SU399942A1 - Способ изготовления цинкового электрода химического источника тока - Google Patents

Способ изготовления цинкового электрода химического источника тока

Info

Publication number
SU399942A1
SU399942A1 SU1770883A SU1770883A SU399942A1 SU 399942 A1 SU399942 A1 SU 399942A1 SU 1770883 A SU1770883 A SU 1770883A SU 1770883 A SU1770883 A SU 1770883A SU 399942 A1 SU399942 A1 SU 399942A1
Authority
SU
USSR - Soviet Union
Prior art keywords
source current
zinc electrode
chemical source
electrode chemical
manufacturing zinc
Prior art date
Application number
SU1770883A
Other languages
English (en)
Inventor
В. В. Тризно Л. Г. Рувинский
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1770883A priority Critical patent/SU399942A1/ru
Application granted granted Critical
Publication of SU399942A1 publication Critical patent/SU399942A1/ru

Description

(1
Известен способ изготовлени  цинкового электрода химического источника тока путем смешивапи  окиси цинка с цинковой пылью и поливиниловым спиртом, многократного пропускани  смеси через сита и сушки с последующей напрессовкой на токоотвод.
При продавливании влажной смеси через отверсти  сита образующиес  стержни слипаютс . В результате в процессе последующей сушки образуютс  агломераты слипшихс  частиц , которые необходимо дробить многократным пропусканием через сита, что усложн ет технологический процесс и способствует истиранию частиц. При этом возникает много пыли, котора  увеличивает количество отходов и нарушает однородность порошка.
Целью изобретени   вл етс  упрощение технологии способа.
По предложепному способу смесь перед первым пропусканием через сито подсушивают до влажности 12-15%.
2
В зкую смесь окиси цинка, цинковой пыли и поливипилового спирта подсушивают до влажности 12-15%, после чего пропускают через сито с размером  чеек 1 мм. Полученный грапул т повторно сушат до влажности 0,1-0,5% и пропускают через сито с размером  чеек 2 мм. Затем гранулированную массу напрессовывают на токоотвод.
При этом электрод имеет высокую однородность и стабильную объемную массу.
Предмет изобретени 
Способ изготовлени  цинкового электрода химического источника тока путем смешивани  окиси цинка с цинковой пылью и поливиниловым спиртом, многократного пропускани  смеси через сита и сушки с последуюшей напрессовкой на токоотвод, отличающийс  тем, что, с целью упрощени  технологии, смесь перед первым пропусканием через сито подсушивают до влажности 12-15%.
SU1770883A 1972-04-10 1972-04-10 Способ изготовления цинкового электрода химического источника тока SU399942A1 (ru)