PE20040137A1 - Metodo para producir cobre blister - Google Patents
Metodo para producir cobre blisterInfo
- Publication number
- PE20040137A1 PE20040137A1 PE2003000540A PE2003000540A PE20040137A1 PE 20040137 A1 PE20040137 A1 PE 20040137A1 PE 2003000540 A PE2003000540 A PE 2003000540A PE 2003000540 A PE2003000540 A PE 2003000540A PE 20040137 A1 PE20040137 A1 PE 20040137A1
- Authority
- PE
- Peru
- Prior art keywords
- reactor
- melting furnace
- white metal
- produce copper
- oxidizing
- Prior art date
Abstract
QUE COMPRENDE: a) ALIMENTAR CONCENTRADO DE COBRE, FUNDENTE Y AIRE CON ALTO CONTENIDO DE OXIGENO EN UN HORNO DE FUSION EN SUSPENSION, TAL COMO UN HORNO DE FUSION RAPIDA, FORMANDOSE DOS FASES FUNDIDAS: TAL COMO METAL BLANCO Y ESCORIA; b) OXIDAR EL METAL BLANCO EN POR LO MENOS UN REACTOR OXIDANTE DISPUESTO PARA SER INSTALADO, DE MODO FIJO POR MEDIO DE UNA ARTESA DE FUSION, EN CONEXION CON DICHO HORNO DE FUSION; Y, c) TRATAR LA ESCORIA, EN UN HORNO ELECTRICO O EN FLOTACION, CON EL FIN DE RECUPERAR EL CONTENIDO DE COBRE DE LA MISMA. EL REACTOR OXIDANTE ES UN REACTOR DE EXPLOSION SUPERFICIAL O UN REACTOR DE INYECCION
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| FI20021114A FI116069B (fi) | 2002-06-11 | 2002-06-11 | Menetelmä raakakuparin valmistamiseksi |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| PE20040137A1 true PE20040137A1 (es) | 2004-05-05 |
Family
ID=8564117
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PE2003000540A PE20040137A1 (es) | 2002-06-11 | 2003-06-02 | Metodo para producir cobre blister |
Country Status (16)
| Country | Link |
|---|---|
| US (1) | US20050199095A1 (es) |
| EP (1) | EP1511868A1 (es) |
| JP (1) | JP2005536629A (es) |
| KR (1) | KR20050007600A (es) |
| CN (1) | CN100385024C (es) |
| AR (1) | AR040256A1 (es) |
| AU (1) | AU2003232264A1 (es) |
| BR (1) | BR0311758A (es) |
| CA (1) | CA2488398A1 (es) |
| EA (1) | EA007445B1 (es) |
| FI (1) | FI116069B (es) |
| MX (1) | MXPA04012084A (es) |
| PE (1) | PE20040137A1 (es) |
| PL (1) | PL372533A1 (es) |
| RS (1) | RS107704A (es) |
| WO (1) | WO2003104504A1 (es) |
Families Citing this family (11)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| FI117769B (fi) * | 2004-01-15 | 2007-02-15 | Outokumpu Technology Oyj | Suspensiosulatusuunin syöttöjärjestelmä |
| DE102005008684B4 (de) * | 2004-03-05 | 2008-10-09 | Merck Patent Gmbh | Verwendung von Flüssigkristall-Displays sowie Verfahren zu deren Verwertung |
| CA2565643C (en) * | 2006-06-28 | 2011-08-02 | Nippon Mining & Metals Co., Ltd. | Operation method of copper smelting |
| FI120157B (fi) * | 2007-12-17 | 2009-07-15 | Outotec Oyj | Menetelmä kuparirikasteen jalostamiseksi |
| JP4908456B2 (ja) | 2008-06-02 | 2012-04-04 | パンパシフィック・カッパー株式会社 | 銅の製錬方法 |
| CN102605191B (zh) | 2012-04-16 | 2013-12-25 | 阳谷祥光铜业有限公司 | 一种铜精矿直接生产粗铜的方法 |
| US9725784B2 (en) | 2012-06-21 | 2017-08-08 | Lawrence F. McHugh | Production of copper via looping oxidation process |
| CN102876902A (zh) * | 2012-10-18 | 2013-01-16 | 铜陵有色金属集团股份有限公司金冠铜业分公司 | 一种铜精矿闪速-熔池复合熔炼方法及奥托昆普闪速炉 |
| FI125793B (en) | 2014-05-14 | 2016-02-15 | Outotec Finland Oy | A method for converting copper-containing material |
| JP6466869B2 (ja) * | 2016-02-29 | 2019-02-06 | パンパシフィック・カッパー株式会社 | 銅製錬炉の操業方法 |
| BE1025772B1 (nl) * | 2017-12-14 | 2019-07-08 | Metallo Belgium | Verbetering in koper-/tin-/loodproductie |
Family Cites Families (10)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5230259B2 (es) * | 1974-03-30 | 1977-08-06 | ||
| FI52358C (fi) * | 1974-11-11 | 1977-08-10 | Outokumpu Oy | Tapa valmistaa raakakuparia jatkuvasti yhdessä vaiheessa epäpuhtaasta sulfidisesta kuparirikasteesta tai -malmista . |
| DE2941225A1 (de) * | 1979-10-11 | 1981-04-23 | Klöckner-Humboldt-Deutz AG, 5000 Köln | Verfahren und vorrichtung zur pyrometallurgischen gewinnung von kupfer |
| US4416690A (en) * | 1981-06-01 | 1983-11-22 | Kennecott Corporation | Solid matte-oxygen converting process |
| US4470845A (en) * | 1983-01-05 | 1984-09-11 | Newmont Mining Corporation | Continuous process for copper smelting and converting in a single furnace by oxygen injection |
| FI67727C (fi) * | 1983-06-15 | 1985-05-10 | Outokumpu Oy | Foerfarande foer att tillverka raokoppar |
| CA1323495C (en) * | 1988-04-29 | 1993-10-26 | Marc Reist | Process and apparatus for converting of solid high-grade copper matte |
| US5194213A (en) * | 1991-07-29 | 1993-03-16 | Inco Limited | Copper smelting system |
| CN1067113C (zh) * | 1998-08-08 | 2001-06-13 | 徐有生 | 铜、镍硫化矿无污染火冶法 |
| TR200201715T2 (tr) * | 2000-01-04 | 2002-10-21 | Outokumpu Oyj | Süspansiyon reaktöründe blister bakırı üretimi için yöntem |
-
2002
- 2002-06-11 FI FI20021114A patent/FI116069B/fi active IP Right Grant
-
2003
- 2003-06-02 CA CA002488398A patent/CA2488398A1/en not_active Abandoned
- 2003-06-02 CN CNB038135205A patent/CN100385024C/zh not_active Expired - Fee Related
- 2003-06-02 PE PE2003000540A patent/PE20040137A1/es not_active Application Discontinuation
- 2003-06-02 KR KR10-2004-7020015A patent/KR20050007600A/ko not_active Withdrawn
- 2003-06-02 AU AU2003232264A patent/AU2003232264A1/en not_active Abandoned
- 2003-06-02 WO PCT/FI2003/000432 patent/WO2003104504A1/en not_active Ceased
- 2003-06-02 RS YUP-1077/04A patent/RS107704A/sr unknown
- 2003-06-02 PL PL03372533A patent/PL372533A1/xx not_active Application Discontinuation
- 2003-06-02 BR BR0311758-8A patent/BR0311758A/pt not_active IP Right Cessation
- 2003-06-02 EA EA200401402A patent/EA007445B1/ru unknown
- 2003-06-02 EP EP03757080A patent/EP1511868A1/en not_active Withdrawn
- 2003-06-02 MX MXPA04012084A patent/MXPA04012084A/es unknown
- 2003-06-02 JP JP2004511562A patent/JP2005536629A/ja not_active Abandoned
- 2003-06-02 US US10/517,506 patent/US20050199095A1/en not_active Abandoned
- 2003-06-10 AR ARP030102064A patent/AR040256A1/es not_active Application Discontinuation
Also Published As
| Publication number | Publication date |
|---|---|
| WO2003104504A1 (en) | 2003-12-18 |
| AR040256A1 (es) | 2005-03-23 |
| EA200401402A1 (ru) | 2005-06-30 |
| CN1659293A (zh) | 2005-08-24 |
| RS107704A (sr) | 2007-04-10 |
| KR20050007600A (ko) | 2005-01-19 |
| BR0311758A (pt) | 2005-03-08 |
| FI20021114A0 (fi) | 2002-06-11 |
| CN100385024C (zh) | 2008-04-30 |
| PL372533A1 (pl) | 2005-07-25 |
| EA007445B1 (ru) | 2006-10-27 |
| US20050199095A1 (en) | 2005-09-15 |
| FI116069B (fi) | 2005-09-15 |
| EP1511868A1 (en) | 2005-03-09 |
| CA2488398A1 (en) | 2003-12-18 |
| AU2003232264A1 (en) | 2003-12-22 |
| JP2005536629A (ja) | 2005-12-02 |
| MXPA04012084A (es) | 2005-03-07 |
| FI20021114L (fi) | 2003-12-12 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| PE20040137A1 (es) | Metodo para producir cobre blister | |
| DK1404483T3 (da) | Forbedringer af eller i forbindelse med loddemetaller | |
| DE69800465D1 (de) | Verfahren und automatische Vorrichtung zum Signieren durch Plasma, insbesondere von Metallen | |
| NO20073255L (no) | Framgangsmate og anordning for a utvinne metall av slagg | |
| MX2007012199A (es) | Operacion de horno de recuperacion de oxido de hierro para ahooro de energia, remocion de metal volatil y control de escoria. | |
| PL392792A1 (pl) | Sposób rafinacji koncentratu miedzi | |
| NO341678B1 (no) | Framgangsmåte for kontinuerlig eller diskontinuerlig utvinning av ett eller flere metaller fra et slagg | |
| CL2009002241A1 (es) | Metodo y sistema para el procesamiento de la escoria de convertidor producida en la fundicion del cobre que comprende alimentacion de la escoria en un horno de reduccion, reduccion del zinc y del cobre mediante calentamiento y remocion del zinc reducido a traves de la volatizacion en el horno de reduccion. | |
| CN1943959A (zh) | 一种激光-电弧复合加工方法 | |
| AR245507A1 (es) | Un procedimiento para recuperar aluminio libre de escorias o desechos de aluminio | |
| CL2009001325A1 (es) | Metodo para fundir cobre, sin suministrar un material de coque, y suministrar un lingote de fundicion en el horno. | |
| MXPA05000748A (es) | Elemento de enfriamiento. | |
| WO2008117044A3 (en) | Method for treating spent pot liner | |
| AR042301A1 (es) | Metodo para tratar escoria | |
| CL2009001729A1 (es) | Método para fundir cobre que comprende generar cobre blister y escoria de ferrita de calcio a partir de mata de cobre, refinar otro cobre blister a partir de la escoria mediante reducción en horno eléctrico, seguido por carguío de la escoria en un horno de fundición, para tratar un concentrado de cobre y la generación de mata. | |
| AR035418A1 (es) | Un ensamble cuadrilateral conveniente para la instalacion en una pared de un horno de arco electrico y un metodo para proporcionar gas en un horno de arco electrico | |
| WO2007070764A3 (en) | Method for controlling foaming of slag in an electric arc furnace | |
| BR9917343A (pt) | Processo para a determinação do comprimento de eletrodo e do nìvel de banho no forno de arco voltaico elétrico | |
| TWI370034B (en) | Device and procedure for the wave soldering | |
| ITMI20050538A1 (it) | Metodo e apparato per il recupero della scoria di metallurgia secondaria -lf-e suo riciclo nel processo produttivo di acciaio tramite forno ad arco elettrico | |
| ES2150266T3 (es) | Procedimiento de reduccion y de fusion de un metal. | |
| AR037779A1 (es) | Metodo y aparato para aumentar la capacidad de una caldera de recuperacion en un horno de fusion metalurgico. | |
| WO2012089754A3 (de) | Verfahren zur pyrometallurgischen behandlung von metallen, metallschmelzen und/ oder schlacken | |
| JP2010221296A (ja) | サブマージアーク溶接方法 | |
| CL2009001730A1 (es) | Metodo para fundir cobre mediante reduccion en horno electrico a temperatura entre 1.250 y 1.350 grados celsius y a una atmosfera reductora de presion parcial de o2 logpo2 menor o igual a -9,3, y la ley de la escoria de ferrita de calcio es reducida a 0,8% o menos. |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| FG | Grant, registration | ||
| FD | Application declared void or lapsed |