DE499142C - Process for making a durable paint - Google Patents
Process for making a durable paintInfo
- Publication number
- DE499142C DE499142C DEE32315D DEE0032315D DE499142C DE 499142 C DE499142 C DE 499142C DE E32315 D DEE32315 D DE E32315D DE E0032315 D DEE0032315 D DE E0032315D DE 499142 C DE499142 C DE 499142C
- Authority
- DE
- Germany
- Prior art keywords
- paint
- water glass
- clay
- making
- durable
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Verfahren zur Herstellung eines haltbaren Anstrichmittels Es sind verschiedene Wasserglas enthaltende Anstrichmittel für Holz oder Mauerwerk bekannt, die zur Erhöhung der Wetterfestigkeit der betreffenden Materialien dienen und das Holz gegen Fäulnis schützen sollen. Indessen sind diese Mittel sehr kompliziert und teilweise schwierig herzustellen sowie aus verhältnismäßig teuren Bestandteilen zusammengesetzt, bedingen also erhebliche Herstellungskosten und sind infolgedessen sehr teuer. Außerdem verbinden sie sich nicht fest mit dem Untergrund., sondern blättern ab und verhalten sich chemischen Einflüssen gegenüber nicht neutral, da sie zum Teil chemisch sehr energisch wirksame Bestandteile, wie Alkalilauge und Zement, enthalten. Demgegenüber besteht das Anstrichmittel gemäß der Erfindung aus sehr billigen und chemisch zu mindest nicht energisch wirksamen, wenn nicht gar neutralen Materialien, nämlich aus Ton und Wasserglas, gegebenenfalls unter Zusatz von Wasser- oder Ölfarben, ist also außerordentlich billig, verbindet sich außerdem aber auch fest mit dem Untergrund und ist chemischen Einflüssen nicht unterworfen.Method of making a durable paint There are various paints containing water glass for wood or masonry are known, which serve to increase the weather resistance of the materials concerned and that To protect wood against rot. However, these means are very complicated and sometimes difficult to manufacture and made of relatively expensive components composed, so require considerable manufacturing costs and are as a result very expensive. In addition, they do not bond firmly to the subsurface., But peel off and do not behave neutrally towards chemical influences, there some of them are chemically very energetically active ingredients, such as alkali and Cement. In contrast, the paint according to the invention consists of very cheap and chemically at least not energetically effective, if not at all neutral materials, namely made of clay and water glass, optionally with additives of water or oil paints, so it is extremely cheap, also combines but also firmly attached to the subsurface and is not subject to chemical influences.
# Das Verfahren zur Herstellung dieses neuen Anstrichmittels besteht darin, daß Ton in Aufschlämmung oder fein gepulvert mit dem Wasserglase verrührt wird, das sich mit ihm derart verbindet, daß ein haltbarer fester Anstrich entsteht. Der Zusatz von Wasserglas regelt sich dabei nach dem Grade der erforderlichen Wetterbeständigkeit des Farbanstriches.# The process for making this new paint is in place in that clay in slurry or finely powdered mixed with the water glass that bonds with it in such a way that a durable, solid coat of paint is created. The addition of water glass is regulated according to the degree of weather resistance required of painting.
Beispielsweise wird Ton von. der gewünschten natürlichen Färbung oder mit einem entsprechenden Zusatz von Wasserfarben mit Wasser angerührt und dann Wasserglas hinzugefügt, das gut mit der Lösung verrührt wird. Dabei genügt z. B. für Anstrichflächen im Innern von Gebäuden ein Zusatz an Wasserglas von nur ro°/o der Tonlösung, um einen hinsichtlich Festigkeit und Farbton genügend haltbaren Anstrich zu erzielen. Der Anstrich ist dann sofort verwendungsbereit. Für Außenflächen wählt man etwa einen Wasserglaszusatz von 5o°/, der Gewichtsmenge des Tones und erhält dadurch einen Anstrich, der allen Anforderungen hinsichtlich Festigkeit; Farb- und Wetterbeständigkeit sowie Schutz gegen Entflammbarkeit des Holzes genügt und etwa einem zweimaligen Ölfarbenanstrich an Wert gleichkommt, ohne dessen leichte Entflammbarkeit zu besitzen.For example, the sound of. the desired natural color or mixed with water with an appropriate addition of watercolors and then water glass added, which is stirred well with the solution. Sufficient z. B. for painted surfaces in the interior of buildings, an addition of water glass of only about 1/0 of the clay solution to achieve a paint that is sufficiently durable in terms of strength and color. The coating is then ready to use immediately. For outdoor areas, for example, you choose an addition of water glass of 50%, the amount by weight of the clay and thereby receives a paint that meets all strength requirements; Color and weather resistance as well as protection against flammability of the wood is sufficient and about twice Oil paint is equivalent in value without having its easy flammability.
Will man einen besonders dauerhaften Anstrich erzielen, der wenigstens einen dreifachen Ölfarbenanstrich ersetzt, so vermischt man fein gepulverten naturfarbenen Ton, gegebenenfalls unter Hinzufügung der gewünschten Wasserfarben, unmittelbar mit Wasserglas, oder man wählt an Stelle von Wasserfarben Ölfarben, verrührt diese zunächst mit dem Tone und setzt darauf Wasserglas hinzu, das sich dann leicht mit der Ton-Ölfarben-Lösung vermischen läßt. In dem letzteren Falle kann man die Ölfarben auch zunächst mit dem Wasserglas verrühren und dann dem Tone zusetzen.If you want to achieve a particularly durable coat of paint, at least that replacing a triple coat of oil paint, finely powdered natural-colored ones are mixed together Clay, optionally with the addition of the desired watercolors, immediately with water glass, or you can choose oil paints instead of watercolors, stir them together first with the clay and then add a glass of water, which is then easy to use mix the clay-oil paint solution. In the latter case one can use the oil paints Mix with the water glass first and then add to the clay.
Außer für Holz oder Steine kann der Anstrich z. B. auch für Dachpappe verwendet werden, um sie haltbar zu machen und vor allem gegen Entflammbarkeit zu schützen. Besonders vorteilhaft ist das Mittel für bereits etwas rissigen Putz, der@sogar schon leiccft zu blättern anfangen kann, da er in die Risse eindringt und den Putz wieder veiliäifet, so daß dieser nicht mehr abfällt, wie beispielsweise beim Ölfarbenanstrich. Der Putz erhält dadurch unter Umständen eine größere Festigkeit und Härte, als er früher gehabt hat.Except for wood or stones, the paint can e.g. B. also for roofing felt used to make them durable and especially against Flammability to protect. The agent is particularly useful for plaster that is already somewhat cracked, the @ can even begin to leaf through the pages easily because it penetrates the cracks and varnish the plaster again so that it no longer falls off, like for example when painting with oil paint. This may give the plaster greater strength and toughness than it used to be.
Das neue Mittel ist somit nicht -nur-hinsichtlich der Preiswürdigkeit und leichteren Herstellung, sondern auch hinsichtlich des natürlichen Farbtones und der mechanischen Festigkeit sowie wegen seiner geringen Entflammbarkeit den bereits bekannten Anstrichmitteln überlegen und ist außerdem sehr gut und sparsam verstreichbar.The new product is therefore not - only - in terms of value for money and easier production, but also with regard to the natural color tone and the mechanical strength as well as because of its low flammability den superior to known paints and is also very good and economical spreadable.
Claims (1)