下底111与所述接触式涂布唇主体1的凸块;所述凸块的底面121是平面。所述接触式涂布唇主体1和接触部12是一体成型的;所述接触式涂布唇主体1和接触部12是耐磨材料制成的。Please refer to FIG. 2. FIG. 2 discloses a first embodiment of a contact coating lip structure according to the present invention; a contact coating lip structure provided in this embodiment includes a contact coating lip body 1. One side of the contact coating lip body 1 is a slurry flow surface 11, and a contact portion 12 is provided on a side of the contact coating lip body 1 remote from the flow surface 11. The contact portion 12 is After the bottom surface 121 of the contact portion 12 is in contact with the substrate 2, the lower bottom 111 of the slurry flow surface 11 is suspended above the substrate 2 so that the slurry flows out in a free state when the slurry flows out. In this embodiment, the contact portion 12 is a bump away from the lower bottom 111 and the contact-type coating lip body 1; a bottom surface 121 of the bump is a flat surface. The contact coating lip body 1 and the contact portion 12 are integrally formed; the contact coating lip body 1 and the contact portion 12 are made of a wear-resistant material.
本实施例配上第二接触式涂布唇主体3就可以构成一个完整的挤压式涂布头,当本实施例垂直向下或斜向向下向基材2上涂布时,接触部12的底面121抵在基材2的前进方向的前面部位,可以起到背辊稳定基材2不产生抖动的作用,同时,涂布头的浆料出口悬在基材2上方,并且浆料流出时呈自由状态流出(即不受传统的接触式涂布唇的延长部的任何影响),与非接触式的涂布效果一样,这样,就达到用接触式涂布的方式,达到了非接触式的涂布效果的目的。This embodiment can be combined with a second contact-type coating lip body 3 to form a complete squeeze-type coating head. When this embodiment is applied vertically or obliquely down onto the substrate 2, the contact portion The bottom surface 121 of 12 abuts on the front part of the substrate 2 in the advancing direction, and can play the role of the back roll to stabilize the substrate 2 without jitter. At the same time, the slurry outlet of the coating head is suspended above the substrate 2 and the slurry When flowing out, it flows out freely (that is, it is not affected by the extension of the traditional contact coating lip). It has the same effect as non-contact coating. In this way, the contact coating method is used to achieve non- Purpose of contact coating effect.
请参见图3,图3揭示的是本发明的接触式涂布唇结构的第二种实施例;本实施例提供的一种接触式涂布唇结构,包括接触式涂布唇主体1,所述接触式涂布唇主体1的一侧面为浆料流动面11,在所述接触式涂布唇主体1的远离所述流动面11的一侧设有接触部12,所述接触部12被设置成所述接触部12的底面121与基材2相接触后,所述浆料流动面11的下底111悬在所述基材2的上方,使浆料流出时呈自由状态流出。本实施例中,所述接触部12是远离所述下底111与所述接触式涂布唇主体1的凸块;所述凸块的底面121是弧面,弧面接触不易刮伤基材2。所述接触式涂布唇主体1和接触部12是一体成型的;所述接触式涂布唇主体1和接触部12是耐磨材料制成的。Please refer to FIG. 3. FIG. 3 discloses a second embodiment of the contact coating lip structure of the present invention; a contact coating lip structure provided in this embodiment includes a contact coating lip body 1. One side of the contact coating lip body 1 is a slurry flow surface 11, and a contact portion 12 is provided on a side of the contact coating lip body 1 remote from the flow surface 11. The contact portion 12 is After the bottom surface 121 of the contact portion 12 is in contact with the substrate 2, the lower bottom 111 of the slurry flow surface 11 is suspended above the substrate 2 so that the slurry flows out in a free state when the slurry flows out. In this embodiment, the contact portion 12 is a bump away from the lower bottom 111 and the contact coating lip body 1; the bottom surface 121 of the bump is an arc surface, and the substrate is not easily scratched by the arc surface contact 2. The contact coating lip body 1 and the contact portion 12 are integrally formed; the contact coating lip body 1 and the contact portion 12 are made of a wear-resistant material.
本实施例配上第二接触式涂布唇主体3就可以构成一个完整的挤压式涂布头,当本实施垂直向下向基材2上涂布时,可以起到无背辊涂布,其接触部12的底面121可以与基材2相接触,达到背辊稳定基材2的作用,同时,涂布头的浆料出口悬在基材上方,并且浆料流出时呈自由状态流出(即不受传统的接触式涂布唇的延长部的任何影响),与非接触式的涂布效果一样,这样,就达到用接触式涂布的方式,达到了非接触式的涂布效果的目的。This embodiment can be combined with a second contact coating lip body 3 to form a complete extrusion coating head. When this embodiment is applied vertically downward to the substrate 2, it can be used without back roller coating. The bottom surface 121 of the contact portion 12 can be in contact with the substrate 2 to achieve the role of the back roll to stabilize the substrate 2. At the same time, the slurry outlet of the coating head is suspended above the substrate, and the slurry flows out in a free state when the slurry flows out. (That is, it is not affected by the extension of the traditional contact coating lip). It has the same effect as the non-contact coating. In this way, the contact coating method is achieved and the non-contact coating effect is achieved. the goal of.
请参见图4,图4是图3所示实施例的外观结构示意图。从图4可以看出,所述接触式涂布唇主体1的浆料流动面11与基材2之间的面夹角α可以在30度至90度之间选择,也就是说,由包含有接触式涂布唇主体1和第二接触式涂布唇主体3构成的涂布头可以与基材的前进方向斜向布置,也可以与基材的前进方向垂直布置,都可以起到非接触式涂布的效果。Please refer to FIG. 4, which is a schematic diagram of an appearance structure of the embodiment shown in FIG. 3. It can be seen from FIG. 4 that the surface angle α between the slurry flowing surface 11 of the contact coating lip body 1 and the substrate 2 can be selected between 30 degrees and 90 degrees, that is, by including The coating head composed of the contact coating lip main body 1 and the second contact coating lip main body 3 can be arranged obliquely to the advancing direction of the substrate, or it can be arranged perpendicular to the advancing direction of the substrate. The effect of contact coating.
请参见图5,图5是图4所示实施例的一种使用状态结构示意图;从图可以看出,基材2可以水平走向外,基材2还可以垂直走向。显然,基材也可以斜着走向(参见图7)。Please refer to FIG. 5. FIG. 5 is a schematic diagram of a structure of a state of use in the embodiment shown in FIG. 4. As can be seen from the figure, the substrate 2 can go horizontally and the substrate 2 can go vertically. Obviously, the substrate can also run diagonally (see Figure 7).
图6是图3所示实施例的一种使用状态结构示意图;图6所示实施例中的基材2是垂直走向的;图7中的基材2是斜着走向的。FIG. 6 is a schematic view of a structure of a use state of the embodiment shown in FIG. 3; the substrate 2 in the embodiment shown in FIG. 6 is vertically oriented; the substrate 2 in FIG. 7 is oriented diagonally.
本发明还提供一种挤压涂布头,包括两个相对而设的接触式涂布唇主体1、3,两个接触式涂布唇主体1、3中的一个为上述的接触式涂布唇结构。The invention also provides a squeeze coating head, which includes two contact coating lip bodies 1, 3 arranged opposite to each other, and one of the two contact coating lip bodies 1, 3 is the above-mentioned contact coating. Lip structure.
本领域的技术人员容易理解,以上所述仅为本发明的较佳实施例而已,并不用以限制本发明,凡在本发明的精神和原则之内所作的任何修改、等同替换和改进等,均应包含在本发明的保护范围之内。 Those skilled in the art can easily understand that the above description is only the preferred embodiments of the present invention and is not intended to limit the present invention. Any modification, equivalent replacement, and improvement made within the spirit and principle of the present invention, All should be included in the protection scope of the present invention.
Claims (1)