US8995A - Improvement in processes for preparing oakum - Google Patents
Improvement in processes for preparing oakum Download PDFInfo
- Publication number
- US8995A US8995A US8995DA US8995A US 8995 A US8995 A US 8995A US 8995D A US8995D A US 8995DA US 8995 A US8995 A US 8995A
- Authority
- US
- United States
- Prior art keywords
- junk
- oakum
- improvement
- preparing
- processes
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Description
nurse firn'rns JOHN A. GORMAOK AND GEO. OORMAOK,.OF NEXV YORK, N. Y. i. I
uwenovetwe nr lN successes FOR PREPARING- ,o AKuM.
Specification forming part of Letters Patent No. 8.995, dated Julie 8, 1852.
ment of what is termed junk or old tarred,
ropes, whereby we are enabled to manufacture a superior qualitv of oakum; and we hereby declare that the following is a full, clear, and exact description of the same.
The nature of our invention consists in the treatment of junk or tarred ropes and such like materials in an aqueous solution of sulphuric or muriatic acid, which solution or solutions impart to the oakum manufactured from the junk new and useful qualities not obtained by any other process heretofore known or practiced.
To enable others skilled in the art to use our in vention,we will proceed to describe the same in all its details.
We take a large vessel made of wood or iron capable of containing water, and we fill it up with water, allowing the quantity to be such as will cover entirely the amount ot'junk which we desire to steep in it, whatever that amount of junk maybe. Ne have no prescribed size of vessel or quantity of junk. The water we employ is from 75 to 100 Fahrenheit. This we have found to be the best temperature; but we do not confine ourselves to any specific temperature. To the quantity of water in the vessel spoken of we add about one per cent. of the common sulphuric acid found at drug gists stores, and then stir itnp'well, sons to mix it thoroughly with the water. The junk which'we design to operate upon is then placed in the vessel in the acidulated solution orliquid and allowed to steep for fifteen or twenty minutes, after which it is taken out and treated in the common'way. We sometimes use more than one per cent. of sulphuric acid to.
the water. Th tion to the qua to be operated on.
iount required is in propority of tar in thejunk which is The greater' the quantity of tar in the junk the greater is the quantity ofacid required. About three per cent. of the acid to the water is the strongestsolution we employ. There is some junk which does not require to be steeped but for a very short time, and when there is but very little tar in the said junk it is suflicient for our purpose only to rinse it in the acidulated liquid. Those skilled in the art will be able to judge by inspection of the quantity of vitriol required, the heat of the liquor, and the time the junk is required to be steeped or merely to be rinsed in the liquor. Muriatic, nitric, and acetic aoidsmay be employed as substitutes for the sulphuric acid; but the sulphuric is the best and cheapest. We do not confine ourselves to the exact mechanical operations, the acidulous solution or mixture of water and acid being the principle of ourinvention and improvement. he effect of the acidulous solution upon the junk is the production ofa tannin in thejunk formed by the combination of the acid and the tar in thejunk. The application of the acid in the aqueous solution tends to distribute the tar more evenly through the fibers of the material, and thus the-tannin is-very equally precipitated among the fibers of thejunk. The oakum produced by this process or application of the ucidulous liquor is very beautiful in comparison with any ever manufactured before, and it has far greater preservative qualities. Junk, after it is rendered'fibrous or reduced from old tarred ropes mto a fibrous state, is named oakum. To bring the common junk into a state of oakum it hasto'be teased and. the fibers are separated with great difficulty. The acid liquor renders the fibers of the junk far easier of separatiomand thus it eoonomizes labor. When common junk is placed in heaps it is liable to heat or ferment, and sometimes Our spontaneous combustion is the result. improvement obviates these evils.
lu'liot weather the tar in thejunk gets soft, and then the fibers of it are separated (picked) with great difficulty. Our improvement removes this evil, and allows the junk 'to be picked with great ease.
Oakuln is employed for spun yarn, and our invention renders it softer than that made by the common process, andthus it can be spun with greater freedom and facility. The result therefore of our invention is a new, useful, and superior product or manufacture.
The principle of the invention is the employment of the acidulous liquor to the junk which produces a vulcanizin g effect upon the oakum, makes it stronger, more durable, enables it to stand the'vgeather better, to be more easily ing it in acidulousliquor, as described, forlhe v operated and brought from a state of junk topurpose hereinset forth.
that of oakum, and to be=easierspun after it JOHN A. (JORMAOK.
is rendered into oakum. GEORGE COBMAOK.
Having thus described our invention, we W'itnesses':
claim-- v 0. D. MUNN,
The treatment of junk by steeping. o r rins- S..H. WALES.