[go: up one dir, main page]

TW200511326A - Process to mitigate stress corrosion cracking of structural materials in high temperature water - Google Patents

Process to mitigate stress corrosion cracking of structural materials in high temperature water

Info

Publication number
TW200511326A
TW200511326A TW093116733A TW93116733A TW200511326A TW 200511326 A TW200511326 A TW 200511326A TW 093116733 A TW093116733 A TW 093116733A TW 93116733 A TW93116733 A TW 93116733A TW 200511326 A TW200511326 A TW 200511326A
Authority
TW
Taiwan
Prior art keywords
high temperature
temperature water
stress corrosion
corrosion cracking
structural materials
Prior art date
Application number
TW093116733A
Other languages
English (en)
Other versions
TWI349291B (en
Inventor
Young-Jin Kim
Thomas Martin Angeliu
Peter Louis Andresen
Original Assignee
Gen Electric
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Gen Electric filed Critical Gen Electric
Publication of TW200511326A publication Critical patent/TW200511326A/zh
Application granted granted Critical
Publication of TWI349291B publication Critical patent/TWI349291B/zh

Links

Classifications

    • GPHYSICS
    • G21NUCLEAR PHYSICS; NUCLEAR ENGINEERING
    • G21CNUCLEAR REACTORS
    • G21C17/00Monitoring; Testing ; Maintaining
    • G21C17/02Devices or arrangements for monitoring coolant or moderator
    • G21C17/022Devices or arrangements for monitoring coolant or moderator for monitoring liquid coolants or moderators
    • G21C17/0225Chemical surface treatment, e.g. corrosion
    • GPHYSICS
    • G21NUCLEAR PHYSICS; NUCLEAR ENGINEERING
    • G21CNUCLEAR REACTORS
    • G21C19/00Arrangements for treating, for handling, or for facilitating the handling of, fuel or other materials which are used within the reactor, e.g. within its pressure vessel
    • G21C19/28Arrangements for introducing fluent material into the reactor core; Arrangements for removing fluent material from the reactor core
    • G21C19/30Arrangements for introducing fluent material into the reactor core; Arrangements for removing fluent material from the reactor core with continuous purification of circulating fluent material, e.g. by extraction of fission products deterioration or corrosion products, impurities, e.g. by cold traps
    • G21C19/307Arrangements for introducing fluent material into the reactor core; Arrangements for removing fluent material from the reactor core with continuous purification of circulating fluent material, e.g. by extraction of fission products deterioration or corrosion products, impurities, e.g. by cold traps specially adapted for liquids
    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02EREDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E30/00Energy generation of nuclear origin
    • Y02E30/30Nuclear fission reactors

Landscapes

  • Physics & Mathematics (AREA)
  • Engineering & Computer Science (AREA)
  • Plasma & Fusion (AREA)
  • General Engineering & Computer Science (AREA)
  • High Energy & Nuclear Physics (AREA)
  • Catalysts (AREA)
  • Preventing Corrosion Or Incrustation Of Metals (AREA)
  • Prevention Of Electric Corrosion (AREA)
TW093116733A 2003-06-16 2004-06-10 Process to mitigate stress corrosion cracking of structural materials in high temperature water TWI349291B (en)

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
US10/462,113 US6724854B1 (en) 2003-06-16 2003-06-16 Process to mitigate stress corrosion cracking of structural materials in high temperature water

Publications (2)

Publication Number Publication Date
TW200511326A true TW200511326A (en) 2005-03-16
TWI349291B TWI349291B (en) 2011-09-21

Family

ID=32070048

Family Applications (1)

Application Number Title Priority Date Filing Date
TW093116733A TWI349291B (en) 2003-06-16 2004-06-10 Process to mitigate stress corrosion cracking of structural materials in high temperature water

Country Status (4)

Country Link
US (1) US6724854B1 (zh)
EP (1) EP1489625A1 (zh)
JP (1) JP2005010160A (zh)
TW (1) TWI349291B (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102612573A (zh) * 2009-11-16 2012-07-25 株式会社东芝 用于高温水体系的抗腐蚀结构以及其防腐方法

Families Citing this family (24)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE10123690A1 (de) * 2001-05-15 2002-12-05 Framatome Anp Gmbh Verfahren zum Schutz der Bauteile des Primärsystems eines Siedewasserreaktors insbesondere vor Spannungsrisskorrosion
US20040022346A1 (en) * 2002-07-31 2004-02-05 General Electric Company Method for forming coatings on structural components with corrosion-mitigating materials
JP4105052B2 (ja) * 2003-07-22 2008-06-18 日立Geニュークリア・エナジー株式会社 原子力プラント構造材料の応力腐食割れを緩和する方法
JP4776219B2 (ja) * 2004-12-09 2011-09-21 株式会社東芝 原子力発電プラントとその耐食性被膜形成方法および原子炉運転方法
US20070003001A1 (en) * 2005-06-30 2007-01-04 General Electric Company Method for mitigation oxide fouling in structural components in light water reactors
WO2008005590A2 (en) 2006-02-22 2008-01-10 University Of Florida Research Foundation, Inc. Nuclear reactor having efficient and highly stable thermal transfer fluid
US8976920B2 (en) * 2007-03-02 2015-03-10 Areva Np Nuclear power plant using nanoparticles in emergency systems and related method
US20080219395A1 (en) * 2007-03-06 2008-09-11 Areva Np Nuclear power plant using nanoparticles in emergency situations and related method
US8160197B2 (en) 2007-03-06 2012-04-17 Areva Np Nuclear power plant using nanoparticies in closed circuits of emergency systems and related method
US20090229714A1 (en) * 2008-03-13 2009-09-17 General Electric Company Method of mitigating stress corrosion cracking in austenitic solid solution strengthened stainless steels
JP5686539B2 (ja) * 2010-07-12 2015-03-18 日立Geニュークリア・エナジー株式会社 排ガス再結合器の出口水素濃度予測装置及び出口水素濃度の予測方法
FR2975215B1 (fr) * 2011-05-11 2013-05-10 Areva Reacteur nucleaire avec dispositif d'injection de nano particules en cas d'accident
US9384862B2 (en) * 2012-06-22 2016-07-05 Ge-Hitachi Nuclear Energy Americas Llc Method of fabricating liquid-metal coolants for nuclear reactors
JP6049384B2 (ja) * 2012-10-03 2016-12-21 株式会社東芝 光触媒注入方法および光触媒注入システム
US20140140465A1 (en) * 2012-11-19 2014-05-22 Hitachi-Ge Nuclear Energy Ltd. Platinum Oxide Colloidal Solution, Manufacturing Method Therefor, Manufacture Apparatus Thereof, and Method of Injection Noble Metal of Boiling Water Nuclear Power Plant
DE102015120722B4 (de) * 2015-11-30 2017-07-27 Areva Gmbh Kernkraftwerk und Verfahren zum Betreiben eines Kernkraftwerks
JP6486860B2 (ja) * 2016-03-31 2019-03-20 日立Geニュークリア・エナジー株式会社 沸騰水型原子炉の腐食環境緩和方法及び原子力プラント
US10457583B2 (en) 2016-03-31 2019-10-29 Hitachi-Ge Nuclear Energy, Ltd. Method for relieving corrosive environment of boiling water reactor, nuclear power plant, and method for injecting noble metal which is carried out in nuclear power plant
JP6585553B2 (ja) * 2016-06-28 2019-10-02 日立Geニュークリア・エナジー株式会社 原子力プラント構成部材の応力腐食割れ抑制方法
JP6890120B2 (ja) 2016-08-04 2021-06-18 ドミニオン エンジニアリング, インク.Dominion Engineering, Inc. 原子力発電所構成部品上への放射性核種堆積の抑制
JP2018155588A (ja) * 2017-03-17 2018-10-04 日立Geニュークリア・エナジー株式会社 貴金属付着量の分析方法
JP7001534B2 (ja) * 2018-04-27 2022-02-04 日立Geニュークリア・エナジー株式会社 原子力プラントの構造部材への放射性核種の付着抑制方法
WO2020056093A1 (en) * 2018-09-12 2020-03-19 Magna International Inc. Electromagnetically assisted metal spray process
JP7104616B2 (ja) * 2018-12-19 2022-07-21 日立Geニュークリア・エナジー株式会社 原子力プラントの炭素鋼部材への放射性核種の付着抑制方法

Family Cites Families (31)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS59134302A (ja) 1983-01-24 1984-08-02 Toshiba Corp 蒸気タ−ビンの腐蝕防止装置
US4842811A (en) 1985-02-05 1989-06-27 Westinghouse Electric Corp. Method for preventing oxygen corrosion in a boiling water nuclear reactor and improved boiling water reactor system
US5130080A (en) 1990-04-02 1992-07-14 General Electric Company Method of providing extended life expectancy for components of boiling water reactors
US5130081A (en) 1990-04-02 1992-07-14 General Electric Company Operation life of on-life boiling water reactors
US5135709A (en) 1991-05-13 1992-08-04 General Electric Company Method for reducing corrosion of components exposed to high-temperature water
US5147602A (en) 1991-05-20 1992-09-15 General Electric Company Corrosion resistant high chromium stainless steel alloy
US5164152A (en) 1991-08-02 1992-11-17 General Electric Company Method for reducing flow assisted corrosion of carbon steel components
US5608766A (en) 1993-10-29 1997-03-04 General Electric Company Co-deposition of palladium during oxide film growth in high-temperature water to mitigate stress corrosion cracking
US5625656A (en) 1993-10-29 1997-04-29 General Electric Company Method for monitoring noble metal distribution in reactor circuit during plant application
US5774516A (en) 1993-10-29 1998-06-30 General Electric Company Modification of oxide film electrical conductivity to maintain low corrosion potential in high-temperature water
US5602888A (en) 1993-10-29 1997-02-11 General Electric Company Radiation-induced palladium doping of metals to protect against stress corrosion cracking
US5818893A (en) 1993-10-29 1998-10-06 General Electric Company In-situ palladium doping or coating of stainless steel surfaces
US5600692A (en) 1993-10-29 1997-02-04 General Electric Company Method for improving tenacity and loading of palladium on palladium-doped metal surfaces
US5773096A (en) 1993-10-29 1998-06-30 General Electric Company Method of catalyst preparation by high-temperature hydrothermal incorporation of noble metals onto surfaces and matrices
US5600691A (en) 1993-10-29 1997-02-04 General Electric Company Noble metal doping or coating of crack interior for stress corrosion cracking protection of metals
US5673297A (en) 1994-04-08 1997-09-30 General Electric Company Method of mitigating stress corrosion cracking of metals in high-temperature water by control of crack tip pH
US5571394A (en) 1995-05-08 1996-11-05 General Electric Company Monolithic sensor switch for detecting presence of stoichiometric H2 /O2 ratio in boiling water reactor circuit
US5581588A (en) 1995-06-23 1996-12-03 General Electric Company Insulated protective coating doped with a noble metal for mitigation of stress corrosion cracking
US5793830A (en) 1995-07-03 1998-08-11 General Electric Company Metal alloy coating for mitigation of stress corrosion cracking of metal components in high-temperature water
US6714618B1 (en) 1997-11-28 2004-03-30 General Electric Company Temperature-based method for controlling the amount of metal applied to metal oxide surfaces to reduce corrosion and stress corrosion cracking
ZA200007228B (en) 1998-10-13 2002-08-01 Gen Electric Application of noble metals to internal surfaces of operating boiling water reactors in the presence of zinc in reactor water.
US6168382B1 (en) 1998-10-20 2001-01-02 General Electric Co. Turbine rotor wheel with forged replacement dovetail and method of repair
JP2000329895A (ja) * 1999-05-21 2000-11-30 Hitachi Ltd 原子炉プラントの運転方法及び原子炉プラントの廃液処理方法
JP4043647B2 (ja) * 1999-06-23 2008-02-06 株式会社東芝 原子炉構造材及び原子炉構造材の腐食低減方法
JP2001124891A (ja) * 1999-07-09 2001-05-11 Hitachi Ltd 原子力プラント構造物の表面処理方法および原子力プラント
US6473480B1 (en) 1999-12-30 2002-10-29 General Electric Company Method and apparatus for maintaining proper noble metal loading for a noble metal application process for water-cooled nuclear reactors
JP4334106B2 (ja) * 2000-03-31 2009-09-30 株式会社東芝 原子炉構造材料の光触媒付着方法
US6344098B1 (en) 2000-12-08 2002-02-05 General Electric Company High strength steam turbine rotor and methods of fabricating the rotor without increased stress corrosion cracking
US20020080906A1 (en) 2000-12-21 2002-06-27 Andresen Peter L. Noble metal catalysis for mitigation of corrosion, erosion and stress corrosion cracking in pressurized water reactor and related high temperature water environments
US6793883B2 (en) 2001-07-05 2004-09-21 General Electric Company Application of catalytic nanoparticles to high temperature water systems to reduce stress corrosion cracking
JP2003215289A (ja) * 2002-01-18 2003-07-30 Hitachi Ltd 中性物質注入系統を有する原子力プラント

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102612573A (zh) * 2009-11-16 2012-07-25 株式会社东芝 用于高温水体系的抗腐蚀结构以及其防腐方法
US9062878B2 (en) 2009-11-16 2015-06-23 Kabushiki Kaisha Toshiba Corrosion-resistant structure for high-temperature water system and corrosion-preventing method thereof
US9771482B2 (en) 2009-11-16 2017-09-26 Kabushiki Kaisha Toshiba Corrosion-resistant structure for high-temperature water system and corrosion-preventing method thereof
US9969889B2 (en) 2009-11-16 2018-05-15 Kabushiki Kaisha Toshiba Corrosion-resistant structure for high-temperature water system and corrosion-preventing method thereof

Also Published As

Publication number Publication date
JP2005010160A (ja) 2005-01-13
EP1489625A1 (en) 2004-12-22
TWI349291B (en) 2011-09-21
US6724854B1 (en) 2004-04-20

Similar Documents

Publication Publication Date Title
TW200511326A (en) Process to mitigate stress corrosion cracking of structural materials in high temperature water
TW200736415A (en) Electroform, methods of making electroforms, and products made from electroforms
TW200710275A (en) Mitigation of stress corrosion cracking of structural materials exposed to a high temperature water
WO2008083228A3 (en) Compositions and methods for treating inflammation and auto-immune diseases
NZ575879A (en) Advanced biorefinery process
WO2003018767A3 (en) Trans-differentiation and re-differentiation of somatic cells and production of cells for cell therapies
DE112007002099A5 (de) Solarzelle, Verfahren zur Herstellung von Solarzellen sowie elektrische Leiterbahn
WO2004050826A3 (en) Method of dynamically culturing embryonic stem cells
EP2023435A4 (en) PROCESS FOR PRODUCING ELECTRODE SUBSTRATE, ELECTRODE SUBSTRATE, PHOTOELECTRIC CONVERTER, AND DYE-SENSITIVE SOLAR CELL
UA102994C2 (ru) АНТИТЕЛО, КОТОРОЕ СПЕЦИФИЧНО СВЯЗЫВАЕТСЯ С IgE/M1' И ИНДУЦИРУЕТ АПОПТОЗ В ЭКСПРЕССИРУЮЩИХ IgE В-КЛЕТКАХ
MY143007A (en) Method and device for cleaning a metal strip
WO2009034479A3 (en) Hydrogen production by contacting a composition with water under an ultrasonic action
SG138546A1 (en) Component of variable thickness having residual compressive stresses therein, and method therefor
WO2007148085A3 (en) Electrode, method of manufacture and use thereof
IL165179A0 (en) Electrode for electric discharge surface treatment, method of electric discharge surface treatment, and apparatus for electric discharge surface treatment
ZA201004360B (en) Method of producing middle distillates by sequenced hydroisomerization and hydrocracking of effluent prodeced by the fischer-tropsch process
GB201009772D0 (en) Metal treatment
WO2006011811A3 (en) Radicals and their use as paramagnetic agents in a dynamic nuclear polarisation process
EP1843974A4 (en) PROCESS AND COMPOSITION FOR THE PRODUCTION OF HYDROGEN
NO20021425D0 (no) Fremgangsmåte for reduksjon av forkoksningen i krakkingsreaktorer
DE60204351D1 (de) Verfahren zur zerstörung von nuklearem graphit durch vergasung in wässrigem medium
WO2009009114A3 (en) Compositions and methods for treating and diagnosing cancer
AU2003216956A1 (en) Method for treating water in order to reduce the metal ion concentration thereof
ATE398169T1 (de) Verfahren zur reinigung von oozysten mittels enzymatischer verdauung von faeces
SI2035556T1 (sl) Metoda za izdelavo lipaze, transformirana celica yarrowia lipolytica sposobna proizvajanja omenjene lipaze in njihove uporabe

Legal Events

Date Code Title Description
MK4A Expiration of patent term of an invention patent