SU572529A1 - Iron-base alloy - Google Patents
Iron-base alloyInfo
- Publication number
- SU572529A1 SU572529A1 SU7602346012A SU2346012A SU572529A1 SU 572529 A1 SU572529 A1 SU 572529A1 SU 7602346012 A SU7602346012 A SU 7602346012A SU 2346012 A SU2346012 A SU 2346012A SU 572529 A1 SU572529 A1 SU 572529A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- iron
- base alloy
- alloy
- manganese
- impurities
- Prior art date
Description
В качестве примесей сплав содержит, вес. %: Марганец0,2-0,4As impurities, the alloy contains, in weight. %: Manganese 0.2-0.4
КремнийДо 0,2Silicon up to 0,2
УглеродДо 0,03CarbonUp to 0.03
Температурный коэффициент линейного расширени сплава 0,2-0,6-10 град в интервале температур плюс 20 - минус 196°С иThe temperature coefficient of linear expansion of the alloy is 0.2-0.6-10 degrees in the temperature range plus 20 - minus 196 ° C and
1,3-2,4-10-8 град-1 в интервале температур 20 -300°С; коррозионна стойкость свыше1.3-2.4-10-8 degrees-1 in the temperature range 20 -300 ° C; corrosion resistance over
4600 ч в морской воде при 40°С.4,600 h in seawater at 40 ° C.
Сплав выплавл ют в открытой индукционной печи по обычной технологии выплавки сплавов на кобальтовой основе.The alloy is melted in an open induction furnace according to a conventional cobalt based alloy smelting technology.
Химический состав сплава приведен табл. 1.The chemical composition of the alloy is given in table. one.
Таблица 1Table 1
В качестве примесей в сплаве присутствует до 0,2 вес. % кремни , до 0,03 вес. % углеро- Ю да и марганец в указанных количествах. Свойства предлагаемого сплава приведены в табл. 2. Таблица 2As impurities in the alloy is up to 0.2 weight. % silicon, to 0.03 wt. % carbon and manganese in the specified amounts. Properties of the proposed alloy are given in table. 2. Table 2