UA43351U - Способ выплавки стали в основной мартеновской печи - Google Patents
Способ выплавки стали в основной мартеновской печиInfo
- Publication number
- UA43351U UA43351U UAU200903040U UAU200903040U UA43351U UA 43351 U UA43351 U UA 43351U UA U200903040 U UAU200903040 U UA U200903040U UA U200903040 U UAU200903040 U UA U200903040U UA 43351 U UA43351 U UA 43351U
- Authority
- UA
- Ukraine
- Prior art keywords
- smelting
- steel
- hearth furnace
- basic open
- furnace
- Prior art date
Abstract
Способ выплавки стали в основной мартеновской печи включает завалку металлического лома, известняка, возвратного конвертерного шлака и других известьсодержащих материалов, окислителей, плавление и доводку. В период доводки и (или) завалки используют брикеты из извести фракций до , при этом максимальный размер брикета составляет 0,02- от глубины ванны печи до уровня основных порогов. Затрата брикетов не превышает 80 % от суммы всех шлакообразующих материалов, которые вводят в печь в соответствующий период плавки.
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| UAU200903040U UA43351U (ru) | 2009-03-31 | 2009-03-31 | Способ выплавки стали в основной мартеновской печи |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| UAU200903040U UA43351U (ru) | 2009-03-31 | 2009-03-31 | Способ выплавки стали в основной мартеновской печи |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| UA43351U true UA43351U (ru) | 2009-08-10 |
Family
ID=50633747
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| UAU200903040U UA43351U (ru) | 2009-03-31 | 2009-03-31 | Способ выплавки стали в основной мартеновской печи |
Country Status (1)
| Country | Link |
|---|---|
| UA (1) | UA43351U (ru) |
-
2009
- 2009-03-31 UA UAU200903040U patent/UA43351U/ru unknown
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Kirschen et al. | Energy efficiency and the influence of gas burners to the energy related carbon dioxide emissions of electric arc furnaces in steel industry | |
| CN103361461B (zh) | 一种转炉冶炼低碳钢磷含量在线预测控制方法 | |
| Holtzer et al. | The recycling of materials containing iron and zinc in the OxyCup process | |
| WO2013012039A9 (ja) | 溶銑の精錬方法 | |
| CN111139332A (zh) | 一种造渣料与轻薄废钢混合加工入炉工艺 | |
| CN104451023A (zh) | 一种留用转炉热渣的冶炼方法 | |
| RU2003119684A (ru) | Брикет для выплавки металла | |
| UA43351U (ru) | Способ выплавки стали в основной мартеновской печи | |
| RU2594996C2 (ru) | Способ выплавки стали в кислородном конвертере | |
| RU2548871C2 (ru) | Способ прямого получения металла из содержащих оксиды железа материалов (варианты) и устройство для его осуществления | |
| KR20120132909A (ko) | 전기로에서의 용강 탈린제 및 탈린 방법 | |
| CN102212641A (zh) | 一种快速成渣的方法 | |
| UA91879C2 (ru) | СПОСОБ выплавки стали в мартеновской печи | |
| UA96638C2 (ru) | СПОСОБ ПЕРЕРАБОТКИ ЦИНК-железосодержащих отходов металлургического производства | |
| RU2007123043A (ru) | Способ выплавки стали в дуговой электросталеплавильной печи | |
| Pal et al. | Refining of hot metal utilizing fluxed iron oxide pellets | |
| CN105219918A (zh) | 降低钢液中磷元素含量的电弧炉炼钢方法 | |
| Feng et al. | Study on refining process for improvement of cleanliness of high carbon steel. | |
| UA50147U (ru) | Способ выплавки стали в основной мартеновской печи | |
| RU2380429C1 (ru) | Способ передела низкомарганцовистого чугуна в конвертере с предварительным нагревом лома | |
| UA38416U (ru) | Способ выплавки стали в основной мартеновской печи | |
| Park et al. | Flux Optimization During Tapping in BOF Process | |
| Smirnov | Optimization of technology for desulfurization of steel in plant of ladle furnace. | |
| MY157863A (en) | A method for separating metallic iron from oxide | |
| UA78622U (ru) | СПОСОБ десульфурации чугуна на литейном ДВОРЕ ДОМЕННОЙ ПЕЧИ |