SU1741476A1 - METHOD OF CORRECTING THE ELECTROLYTE COMPOSITION WHEN RECEIVING ZIRCONIUM - Google Patents

METHOD OF CORRECTING THE ELECTROLYTE COMPOSITION WHEN RECEIVING ZIRCONIUM

Info

Publication number
SU1741476A1
SU1741476A1 SU3206027/02A SU3206027A SU1741476A1 SU 1741476 A1 SU1741476 A1 SU 1741476A1 SU 3206027/02 A SU3206027/02 A SU 3206027/02A SU 3206027 A SU3206027 A SU 3206027A SU 1741476 A1 SU1741476 A1 SU 1741476A1
Authority
SU
USSR - Soviet Union
Prior art keywords
electrolyte
zirconium
loading
amount
temperature
Prior art date
Application number
SU3206027/02A
Other languages
Russian (ru)
Inventor
А.Д. Манахов
Г.Н. Титов
П.И. Москаленко
Original Assignee
Чепецкий механический завод
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Чепецкий механический завод filed Critical Чепецкий механический завод
Priority to SU3206027/02A priority Critical patent/SU1741476A1/en
Application granted granted Critical
Publication of SU1741476A1 publication Critical patent/SU1741476A1/en

Abstract

Способ корректировки состава электролита при получении циркония, включающий контроль количества электричества и состава электролита, расчет величины загрузки исходных солей фторцирконата и хлорида калия и загрузку их в электролизер, отличающийся тем, что, с целью увеличения выхода циркония по току за счет повышения точности состава электролита, перед загрузкой измеряют температуру электролита и расчет величины загрузки исходных солей ведут по формуламP= A· Q - B(C- C') + D(T - T')P= A· Q - B(C- C') + D(T - T')P, P- количество солей фторцирконата и хлорида калия, загружаемых в текущем периоде, кг;Q - количество электричества за прошедший период, кА · ч;C, C- содержание циркония и хлора в электролите в прошедшем периоде, мас.%;T - результат измерения температуры электролита перед загрузкой,C;C', C'- заданные значения содержания циркония и хлора в электролите, мас.%;T' - заданное значение температуры электролита,C;A, B, D, A, B, D- заданные коэффициенты A= 1,6 - 2,0, B= 2 - 40, D= 1,4 - 3,7, A= 1,3 - 3,1; B= 10 - 30, D= 0,8 - 2,6.The method of adjusting the composition of the electrolyte upon receipt of zirconium, including controlling the amount of electricity and the composition of the electrolyte, calculating the load of the initial salts of fluorocirconate and potassium chloride and loading them into the electrolyzer, characterized in that in order to increase the output of zirconium by before loading, measure the temperature of the electrolyte and calculate the loading of the starting salts using the formulas P = A · Q - B (C-C ') + D (T - T') P = A · Q - B (C-C ') + D ( T - T ') P, P is the amount of salts of fluorocirconate and potassium chloride I, loaded in the current period, kg; Q - the amount of electricity for the past period, kA · h; C, C - the content of zirconium and chlorine in the electrolyte in the past period, wt.%; T - the result of measuring the temperature of the electrolyte before loading, C; C ', C'- set points of zirconium and chlorine in the electrolyte, wt.%; T' - set point of the electrolyte temperature, C; A, B, D, A, B, D - set factors A = 1.6 - 2 , 0, B = 2-40, D = 1.4-3.7, A = 1.3-3.1; B = 10 - 30, D = 0.8 - 2.6.

SU3206027/02A 1988-07-04 1988-07-04 METHOD OF CORRECTING THE ELECTROLYTE COMPOSITION WHEN RECEIVING ZIRCONIUM SU1741476A1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
SU3206027/02A SU1741476A1 (en) 1988-07-04 1988-07-04 METHOD OF CORRECTING THE ELECTROLYTE COMPOSITION WHEN RECEIVING ZIRCONIUM

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
SU3206027/02A SU1741476A1 (en) 1988-07-04 1988-07-04 METHOD OF CORRECTING THE ELECTROLYTE COMPOSITION WHEN RECEIVING ZIRCONIUM

Publications (1)

Publication Number Publication Date
SU1741476A1 true SU1741476A1 (en) 2000-02-27

Family

ID=60532669

Family Applications (1)

Application Number Title Priority Date Filing Date
SU3206027/02A SU1741476A1 (en) 1988-07-04 1988-07-04 METHOD OF CORRECTING THE ELECTROLYTE COMPOSITION WHEN RECEIVING ZIRCONIUM

Country Status (1)

Country Link
SU (1) SU1741476A1 (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
RU2400568C2 (en) * 2008-08-08 2010-09-27 Открытое акционерное общество "Высокотехнологический научно-исследовательский институт неорганических материалов имени академика А.А.Бочвара" Method of producing zirconium through molten electrolyte electrolysis (versions)
RU2654397C2 (en) * 2016-09-06 2018-05-17 Акционерное общество "Высокотехнологический научно-исследовательский институт неорганических материалов имени академика А.А. Бочвара" Method of producing zirconium through molten electrolyte electrolysis (versions)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
RU2400568C2 (en) * 2008-08-08 2010-09-27 Открытое акционерное общество "Высокотехнологический научно-исследовательский институт неорганических материалов имени академика А.А.Бочвара" Method of producing zirconium through molten electrolyte electrolysis (versions)
RU2654397C2 (en) * 2016-09-06 2018-05-17 Акционерное общество "Высокотехнологический научно-исследовательский институт неорганических материалов имени академика А.А. Бочвара" Method of producing zirconium through molten electrolyte electrolysis (versions)

Similar Documents

Publication Publication Date Title
GEP19970775B (en) Method for the production of human erythropoietin
ES8704552A1 (en) Use of a lead alloy for the anodes in the electrolytic production of zinc.
SU1741476A1 (en) METHOD OF CORRECTING THE ELECTROLYTE COMPOSITION WHEN RECEIVING ZIRCONIUM
DK402187A (en) NICKEL Alloy Anodes for Electrochemical Dechlorination
GB1449118A (en) Aluminum sacrificial anode
IN164906B (en)
Valette Energies involved in the specific adsorption of halides on sd metals: Part I. Analysis of experimental results
Schaller et al. On the Thermodynamics of Cobalt--Aluminium Alloys
Kochergin High-Temperature Corrosion of Lanthanum in an Equimolar Mixture of Sodium and Potassium Chlorides
SU1741477A1 (en) METHOD OF CONTROL OF HAFNY CONCENTRATION IN THE ZIRCONIUM OF CATHODE PRODUCT
ATE145152T1 (en) ELECTROCHEMICAL CELL AND USE THEREOF FOR ELECTROCHEMICAL SEPARATION OR EXTRACTION OF OXYGEN
US4306948A (en) Limiting production of an electrolytic alkali metal cell
JPS6470450A (en) Novel nitrogen-containing perfluorocarboxylic fluoride and its preparation
JPS52106309A (en) Control of alumina supplying for aluminum electrolytic cell
Valette Energies involved in the specific adsorption of halides on sd metals: Part II. Parallelism with energies involved in the formation of the corresponding bulk compounds and comparison with sp metals
GB648337A (en) Process for the manufacture of aluminium by means of melt electrolysis at relatively low temperatures
GB1392263A (en) Electrolysis of aluminium
SU464636A1 (en) Lead based alloy
Vetyukov et al. Equilibrium of Aluminum With Cryolite-Alumina Melts
Sagadieva et al. The Method of Inverse Voltammetry Used to Study the Anodic Oxidation of an Amalgam of Cerium and Terbium
Lietzke et al. The thermodynamic properties of deuterium chloride-sodium chloride mixtures in heavy water
SU395511A1 (en) METHOD OF OBTAINING AN ALLOY PLATINUM - PALLADIUM
Kirilenko et al. As sub (2) Se sub (3)-Se-TlAsSe sub (2)-system.
ES262980A1 (en) PROCEDURE FOR OBTAINING QUATERNARY SALTS
Naka et al. High Corrosion Resistance of CoCrMoHf Amorphous Alloys