PE20020619A1 - Proceso de lixiviacion a presion para el zinc - Google Patents
Proceso de lixiviacion a presion para el zincInfo
- Publication number
- PE20020619A1 PE20020619A1 PE2001000915A PE2001000915A PE20020619A1 PE 20020619 A1 PE20020619 A1 PE 20020619A1 PE 2001000915 A PE2001000915 A PE 2001000915A PE 2001000915 A PE2001000915 A PE 2001000915A PE 20020619 A1 PE20020619 A1 PE 20020619A1
- Authority
- PE
- Peru
- Prior art keywords
- zinc
- solution
- iron
- pressure leaching
- produce
- Prior art date
Abstract
QUE COMPRENDE: a) SOMETER UN CONCENTRADO DE SULFURO DE ZINC A LIXIVIACION POR PRESION CON UNA SOLUCION DE LIXIVIACION ACIDA QUE CONTIENE POR LO MENOS 15 g/L DE Fe EN SOLUCION, HASTA PRODUCIR UNA SOLUCION DE Zn Y UN RESIDUO DE LIXIVIACION SOLIDO QUE CONTIENE Fe; b) SOMETER LA SOLUCION DE Zn A EXTRACCION POR SOLVENTE DEL Zn, PARA PRODUCIR UN REFINADO Y UNA SOLUCION MATRIZ DE Zn; Y, c) SOMETER LA SOLUCION MATRIZ DE Zn A ELECTROEXTRACCION, PARA RECUPERAR Zn Y PRODUCIR UN ELECTROLITO AGOTADO RESULTANTE QUE SE RECICLA A LA EXTRACCION POR SOLVENTE DE Zn. LA LIXIVIACION POR PRESION ES EFECTUADA EN DOS ETAPAS CONTRACORRIENTE: UNA PARA PRODUCIR LA SOLUCION DE Zn Y UN RESIDUO INTERMEDIO, Y OTRA DONDE EL RESIDUO INTERMEDIO ES LIXIVIADO CON LA SOLUCION ACIDA DE (a). ADEMAS, SE REFIERE A UN METODO PARA SEPARAR Fe DE UN REFINADO QUE LO CONTIENE, QUE COMPRENDE LIXIVIAR POR PRESION UNA MENA DE SULFATO DE Zn CON DICHO REFINADO PARA PRODUCIR UN RESIDUO SOLIDO DE LIXIVIACION QUE CONTIENE Fe Y UNA SOLUCION DE Zn
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US09/659,098 US6471849B1 (en) | 2000-09-11 | 2000-09-11 | Process for the recovery of zinc from a zinc sulphide ore or concentrate |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| PE20020619A1 true PE20020619A1 (es) | 2002-08-12 |
Family
ID=24644008
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PE2001000915A PE20020619A1 (es) | 2000-09-11 | 2001-09-11 | Proceso de lixiviacion a presion para el zinc |
Country Status (13)
| Country | Link |
|---|---|
| US (1) | US6471849B1 (es) |
| EP (1) | EP1325164B1 (es) |
| JP (1) | JP2004507624A (es) |
| KR (1) | KR100730869B1 (es) |
| AT (1) | ATE295902T1 (es) |
| AU (2) | AU8746801A (es) |
| CA (1) | CA2421722C (es) |
| DE (1) | DE60110924T2 (es) |
| ES (1) | ES2244651T3 (es) |
| MX (1) | MXPA03002100A (es) |
| PE (1) | PE20020619A1 (es) |
| WO (1) | WO2002020855A2 (es) |
| ZA (1) | ZA200301902B (es) |
Families Citing this family (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR101043398B1 (ko) * | 2009-07-02 | 2011-06-22 | 고려아연 주식회사 | 아연 정광을 이용한 구리 회수 방법 및 구리 전해액 제조 방법 |
| CN102560147B (zh) * | 2011-12-30 | 2014-03-26 | 株洲冶炼集团股份有限公司 | 一种从铟萃余液、锌浮渣中回收锌的方法 |
| CA2881600C (en) * | 2012-08-07 | 2021-04-27 | Glencore Queensland Limited | Recovery of zinc from lead slag |
| CN103911511B (zh) * | 2014-04-28 | 2016-08-17 | 北京矿冶研究总院 | 一种从锌溶液中除铁的方法 |
| US9410225B2 (en) | 2014-05-13 | 2016-08-09 | Teck Resources Limited | Process for recovery of copper from arsenic-bearing and/or antimony-bearing copper sulphide concentrates |
| PE20191621A1 (es) | 2017-04-14 | 2019-11-06 | Sherritt Int Corporation | Lixiviacion oxidativa presurizada, de bajo contenido de solidos y baja acidez de materiales de alimentacion sulfurados |
| KR101889680B1 (ko) * | 2018-02-01 | 2018-08-17 | 고려아연 주식회사 | 황산아연 용액으로부터 철을 회수하는 방법 |
Family Cites Families (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CA1049953A (en) | 1975-10-22 | 1979-03-06 | Herbert Veltman | Two-stage pressure leaching process for zinc and iron bearing mineral sulphides |
| US4330379A (en) * | 1979-01-24 | 1982-05-18 | National Institute For Metallurgy | Leaching of zinc containing sulphide minerals |
| CA1212242A (en) * | 1982-07-27 | 1986-10-07 | Donald R. Weir | Recovery of zinc from zinc-containing sulphidic material |
| US5902474A (en) * | 1993-07-29 | 1999-05-11 | Cominco Engineering Services Ltd. | Chloride assisted hydrometallurgical extraction of metal |
| US5869012A (en) * | 1993-07-29 | 1999-02-09 | Cominco Engineering Services Ltd. | Chloride assisted hydrometallurgical extraction of metal |
| ES2103134T3 (es) * | 1993-08-27 | 1997-08-16 | Union Miniere Sa | Procedimiento para extraccion de zinc de concentrados sulfurados. |
| GB9422476D0 (en) * | 1994-11-08 | 1995-01-04 | Sherritt Inc | Recovery of zinc from sulphidic concentrates |
| AUPN191395A0 (en) * | 1995-03-22 | 1995-04-27 | M.I.M. Holdings Limited | Atmospheric mineral leaching process |
-
2000
- 2000-09-11 US US09/659,098 patent/US6471849B1/en not_active Expired - Fee Related
-
2001
- 2001-09-11 EP EP01966924A patent/EP1325164B1/en not_active Expired - Lifetime
- 2001-09-11 DE DE60110924T patent/DE60110924T2/de not_active Expired - Fee Related
- 2001-09-11 AU AU8746801A patent/AU8746801A/xx active Pending
- 2001-09-11 CA CA002421722A patent/CA2421722C/en not_active Expired - Fee Related
- 2001-09-11 JP JP2002525860A patent/JP2004507624A/ja active Pending
- 2001-09-11 PE PE2001000915A patent/PE20020619A1/es not_active Application Discontinuation
- 2001-09-11 AU AU2001287468A patent/AU2001287468B2/en not_active Ceased
- 2001-09-11 WO PCT/CA2001/001288 patent/WO2002020855A2/en not_active Ceased
- 2001-09-11 AT AT01966924T patent/ATE295902T1/de not_active IP Right Cessation
- 2001-09-11 MX MXPA03002100A patent/MXPA03002100A/es active IP Right Grant
- 2001-09-11 ES ES01966924T patent/ES2244651T3/es not_active Expired - Lifetime
- 2001-09-11 KR KR1020037003517A patent/KR100730869B1/ko not_active Expired - Fee Related
-
2003
- 2003-03-07 ZA ZA200301902A patent/ZA200301902B/en unknown
Also Published As
| Publication number | Publication date |
|---|---|
| ES2244651T3 (es) | 2005-12-16 |
| WO2002020855A3 (en) | 2002-10-03 |
| DE60110924T2 (de) | 2006-04-27 |
| ATE295902T1 (de) | 2005-06-15 |
| US6471849B1 (en) | 2002-10-29 |
| KR20030043957A (ko) | 2003-06-02 |
| AU8746801A (en) | 2002-03-22 |
| ZA200301902B (en) | 2004-06-25 |
| CA2421722A1 (en) | 2002-03-14 |
| AU2001287468B2 (en) | 2006-03-30 |
| EP1325164B1 (en) | 2005-05-18 |
| MXPA03002100A (es) | 2004-05-05 |
| EP1325164A2 (en) | 2003-07-09 |
| CA2421722C (en) | 2009-05-12 |
| JP2004507624A (ja) | 2004-03-11 |
| WO2002020855A2 (en) | 2002-03-14 |
| DE60110924D1 (de) | 2005-06-23 |
| KR100730869B1 (ko) | 2007-06-20 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| AP1454A (en) | Method for recovering copper from sulfide ore materials using high temperature pressure leaching, solvent extraction and electrowinning. | |
| NO883374D0 (no) | Fremgangsmaate til felles adskillelse av forstyrrelseselementer fra verdimetallelektrolytopploesninger. | |
| ES543511A0 (es) | Un procedimiento hidrometalurgico para extraer zinc y cobre y recuperar plomo y-o metales preciosos, principalmente la plata, de materias sulfurosas zinciferas | |
| EA200000222A1 (ru) | Способ извлечения меди из сульфидной медной руды или концентрата | |
| ATE256202T1 (de) | Ionentauscherharz-verfahren zur gewinnung von nickel und kobalt aus oxiderz-laugungsschlamm | |
| DK0862659T3 (da) | Fremgangsmåde til udvinding af nikkel fra Ni-Fe-Mg-lateritmalm med højt magnesiumindhold | |
| ES437687A1 (es) | Procedimiento para la obtencion de cobre electrolitico a partir de minerales cupriferos. | |
| EA200100893A1 (ru) | Способ извлечения металлов из медно-сульфидных и/или медно-железосульфидных руд | |
| ATE405681T1 (de) | Verfahren zur extraktion von nickel und cobalt aus lateriterzen | |
| PE20020619A1 (es) | Proceso de lixiviacion a presion para el zinc | |
| MX2007002456A (es) | Metodo mejorado para lixiviacion en montones y vertederos acoplado con extraccion de solventes de metales. | |
| ES8506106A1 (es) | Un metodo para extraer cobre de minerales o concentrados sulfurados | |
| Xue et al. | Solvent extraction of iron(III) from acid sulfate solutions with Eichrom's Dipix extractant | |
| FR2396573A1 (fr) | Extraction par solvants de metaux non ferreux a partir d'une solution aqueuse acide contenant du fer | |
| ES2005142A6 (es) | Proceso para la recuperacion de metales no ferrosos de concentrados de sulfuros polimetalicos | |
| JPS56114832A (en) | Wet treatment of manganese nodules | |
| ES2123417A1 (es) | Procedimiento hidrometalurgico para la recuperacion de cobre de minerales sulfurados. | |
| Wang | The Recovery of Lean Copper Ores | |
| Hilbrans et al. | Cyclone smelting for residues from zinc metal production | |
| TH37505A (th) | การสกัดโลหะแบบไฮโดรโลหะวิทยาที่มีคลอไรด์ช่วย | |
| KR910012305A (ko) | 제강용 전기로 분진으로부터 유가금속의 회수방법 | |
| GB1474973A (en) | Production of copper | |
| RU93008768A (ru) | Способ выщелачивания свинцового концентрата | |
| RU94040270A (ru) | Способ выделения металлов из минерального сырья путем гидрометаллургической переработки |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| FG | Grant, registration | ||
| FD | Application declared void or lapsed |