LU36676A1 - - Google Patents
Info
- Publication number
- LU36676A1 LU36676A1 LU36676DA LU36676A1 LU 36676 A1 LU36676 A1 LU 36676A1 LU 36676D A LU36676D A LU 36676DA LU 36676 A1 LU36676 A1 LU 36676A1
- Authority
- LU
- Luxembourg
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21C—PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- C21C7/00—Treating molten ferrous alloys, e.g. steel, not covered by groups C21C1/00 - C21C5/00
- C21C7/10—Handling in a vacuum
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
Publications (1)
| Publication Number | Publication Date |
|---|---|
| LU36676A1 true LU36676A1 (en) |
Family
ID=1770091
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| LU36676D LU36676A1 (en) |
Country Status (1)
| Country | Link |
|---|---|
| LU (1) | LU36676A1 (en) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP0709469A1 (en) * | 1994-10-18 | 1996-05-01 | Kawasaki Steel Corporation | Method of producing molten aluminium-killed steel for thin steel sheet |
-
0
- LU LU36676D patent/LU36676A1/xx unknown
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| EP0709469A1 (en) * | 1994-10-18 | 1996-05-01 | Kawasaki Steel Corporation | Method of producing molten aluminium-killed steel for thin steel sheet |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US6117389A (en) | Titanium killed steel sheet and method | |
| CN113186458B (en) | Medium-carbon aluminum killed steel for cold heading and smelting method thereof | |
| US5616188A (en) | Method of producing molten aluminum-killed steel for thin steel sheet | |
| FR2451403B1 (en) | STEEL FOR COLD FORGING HAVING GOOD MACHINABILITY AND PROCESS FOR PREPARING SAME | |
| JP2559692B2 (en) | Anti-blurring defect prevention method for ultra low carbon cold rolled steel sheet | |
| TWI773342B (en) | Fertilizer iron series stainless steel | |
| KR100605712B1 (en) | How to prevent clogging of immersion nozzle of aluminum and sulfurized steel | |
| CN100549187C (en) | The method of aluminium deoxidized steel refining desulfuration | |
| JPH01149943A (en) | Cold-rolled steel sheet with excellent workability | |
| CN109022680B (en) | A method for preventing flocculation of low-silicon aluminum killed steel in the first tank | |
| LU36676A1 (en) |