SU663747A1 - Master alloy - Google Patents
Master alloyInfo
- Publication number
- SU663747A1 SU663747A1 SU782569385A SU2569385A SU663747A1 SU 663747 A1 SU663747 A1 SU 663747A1 SU 782569385 A SU782569385 A SU 782569385A SU 2569385 A SU2569385 A SU 2569385A SU 663747 A1 SU663747 A1 SU 663747A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- master alloy
- ligature
- metal
- composition
- alloy
- Prior art date
Description
(54) ЛИГАТУРА(54) LIGATURE
чающиес друг от друга содержанием алюмини : вес.%: 0,05; 0,2; 0,3, а также содержанием железа, составл ющим дополнительную до 100% часть в каждом ооставе.aluminum content of each other: wt.%: 0.05; 0.2; 0.3, as well as the iron content, which constitutes an additional part up to 100% in each composition.
Лигатуру выплабл ли в открытых индукционных печах с использованием в качестве шихты отходов метаплургшгеского произрол-лва с впе дением элементов до необходимых концентрацийThe ligature was smoothed out in open induction furnaces, using as a charge the waste of the metaplurgic process, with the elements flowing to the required concentrations
Выход годного на опытном металле на 6,2% вьше, чем на металле серийной выплавки. В составе шихты использовали до 60% указанной лигатуры.The yield on the experimental metal is 6.2% higher than on the metal of the serial smelting. In the composition of the mixture used up to 60% of the specified ligature.
Сведени по качеству марочного металла, вь1плавленного с использованием предлагаемой лигатуры, приведены в таблице. Data on the quality of the brand metal melted using the proposed master alloy are given in the table.