DE486977C - Method of weighing and fastening leather - Google Patents
Method of weighing and fastening leatherInfo
- Publication number
- DE486977C DE486977C DER67186D DER0067186D DE486977C DE 486977 C DE486977 C DE 486977C DE R67186 D DER67186 D DE R67186D DE R0067186 D DER0067186 D DE R0067186D DE 486977 C DE486977 C DE 486977C
- Authority
- DE
- Germany
- Prior art keywords
- leather
- weighing
- parts
- fastening
- glue
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Verfahren zum -Beschweren und Festmachen von Leder Bisher hat man versucht, durch Anwendung von Leire, der in Gegenwart von überschüssigem Gerbstoff unlöslich gemacht wurde, Leder fester zu machen. Für diesen Zweck eignet sich aber Leim nur 'unvollkommen, weil. er wegen seiner hochmolekularen Zusammensetzung schwer in das Leder eindringt. Auch ist es bekannt, mit Säure oder Alkali gespaltenen Leim zum Festmachen von Leder zu verwenden. Derart abgebauter Leim hat aber den Nachteil, daß er zuviel Alkaüsalz enthält, welches im Leder unerwünscht ist. Außerdem ist mit Alkali behandelter Leim wegen der noch immer beträchtlichen Molekülgröße nicht geeignet, vollständig in das Leder einzudringen.Method for weighting and securing leather So far, one has tried by applying leire in the presence of excess tanning agent made insoluble to make leather stronger. For this purpose, however, is suitable Glue just 'imperfect because. it is heavy because of its high molecular composition penetrates the leather. It is also known to split glue with acid or alkali to be used for fastening leather. However, such degraded glue has the disadvantage that it contains too much alkali salt, which is undesirable in leather. Also is alkali treated glue does not because of the still considerable molecular size able to penetrate completely into the leather.
Es wurde gefunden, daß Eiweißstoffe, die bei gewöhnlicher oder höherer Temperatur mit Enzymen so weit abgebaut werden, daß der Formolstickstoff io % des Gesamtstickstoffes nicht überschreitet, den überschüssigen Gerbstoff im Leder sehr gut abbinden, das Leder beschweren und festmachen.It has been found that protein substances, which at ordinary or higher Temperature are reduced so far with enzymes that the formol nitrogen io% des Total nitrogen does not exceed the excess tannin in the leather very much Tie off well, weigh down the leather and fasten it.
Gegebenenfalls können noch Haltbarkeitszusätze gemacht werden. Beispielsweise wird so gearbeitet, daß ioo Teile Leder mit a Teilen, mit Enzym abgebautem Eiweiß und mit io Teilen Wasser gewalkt werden. Das zur Verwendung gelangende abgebaute Eiweiß. kann z. B. so gewonnen werden, daß. 65 Teile Leim mit 4.o Teilen Wasser versetzt werden. Diese Lösung wird alkalisch gemacht und mit o,o5 Teilecu handelsüblichem Pankreatin versetzt. Nach einstündiger Reaktionsdauer wird der Abbauprozeß, durch Erhitzen auf 9o bis ioo° beendet. Die so abgebauten Erzeugnisse können gegebenenfalls Zusätze zwecks Haltbai-machung erhalten.If necessary, shelf life additions can be made. For example it is worked in such a way that 100 parts of leather with a parts of enzyme-degraded protein and tumbled with 10 parts of water. The dismantled that is to be used Protein. can e.g. B. be obtained so that. 65 parts of glue with 4.o parts of water be moved. This solution is made alkaline and with 0.05 parts cu commercially available Pancreatin spiked. After a reaction time of one hour, the degradation process is through Heating to 90 to 100 ° ended. The products degraded in this way can, if necessary Received additives for the purpose of holding.
Claims (1)