CN102794360A - 支腿槽管板成型模具 - Google Patents
支腿槽管板成型模具 Download PDFInfo
- Publication number
- CN102794360A CN102794360A CN2012102820400A CN201210282040A CN102794360A CN 102794360 A CN102794360 A CN 102794360A CN 2012102820400 A CN2012102820400 A CN 2012102820400A CN 201210282040 A CN201210282040 A CN 201210282040A CN 102794360 A CN102794360 A CN 102794360A
- Authority
- CN
- China
- Prior art keywords
- mould
- plate
- supporting leg
- turning cylinder
- rotating shaft
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种支腿槽管板成型模具,在上模固定座下部的左右两侧分别装有一个能转动的转动轴,转动轴联接有一个复位弹簧;下模的凸模对板料进行固定和定位,在凸模的左右两侧分别装有顶料板,在顶料板的下方装有退料弹簧;当上模通过油压机向下对固定在凸模上的板料进行压制时,使转动轴接触下模后发生转动,直到上模和下模完全闭合,将固定在凸模上的板料转弯成型。采用转动轴的结构,在油压机的压制作用下,使转动轴接触下模后发生转动,顺利将凸模上的板料转弯成型,转动轴的转动距离短,工作效率提高了一倍,转动轴采取回弹角设计,可使工件成型后完全达到90度直壁,具有生产效率高、工作行程短、产品回弹小且产品质量稳定的特点。
Description
技术领域
本发明属于板料冲压成型设备技术领域,涉及一种主要用于生产半挂车支承装置的支腿槽管板成型模具。
背景技术
支腿产品是半挂车的支承装置,随着世界经济的发展,半挂车的需求量不断增加,由于支腿需求量的增加,更多的企业开始生产支腿,竞争日益激烈。
原有传统模具采用将利用上模11将工件13完全压进下模12的凹模型腔内,由于该工件13有130MM高,760MM长,其行程大,工作时间长,并且无法克服板料本身回弹带来的质量问题。
传统的制造支腿槽管板的压型模具由于生产效率低,工作行程长,产品回弹大,质量不稳定已不能满足生产的要求,它已成为制约生产的工艺瓶颈。
发明内容
为了克服现有技术的上述缺点,本发明提供一种具有生产效率高、工作行程短、产品回弹小且质量稳定的支腿槽管板成型模具。
本发明解决其技术问题所采用的技术方案是:一种支腿槽管板成型模具,包括上模和下模,在上模固定座下部的左右两侧分别装有一个能转动的转动轴,转动轴联接有一个复位弹簧;下模的凸模对板料进行固定和定位,在凸模的左右两侧分别装有顶料板,在顶料板的下方装有退料弹簧;当上模通过油压机向下对固定在凸模上的板料进行压制时,使转动轴接触下模后发生转动,直到上模和下模完全闭合,将固定在凸模上的板料转弯成型。
在所述转动轴上开有一个小于90度角的缺口。
所述复位弹簧的一端与转动轴相联接,它的另一端通过螺栓固定在固定座上,当板料成型完毕后,上模在油压机的作用下向上回程运动时,复位弹簧带动转动轴自动复位,下模弹簧使顶料板运动顶出工件。
所述退料弹簧的一端与顶料板相接触,它的另一端固定在下模的底座内,当板料成型完毕后,上模在油压机的作用下向上回程运动时,退料弹簧带动顶料板运动,顶出工件。
在两个转动轴之间的固定座的下边缘上装有压料板。
本发明的有益效果是:采用了转动轴的结构,在油压机的压制作用下,使转动轴接触下模后发生转动,顺利将凸模上的板料转弯成型,转动轴的转动距离为原模具行程的一半,工作效率提高了一倍,转动轴采取回弹角设计,可使工件成型后完全达到90度直壁,具有生产效率高、工作行程短、产品回弹小且产品质量稳定的特点。
附图说明
图1是现有槽管板成型模结构示意图。
图2是本发明结构示意图。
图1中:11-上模,12-下模,13-工件,14-顶料板。
图2中:1-固定座,2-转动轴,3-复位弹簧,4-压料板,5-退料弹簧,6-顶料板,7-凸模。
具体实施方式
下面结合附图和实施例对本发明进一步说明。
参见图2,一种支腿槽管板成型模具,包括上模和下模,在上模固定座1下部的左右两侧分别装有一个能转动的转动轴2,在所述转动轴2上开有一个小于90度角的缺口,转动轴2联接有一个复位弹簧3,在两个转动轴2之间的固定座1的下边缘上装有压料板4;下模的凸模7对板料进行固定和定位,在凸模7的左右两侧分别装有顶料板6,在顶料板6的下方装有退料弹簧5;当上模通过油压机向下对固定在凸模7上的板料进行压制时,使转动轴2接触下模后发生转动,直到上模和下模完全闭合,将固定在凸模7上的板料转弯成型。
所述复位弹簧3的一端与转动轴2相联接,它的另一端通过螺栓固定在固定座1上,当板料成型完毕后,上模在油压机的作用下向上回程运动时,复位弹簧3带动转动轴2自动复位;所述退料弹簧5的一端与顶料板6相接触,它的另一端固定在下模的底座内,当板料成型完毕后,上模在油压机的作用下向上回程运动时,退料弹簧5带动顶料板6运动,顶出工件。
本发明采用了转动轴的结构,在油压机的压制作用下,使转动轴接触下模后发生转动,顺利将凸模上的板料转弯成型,转动轴的转动距离为原模具行程的一半,工作效率提高了一倍,转动轴采取回弹角设计,可使工件成型后完全达到90度直壁,具有生产效率高、工作行程短、产品回弹小且产品质量稳定的特点。
Claims (5)
1.一种支腿槽管板成型模具,包括上模和下模,其特征是:在上模固定座下部的左右两侧分别装有一个能转动的转动轴,转动轴联接有一个复位弹簧;下模的凸模对板料进行固定和定位,在凸模的左右两侧分别装有顶料板,在顶料板的下方装有退料弹簧;当上模通过油压机向下对固定在凸模上的板料进行压制时,使转动轴接触下模后发生转动,直到上模和下模完全闭合,将固定在凸模上的板料转弯成型。
2.如权利要求1所述支腿槽管板成型模具,其特征是:在所述转动轴上开有一个小于90度角的缺口。
3.如权利要求1所述支腿槽管板成型模具,其特征是:所述复位弹簧的一端与转动轴相联接,它的另一端通过螺栓固定在固定座上,当板料成型完毕后,上模在油压机的作用下向上回程运动时,复位弹簧带动转动轴自动复位,下模弹簧使顶料板运动顶出工件。
4.如权利要求1所述支腿槽管板成型模具,其特征是:所述退料弹簧的一端与顶料板相接触,它的另一端固定在下模的底座内,当板料成型完毕后,上模在油压机的作用下向上回程运动时,退料弹簧带动顶料板运动,顶出工件。
5.如权利要求1或2所述支腿槽管板成型模具,其特征是:在两个转动轴之间的固定座的下边缘上装有压料板。