PE116399A1 - Metodo para limitar puntos maximos de temperatura y/o aumentar la capacidad de produccion de un horno de refinacion continua de cobre con soplado en la parte alta - Google Patents
Metodo para limitar puntos maximos de temperatura y/o aumentar la capacidad de produccion de un horno de refinacion continua de cobre con soplado en la parte altaInfo
- Publication number
- PE116399A1 PE116399A1 PE1998000911A PE00091198A PE116399A1 PE 116399 A1 PE116399 A1 PE 116399A1 PE 1998000911 A PE1998000911 A PE 1998000911A PE 00091198 A PE00091198 A PE 00091198A PE 116399 A1 PE116399 A1 PE 116399A1
- Authority
- PE
- Peru
- Prior art keywords
- copper
- blister
- oven
- mata
- increasing
- Prior art date
Abstract
CONSISTE EN UN METODO PARA LIMITAR PUNTOS MAXIMOS DE TEMPERATURA ENTRE 1100-1400�C, EN UN BANO DE COBRE BLISTER FUNDIDO MANTENIDO EN UN HORNO DE REFINACION CONTINUA CON SOPLADO EN LA PARTE ALTA, ADAPTADO PARA RECIBIR EN FORMA CONTINUA MATA DE COBRE FUNDIDO DE UN HORNO DE SEPARACION Y DESCARGAR CONTINUAMENTE COBRE BLISTER FUNDIDO A UN HORNO ANODICO. ESTE METODO COMPRENDE EL PASO DE ANADIR MATA DE COBRE SOLIDO, FINAMENTE DIVIDIDO, AL BANO DE COBRE BLISTER FUNDIDO PARA MANTENER EL RANGO DE TEMPERATURAS MENCIONADO, DADA LA REACCION EXOTERMICA DE OXIDACION DEL HIERRO Y AZUFRE EN EL COBRE BLISTER, Y TOMANDO EN CUENTA QUE LA REFUNDICION DE LA MATA CONSUME EL CALOR DEL BANO, DISMINUYENDO SU TEMPERATURA
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US08/936,322 US6042632A (en) | 1996-01-17 | 1997-09-24 | Method of moderating temperature peaks in and/or increasing throughput of a continuous, top-blown copper converting furnace |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| PE116399A1 true PE116399A1 (es) | 1999-11-22 |
Family
ID=25468472
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PE1998000911A PE116399A1 (es) | 1997-09-24 | 1998-09-24 | Metodo para limitar puntos maximos de temperatura y/o aumentar la capacidad de produccion de un horno de refinacion continua de cobre con soplado en la parte alta |
Country Status (9)
| Country | Link |
|---|---|
| US (1) | US6042632A (es) |
| JP (1) | JP4418588B2 (es) |
| KR (1) | KR100566177B1 (es) |
| AU (1) | AU741047B2 (es) |
| CA (1) | CA2304651A1 (es) |
| ES (1) | ES2164036B2 (es) |
| ID (1) | ID25891A (es) |
| PE (1) | PE116399A1 (es) |
| WO (1) | WO1999015706A1 (es) |
Families Citing this family (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| TR200201715T2 (tr) * | 2000-01-04 | 2002-10-21 | Outokumpu Oyj | Süspansiyon reaktöründe blister bakırı üretimi için yöntem |
| US6517617B1 (en) | 2000-09-20 | 2003-02-11 | Whi Usa, Inc. | Method and apparatus to clean and apply foamed corrosion inhibitor to ferrous surfaces |
| US6478847B1 (en) | 2001-08-31 | 2002-11-12 | Mueller Industries, Inc. | Copper scrap processing system |
| JP4736668B2 (ja) * | 2005-09-26 | 2011-07-27 | 株式会社デンソー | 負荷駆動装置の信号検出装置 |
| FI124028B (en) * | 2012-06-13 | 2014-02-14 | Outotec Oyj | Method and arrangement for refining copper concentrate |
| FI127349B (en) * | 2015-04-23 | 2018-04-13 | Outotec Finland Oy | Melting of scrap metal in anode furnace processes |
| CN108193057B (zh) * | 2018-02-08 | 2023-09-12 | 宜兴曜源科技发展有限公司 | 一种铜吹炼渣热态加入铜熔炼炉系统及其操作方法 |
| EP4061972B1 (en) * | 2019-11-22 | 2023-10-11 | Aurubis Beerse | Improved copper smelting process |
Family Cites Families (18)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5839214B2 (ja) * | 1977-12-30 | 1983-08-29 | 三菱マテリアル株式会社 | 非鉄金属の製錬法 |
| US4415356A (en) * | 1980-10-01 | 1983-11-15 | Inco Limited | Process for autogenous oxygen smelting of sulfide materials containing base metals |
| US4416690A (en) * | 1981-06-01 | 1983-11-22 | Kennecott Corporation | Solid matte-oxygen converting process |
| US4470845A (en) * | 1983-01-05 | 1984-09-11 | Newmont Mining Corporation | Continuous process for copper smelting and converting in a single furnace by oxygen injection |
| FI69871C (fi) * | 1984-07-18 | 1986-05-26 | Outokumpu Oy | Foerfarande och anordning foer behandling av sulfidkoncentrat eller -malmer till raometaller |
| JPS6160836A (ja) * | 1984-08-31 | 1986-03-28 | Sumitomo Metal Mining Co Ltd | 銅転炉の操業法 |
| CA1323495C (en) * | 1988-04-29 | 1993-10-26 | Marc Reist | Process and apparatus for converting of solid high-grade copper matte |
| JP2689540B2 (ja) * | 1988-11-21 | 1997-12-10 | 三菱マテリアル株式会社 | 低酸素含有銅の製造方法及び製造装置 |
| PL169695B1 (pl) * | 1990-11-20 | 1996-08-30 | Mitsubishi Materials Corp | Sposób ciaglego wytopu miedzi PL PL PL |
| MY110307A (en) * | 1990-11-20 | 1998-04-30 | Mitsubishi Materials Corp | Apparatus for continuous copper smelting |
| US5380353A (en) * | 1990-11-20 | 1995-01-10 | Mitsubishi Materials Corporation | Copper smelting apparatus |
| JPH04183828A (ja) * | 1990-11-20 | 1992-06-30 | Mitsubishi Materials Corp | 銅の製錬方法 |
| JP2811956B2 (ja) * | 1990-11-20 | 1998-10-15 | 三菱マテリアル株式会社 | 冶金炉の底抜き装置 |
| SE9103412L (sv) * | 1990-11-20 | 1992-05-21 | Mitsubishi Materials Corp | Roerformig vattenkyld mantel foer ugnar |
| JPH05287402A (ja) * | 1992-04-09 | 1993-11-02 | Mitsubishi Materials Corp | 極低酸素銅の製造法およびその製造法により得られた極低酸素銅 |
| US5215571A (en) * | 1992-10-14 | 1993-06-01 | Inco Limited | Conversion of non-ferrous matte |
| AUPM657794A0 (en) * | 1994-06-30 | 1994-07-21 | Commonwealth Scientific And Industrial Research Organisation | Copper converting |
| US5449395A (en) * | 1994-07-18 | 1995-09-12 | Kennecott Corporation | Apparatus and process for the production of fire-refined blister copper |
-
1997
- 1997-09-24 US US08/936,322 patent/US6042632A/en not_active Expired - Lifetime
-
1998
- 1998-09-21 AU AU94022/98A patent/AU741047B2/en not_active Ceased
- 1998-09-21 ES ES200050025A patent/ES2164036B2/es not_active Expired - Fee Related
- 1998-09-21 KR KR1020007003117A patent/KR100566177B1/ko not_active Expired - Fee Related
- 1998-09-21 ID IDW20000562A patent/ID25891A/id unknown
- 1998-09-21 CA CA002304651A patent/CA2304651A1/en not_active Abandoned
- 1998-09-21 WO PCT/US1998/019722 patent/WO1999015706A1/en not_active Ceased
- 1998-09-21 JP JP2000512993A patent/JP4418588B2/ja not_active Expired - Fee Related
- 1998-09-24 PE PE1998000911A patent/PE116399A1/es not_active Application Discontinuation
Also Published As
| Publication number | Publication date |
|---|---|
| ID25891A (id) | 2000-11-09 |
| US6042632A (en) | 2000-03-28 |
| AU9402298A (en) | 1999-04-12 |
| AU741047B2 (en) | 2001-11-22 |
| CA2304651A1 (en) | 1999-04-01 |
| KR20010015612A (ko) | 2001-02-26 |
| JP2001517734A (ja) | 2001-10-09 |
| JP4418588B2 (ja) | 2010-02-17 |
| KR100566177B1 (ko) | 2006-03-29 |
| ES2164036B2 (es) | 2004-05-16 |
| ES2164036A1 (es) | 2002-02-01 |
| WO1999015706A1 (en) | 1999-04-01 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| PE116399A1 (es) | Metodo para limitar puntos maximos de temperatura y/o aumentar la capacidad de produccion de un horno de refinacion continua de cobre con soplado en la parte alta | |
| ES2845350T3 (es) | Método de tratamiento de hierro con grafito esferoidal | |
| MX166647B (es) | Metodo para fabricacion continua de acero | |
| BR9902358A (pt) | Método de pprodução de metal reduzido, e de forno de fundição móvel para a produção do mesmo | |
| ES271045Y (es) | Disposicion de electrodos de contacto para hornos de fundicion de arco electrico o de resistencia. | |
| FI117768B (fi) | Jäähdytyselementti | |
| ES2170547T3 (es) | Instalacion de reduccion de oxidos de hierro y de fusion de hierro. | |
| BR0105935A (pt) | Método para produzir ferro metálico fundido | |
| ID24294A (id) | Dinding refraktori, bejana metalurgi yang berisi dinding refraktori tersebut dan metode dimana dinding refraktori tersebut diterapkan | |
| BR0116090A (pt) | Processo para melhorar o rendimento de fundição e a qualidade de metais e ligas brutos de fusão, aparelho para aplicar um arco elétrico móvel sobre metais e ligas em fusão, e, eletrodo | |
| ES483637A1 (es) | Un horno de refinacion giratorio para metales no ferricos | |
| ES2171324T3 (es) | Dispositivo precalentador de material de carga, comprendiendo tramos de pared de cuba reemplazables. | |
| ES2178239T3 (es) | Estructura de pared refractaria. | |
| AR014307A1 (es) | Coquilla enfriada por liquido | |
| BR0213344A (pt) | Pia de fundido | |
| BR9809140A (pt) | Combinação de um cartucho carregado com grãosde chumbo e uma ferramenta de balìsticaindustrial | |
| US3237930A (en) | Melting furnace | |
| ES556520A0 (es) | Instalacion de colada continua vertical o en arco para acero | |
| US3729307A (en) | Method and apparatus for electroslag remelting of metals,particularly steel | |
| Brimacombe et al. | Toward a basic understanding of injection phenomena in the copper converter | |
| GB1585570A (en) | Melting and casting apparatus | |
| ES8702636A1 (es) | Procedimiento y dispositivo para la fusion de metales lige- ros | |
| US2732294A (en) | Manufacture of copper | |
| BG107531A (en) | Bottom structure for a smelting furnace | |
| FR2236942A1 (en) | Continuous melting of iron-bearing matls. in an arc furnace - using controlled height of slag and charge for low power consumption |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| FG | Grant, registration | ||
| FD | Application declared void or lapsed |