TW200606107A - Method for nickel and cobalt recovery from laterite ores by reaction with concentrated acid and water leaching - Google Patents
Method for nickel and cobalt recovery from laterite ores by reaction with concentrated acid and water leachingInfo
- Publication number
- TW200606107A TW200606107A TW094121431A TW94121431A TW200606107A TW 200606107 A TW200606107 A TW 200606107A TW 094121431 A TW094121431 A TW 094121431A TW 94121431 A TW94121431 A TW 94121431A TW 200606107 A TW200606107 A TW 200606107A
- Authority
- TW
- Taiwan
- Prior art keywords
- nickel
- reaction
- laterite ores
- concentrated acid
- water leaching
- Prior art date
Abstract
A process for leaching laterite ores containing limonite and saprolite in a two stage process. The first stage consisting of mixing and reacting the ore with concentrated mineral acid, and the second stage consisting of preparing a slurry of the acid/ore mixture in water and leaching the mixture to dissolve nickel and cobalt. Iron is efficiently separated from nickel and cobalt in the solid leach residue primarily as an oxide or hydroxide of ferric iron other than jarosite.
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US58324304P | 2004-06-28 | 2004-06-28 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| TW200606107A true TW200606107A (en) | 2006-02-16 |
Family
ID=35781546
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| TW094121431A TW200606107A (en) | 2004-06-28 | 2005-06-27 | Method for nickel and cobalt recovery from laterite ores by reaction with concentrated acid and water leaching |
Country Status (13)
| Country | Link |
|---|---|
| US (1) | US20060002835A1 (en) |
| EP (1) | EP1784516A4 (en) |
| JP (1) | JP2008504439A (en) |
| KR (1) | KR20070053211A (en) |
| CN (1) | CN100410399C (en) |
| AU (1) | AU2005256213A1 (en) |
| BR (1) | BRPI0512430A (en) |
| CA (1) | CA2571492A1 (en) |
| DO (1) | DOP2005000119A (en) |
| GT (1) | GT200500177A (en) |
| TW (1) | TW200606107A (en) |
| WO (1) | WO2006000098A1 (en) |
| ZA (1) | ZA200700592B (en) |
Families Citing this family (39)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP1971697B1 (en) * | 2006-01-10 | 2012-07-25 | Murrin Murrin Operations Pty Ltd | Hematite precipitation |
| CA2640122A1 (en) * | 2006-01-31 | 2007-08-09 | Murrin Murrin Operations Pty Ltd | Improved base metal recovery process from heap leaching |
| WO2007095689A1 (en) * | 2006-02-24 | 2007-08-30 | Murrin Murrin Operations Pty Ltd | Hematite precipitation at elevated temperature and pressure |
| WO2008003160A1 (en) * | 2006-07-03 | 2008-01-10 | Curlook Enterprises Inc. | Metal recovery system as applied to the high pressure leaching of limonitic nickel laterite ores |
| AU2011218755B9 (en) * | 2006-09-06 | 2014-05-15 | Eramet | Process for the hydrometallurgical treatment of a lateritic nickel/cobalt ore and process for producing nickel and/or cobalt intermediate concentrates or commercial products using it |
| FR2905383B1 (en) * | 2006-09-06 | 2008-11-07 | Eramet Sa | PROCESS FOR THE HYDROMETALLURGICAL TREATMENT OF A NICKEL ORE AND LATERITE COBALT, AND PROCESS FOR PREPARING INTERMEDIATE CONCENTRATES OR COMMERCIAL NICKEL AND / OR COBALT PRODUCTS USING THE SAME |
| US7901484B2 (en) | 2007-08-28 | 2011-03-08 | Vale Inco Limited | Resin-in-leach process to recover nickel and/or cobalt in ore leaching pulps |
| AP2010005222A0 (en) | 2007-09-14 | 2010-04-30 | Barrick Gold Corp | Process for recovering platinum group metals usingreductants |
| FI120943B (en) * | 2008-02-19 | 2010-05-14 | Norilsk Nickel Finland Oy | Method for the separation of zinc, iron, calcium, copper and manganese from aqueous cobalt and / or nickel solutions |
| FI121180B (en) * | 2008-11-03 | 2010-08-13 | Outotec Oyj | A method for treating nickel plater ore |
| CN102227509A (en) * | 2008-11-28 | 2011-10-26 | Bhp比利通Ssm开发有限公司 | Method for separating limonite and saprolite |
| CN101619400B (en) * | 2009-08-05 | 2011-03-09 | 江西稀有稀土金属钨业集团有限公司 | Method for extracting cobalt and nickel from nickel laterite |
| FI122030B (en) | 2009-09-24 | 2011-07-29 | Norilsk Nickel Finland Oy | Recovery of nickel and cobalt from laterite |
| FI123646B (en) | 2010-02-25 | 2013-08-30 | Outotec Oyj | Method for streamlining solid-particle liquid separation in connection with leaching of laterites |
| FI123054B (en) * | 2010-12-17 | 2012-10-15 | Outotec Oyj | Method of separating nickel from a low nickel material |
| US8597601B2 (en) * | 2011-06-03 | 2013-12-03 | Vale S.A. | Selective base metals leaching from laterite ores |
| CN103131855A (en) * | 2011-11-29 | 2013-06-05 | 沈阳有色金属研究院 | Method for treating normal pressure leaching of transitional nickel laterite ore |
| KR101359121B1 (en) * | 2011-12-28 | 2014-02-06 | 재단법인 포항산업과학연구원 | Method for Reducing Waste in Nickel Smelting Process |
| WO2014047672A1 (en) * | 2012-09-28 | 2014-04-03 | Direct Nickel Pty Ltd | Method for the recovery of metals from nickel bearing ores and concentrates |
| CN103710542B (en) * | 2014-01-13 | 2016-01-27 | 中国恩菲工程技术有限公司 | Class iron ore concentrate and preparation method thereof |
| US10112842B2 (en) * | 2014-11-18 | 2018-10-30 | Alliance Magnésium | Process to produce magnesium compounds, and various by-products using sulfuric acid in a HCl recovery loop |
| CN104651610A (en) * | 2014-12-31 | 2015-05-27 | 金川集团股份有限公司 | Method for recovering nickel, cobalt, iron, silicon and magnesium from laterite-nickel ores |
| CN104611548A (en) * | 2014-12-31 | 2015-05-13 | 金川集团股份有限公司 | Method for recovering nickel in low-grade laterite-nickel ore |
| CN104651609A (en) * | 2014-12-31 | 2015-05-27 | 金川集团股份有限公司 | Method for recovering nickel, cobalt and iron from laterite-nickel ores |
| JP6020971B2 (en) * | 2015-03-23 | 2016-11-02 | 住友金属鉱山株式会社 | Method for producing cobalt powder |
| CN104805310B (en) * | 2015-04-17 | 2016-08-24 | 北京矿冶研究总院 | Method for leaching cobalt from high-valence cobalt oxide-containing raw material |
| CN107312930B (en) * | 2017-07-07 | 2018-08-28 | 金川集团股份有限公司 | A kind of method that low nickel matte leaching solution pyrolysis removes iron |
| US11473170B2 (en) | 2017-09-25 | 2022-10-18 | Mohammad Asadrokht | Treatment of non-sulfidic nickeliferous resources and recovery of metal values therefrom |
| HUE059215T2 (en) * | 2017-12-21 | 2022-10-28 | Bhp Chile Inc | Water balance in a chloride heap leach |
| JP7042719B2 (en) * | 2018-06-21 | 2022-03-28 | 日揮グローバル株式会社 | Method for manufacturing nickel sulfate compound |
| CN109279665B (en) * | 2018-09-13 | 2020-09-25 | 郑忆依 | Treatment method of nickel cobalt lithium manganate ternary waste |
| CN109234526B (en) * | 2018-11-26 | 2020-11-03 | 中国恩菲工程技术有限公司 | Treatment method of laterite-nickel ore |
| CA3122864A1 (en) * | 2019-05-06 | 2020-11-12 | Chen Xia | Process and system for extraction of rare earth elements using an acid soak |
| CN111100985B (en) * | 2019-12-30 | 2021-05-18 | 荆门市格林美新材料有限公司 | A kind of comprehensive treatment method of sodium ammonium waste liquid applied to laterite nickel ore |
| AU2020428275A1 (en) * | 2020-02-14 | 2022-09-22 | Metso Finland Oy | Enhanced recovery of nickel and cobalt from laterites |
| JP7628014B2 (en) * | 2020-09-01 | 2025-02-07 | ピーティー. ハイドロテック メタル インドネシア | Process for recovering nickel, cobalt and other metals from lateritic nickel ore |
| CN113025832B (en) * | 2021-03-02 | 2022-07-15 | 重庆大学 | Method for extracting nickel from laterite nickel ore while mineralizing CO2 |
| CN113151677B (en) * | 2021-04-26 | 2022-09-09 | 赣州逸豪优美科实业有限公司 | Method for leaching cobalt intermediate product by sulfate without acid |
| CN115786602B (en) * | 2022-10-11 | 2024-04-09 | 中国恩菲工程技术有限公司 | Method for preparing hematite by using iron-aluminum slag |
Family Cites Families (17)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CA446289A (en) * | 1948-01-20 | S. Renzoni Louis | Purification of cobalt precipitates containing iron and other impurities | |
| US2899300A (en) * | 1959-08-11 | Method for extracting nickel from | ||
| US3093559A (en) * | 1958-06-20 | 1963-06-11 | Merwin G White | Treatment of lateritic ores |
| US3244513A (en) * | 1962-07-25 | 1966-04-05 | Sherritt Gordon Mines Ltd | Process for the treatment of lateritic ores to obtain cobalt and nickel values |
| US3793432A (en) * | 1972-01-27 | 1974-02-19 | D Weston | Hydrometallurgical treatment of nickel group ores |
| US4097575A (en) * | 1976-11-05 | 1978-06-27 | Amax Inc. | Roast-neutralization-leach technique for the treatment of laterite ore |
| US4125588A (en) * | 1977-08-01 | 1978-11-14 | The Hanna Mining Company | Nickel and magnesia recovery from laterites by low temperature self-sulfation |
| FI773588A7 (en) * | 1977-11-28 | 1979-05-29 | Outokumpu Oy | HYDROMETALLURGISK PROCESS FOER BEHANDLING AV OXIDER OCH FERRITER INNEHAOLLANDE JAERN OCH ANDRA METALLER |
| US5178666A (en) * | 1991-12-03 | 1993-01-12 | Inco Limited | Low temperature thermal upgrading of lateritic ores |
| USRE37251E1 (en) * | 1993-07-29 | 2001-07-03 | Cominco Engineering Services Ltd. | Chloride assisted hydrometallurgical extraction of metal |
| US5571308A (en) * | 1995-07-17 | 1996-11-05 | Bhp Minerals International Inc. | Method for recovering nickel from high magnesium-containing Ni-Fe-Mg lateritic ore |
| US6350420B1 (en) * | 1999-10-15 | 2002-02-26 | Bhp Minerals International, Inc. | Resin-in-pulp method for recovery of nickel and cobalt |
| US6379636B2 (en) * | 1999-11-03 | 2002-04-30 | Bhp Minerals International, Inc. | Method for leaching nickeliferous laterite ores |
| US6261527B1 (en) * | 1999-11-03 | 2001-07-17 | Bhp Minerals International Inc. | Atmospheric leach process for the recovery of nickel and cobalt from limonite and saprolite ores |
| US6312500B1 (en) * | 2000-03-30 | 2001-11-06 | Bhp Minerals International Inc. | Heap leaching of nickel containing ore |
| US6391089B1 (en) * | 2000-11-29 | 2002-05-21 | Walter Curlook | Acid leaching of nickel laterite ores for the extraction of their nickel and cobalt values |
| AUPS201902A0 (en) * | 2002-04-29 | 2002-06-06 | Qni Technology Pty Ltd | Modified atmospheric leach process for laterite ores |
-
2005
- 2005-06-27 BR BRPI0512430-1A patent/BRPI0512430A/en not_active IP Right Cessation
- 2005-06-27 CN CNB2005800284977A patent/CN100410399C/en not_active Expired - Fee Related
- 2005-06-27 EP EP05759184A patent/EP1784516A4/en not_active Withdrawn
- 2005-06-27 AU AU2005256213A patent/AU2005256213A1/en not_active Abandoned
- 2005-06-27 JP JP2007518426A patent/JP2008504439A/en active Pending
- 2005-06-27 WO PCT/CA2005/001003 patent/WO2006000098A1/en not_active Ceased
- 2005-06-27 US US11/166,125 patent/US20060002835A1/en not_active Abandoned
- 2005-06-27 TW TW094121431A patent/TW200606107A/en unknown
- 2005-06-27 KR KR20077002266A patent/KR20070053211A/en not_active Withdrawn
- 2005-06-27 CA CA 2571492 patent/CA2571492A1/en not_active Abandoned
- 2005-06-28 GT GT200500177A patent/GT200500177A/en unknown
- 2005-06-28 DO DO2005000119A patent/DOP2005000119A/en unknown
-
2007
- 2007-01-22 ZA ZA200700592A patent/ZA200700592B/en unknown
Also Published As
| Publication number | Publication date |
|---|---|
| CN100410399C (en) | 2008-08-13 |
| US20060002835A1 (en) | 2006-01-05 |
| AU2005256213A1 (en) | 2006-01-05 |
| CN101006190A (en) | 2007-07-25 |
| DOP2005000119A (en) | 2005-12-30 |
| ZA200700592B (en) | 2008-05-28 |
| JP2008504439A (en) | 2008-02-14 |
| KR20070053211A (en) | 2007-05-23 |
| EP1784516A1 (en) | 2007-05-16 |
| GT200500177A (en) | 2006-03-16 |
| CA2571492A1 (en) | 2006-01-05 |
| WO2006000098A1 (en) | 2006-01-05 |
| BRPI0512430A (en) | 2008-03-04 |
| EP1784516A4 (en) | 2008-07-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| TW200606107A (en) | Method for nickel and cobalt recovery from laterite ores by reaction with concentrated acid and water leaching | |
| Faris et al. | The direct leaching of nickel sulfide flotation concentrates–a historic and state-of-the-art review part I: Piloted processes and commercial operations | |
| CN101323909B (en) | A method of microwave selective reduction roasting-dilute acid leaching nickel oxide ore | |
| CN101338377B (en) | A high-efficiency leaching process for nickel in laterite nickel ore | |
| ATE256201T1 (en) | METHOD FOR LEACHING AT AMBIENT PRESSURE FOR EXTRACTION OF NICKEL AND COBALT FROM LIMONITE AND SAPROLITE ORES | |
| TW200607867A (en) | Method for nickel and cobalt recovery from laterite ores by combination of atmospheric and moderate pressure leaching | |
| CN102226232A (en) | Method for processing laterite-nickel ore | |
| CA2484134A1 (en) | Atmospheric pressure leach process for lateritic nickel ore | |
| CN101550483A (en) | Combined flow path processing method of laterite nickel | |
| CN111647742B (en) | Method for extracting nickel, cobalt and manganese from nickel-cobalt-manganese multi-metal oxide ore by wet process step by step | |
| CN101805828A (en) | Low-cost method for disposing red soil nickel ore | |
| AU2005248187B2 (en) | Method of recovering nickel or cobalt | |
| CN105568001A (en) | Combined high-pressure acid leaching method for cobalt alloy and oxide cobalt minerals | |
| WO2019035319A1 (en) | Leaching treatment method, and wet smelting method of nickel oxide ore | |
| CN101139656A (en) | Laterite nickel ore leaching method | |
| US3773891A (en) | Acid leaching of lateritic ores | |
| CN113735199A (en) | Method for preparing nickel sulfate from nickel iron | |
| Faris et al. | The Direct Leaching of Nickel Sulfide Flotation Concentrates–A Historic and State-of-the-Art Review Part III: Laboratory Investigations into Atmospheric Leach Processes | |
| CN103374656A (en) | Technique for recycling nickel, ferrum and cobalt from nickel oxide ore | |
| US9776885B2 (en) | Method for producing hematite for ironmaking | |
| CN110564961B (en) | Method for reducing leached hydrocobaltite | |
| CN102021332B (en) | Technology for recycling Ni, Co, Fe, and Mg from nickel oxide mineral | |
| US8454723B2 (en) | Saprolite neutralisation of heap leach process | |
| AU2019428963B2 (en) | Economical method, using combination of wet and dry processes, for smelting nickel from nickel sulfide ores | |
| Bahfie et al. | Development of laterite ore processing and its applications |